... Abstract This chapter discusses the phase transformations of peritectic alloy systems. It describes the processes involved with equilibrium and nonequilibrium freezing, the mechanisms of peritectic formation, and the resulting microstructures. It also discusses the formation of peritectic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240075
EISBN: 978-1-62708-251-8
... curves and construction of eutectic phase diagram. Source: Ref 6 Although not as common as the eutectic reaction, the peritectic reaction is another liquid-solid transformation that at first appears to be similar to the eutectic reaction but is actually very different. The silver-platinum system...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220129
EISBN: 978-1-62708-259-4
.... , Arai Y. , Suzuki M. , and Emi T. , Kinetics of Peritectic Reaction and Transformation in Fe-C Alloys . Metallur. Mat. Trans. B , Vol 31B , October 2000 , p 981 – 91 10.1007/s11663-000-0074-3 14. Wikipedia , Adolf Ledebur , 2007 , http://de.wikipedia.org/wiki...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420143
EISBN: 978-1-62708-310-2
... similar to peritectic transformations, except that the initial phases are both solid. An example of a peritectoid transformation is provided by the formation of the intermetallic compound U 3 Si in uranium-silicon alloys. The relevant phase diagram is shown in Fig. 8.30 . Casting uranium at the proper...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420015
EISBN: 978-1-62708-310-2
... almost exclusively by the rate of heat removal. Important liquid-solid transformations include the eutectic, peritectic, and monotectic reactions that are covered in Chapters 5 , 6 , and 7 in this book, respectively. Solid-state phase transformations occur when one or more parent phases, usually...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480031
EISBN: 978-1-62708-318-8
... Abstract This chapter describes the structures, phases, and phase transformations observed in metals and alloys as they solidify and cool to lower temperatures. It begins with a review of the solidification process, covering nucleation, grain growth, and the factors that influence grain...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420171
EISBN: 978-1-62708-310-2
..., such as a peritectic transformation. A congruent melting phase melts in the same manner as a pure metal. In this case, the phase diagram is divided into essentially independent sections. In Fig. 9.1 , the congruent melting β phase divides the lead-magnesium diagram into two separate eutectic reactions...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560309
EISBN: 978-1-62708-291-4
..., including electroslag, TIG, gas, electron-beam, and arc welding as well as vacuum diffusion, forge, friction, electrical-resistance, and explosive welding. It also discusses the effect of welding temperature, pressure, and composition on the transformations that occur in and around the weld, and it includes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420239
EISBN: 978-1-62708-310-2
... isothermal and vertical sections as well as liquid projections. It also explains how diffusion couples provide a window into local equilibria and identifies typical phase diagram construction errors along with problems stemming from phase-boundary curvatures and congruent transformations. phase...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430027
EISBN: 978-1-62708-253-2
.... The iron-carbon diagram shows three horizontal lines each representing an invariant transformation occurring at reaction points having constant temperature and involving three phases. These reactions are known as peritectic, eutectic, and eutectoid reactions. Peritectic reaction occurs at a...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410621
EISBN: 978-1-62708-265-5
... high-speed, water-hardening, shock-resistant, and hot and cold work tool steels. It discusses the influence of alloy design on the evolution of microstructure and properties during solidification, heat treating, and hardening operations. It also describes critical phase transformations and the effects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230179
EISBN: 978-1-62708-298-3
... 10.1016/0001-6160(80)90034-6 Figure 15.1 . This system has one incongruent melting compound, AgBe 2 . The compound melts peritectically at a temperature of 1010 °C (1850 °F), and it decomposes at temperatures below 760 °C (1400 °F). The eutectic between this compound and pure silver is at 880...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410017
EISBN: 978-1-62708-265-5
... of peritectic alloys , International Materials Reviews , Vol. 41 , 1996 , p 129 - 164 10.1179/imr.1996.41.4.129 3.22 Shibata H. , Arai Y. , Suzuki M. , and Emi T. , Kintetics of Peritectic Reaction and Transformation in Fe-C Alloys , Metallurgical and Materials...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420191
EISBN: 978-1-62708-310-2
.... eutectic reactions peritectic reactions space model ternary phase diagram TERNARY SYSTEMS are those having three components. It is not possible to describe the composition of a ternary alloy with a single number or fraction, as was done with binary alloys, but the statement of two independent...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730011
EISBN: 978-1-62708-283-9
... . This system is called eutectic. Fig. 2.4 The lead-tin phase diagram. Source: Ref 2.1 The reaction L → α + β on cooling through 183° is a eutectic reaction that on cooling, a liquid transforms into two solid phases at the same time. When a liquid containing 62% Sn cools, the α...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2016
DOI: 10.31399/asm.tb.ascaam.t59190001
EISBN: 978-1-62708-296-9
.... Dinnis C.M. , Dahle A.K. , and Taylor J.A. , Three-Dimensional Analysis of Eutectic Grains in Hypoeutectic Al-Si Alloys , Mat. Sci. Eng. A-Struct. , Vol 392A , 2005 , p 440 – 448 10.1016/j.msea.2004.10.037 63. Wołczyński W.S. , Lamella/Rod Transformation as Described by...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410439
EISBN: 978-1-62708-265-5
... The Brimacombe Memorial Symposium , Irons G. A. and Cramb A. W. , Ed., The Metallurgical Society of CIM (MetSoc), 2000 19.10 Shibata H. , Arai Y. , Suzuki M. , and Emi T. , Kintetics of Peritectic Reaction and Transformation in Fe-C alloys , Metall. and Mater...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420339
EISBN: 978-1-62708-310-2
... phase change is different from reactions at the invariant points of phase transformation (e.g., a eutectic or peritectic), where any change in temperature or composition results in complete transformation of the parent into a matrix with a different crystal structure. Fig. 16.1 Equilibrium phase...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410163
EISBN: 978-1-62708-265-5
... chemical variations produced by interdendritic segregation. banding chemical segregation inclusions solidification structure THE PREVIOUS CHAPTERS describing austenite and the solid-state phase transformations that produce microstructures consisting of ferrite, cementite, pearlite, bainite...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130503
EISBN: 978-1-62708-284-6
... been heated to nearly the melting temperature, followed by rapid cooling. Because of its higher carbon content and large austenite grain size, the coarse-grained HAZ develops a significantly higher hardness than the weld metal. The HAZ will transform to martensite upon cooling if the carbon equivalent...