1-20 of 977 Search Results for

performance testing

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000147
EISBN: 978-1-62708-312-6
... and performance data from various sources. electrochemical corrosion test ferric chloride test ferroxyl test immersion testing oxidation resistance salt spray testing sintering stainless steel CORROSION DATA of sintered stainless steels should be viewed somewhat differently from those of wrought...
Image
Published: 30 April 2020
Fig. 7.21 Outline of how strength tests are performed during thermal binder burnout using a three-point fracture test on rectangular samples More
Image
Published: 01 June 1988
Fig. 4.3 Test data sheet for recording performance of an RF power supply with a calorimeter Source: Ameritherm, Inc. More
Image
Published: 01 August 1999
Fig. 17 Influence of specimen configuration on SCC test performance (alternate immersion in 3.5% sodium chloride per ASTM G 44). Aluminum alloy 7075-T7X51 specimens stressed 310 MPa (45 ksi); each point represents 60 to 90 specimens. Source: Ref 25 More
Image
Published: 01 January 2017
Fig. 17.17 Influence of specimen configuration on SCC test performance (alternate immersion in 3.5% NaCl per ASTM G 44). Aluminum alloy 7075-T7X51 specimens stressed 310 MPa (45 ksi); each point represents 60 to 90 specimens. Source: Ref 17.18 More
Image
Published: 01 November 2007
Fig. 3.26 Cyclic oxidation tests performed on 253MA, 353MA, and 800H at 871, 982, 1093, and 1150 °C (1600, 1800, 2000, and 2100 °F) for 1640 h with specimens cycling to room temperature every 160 h. Source: Ref 34 More
Image
Published: 01 December 1995
Fig. 17-18 An impact test being performed More
Image
Published: 01 July 1997
Fig. 5 Comparison of MCL data obtained from varestraint weldability tests performed on aluminum binary alloys using 4% augmented strain. Source: Ref 5 More
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290193
EISBN: 978-1-62708-319-5
... Abstract When a material is sintered and evaluated for performance, the primary focus is on mechanical properties. This chapter discusses structural properties for representative materials. Some guidelines are presented on the types of tests and how property values depend on the testing...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ciktmse.t56080001
EISBN: 978-1-62708-460-4
... of a potent corrosion inhibitor. Weight Loss Measurement Weight loss measurement is a simple operation that permits efficient and cost-effective data acquisition by enabling simultaneous testing of multiple samples. It also yields comparable results with good reproducibility when performed by following...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ciktmse.t56080029
EISBN: 978-1-62708-460-4
..., and the development of a test plan to evaluate the long-term corrosion protection of a potential inhibitor. acid pickling corrosion current density corrosion inhibitors corrosion kinetics corrosion potential inhibitor efficiency PDS curves Stern-Geary equation Tafel slope Problem 1 List...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220667
EISBN: 978-1-62708-259-4
...- or macrostructural feature of an item To test a hypothesis related to the behavior or performance of an item To investigate structure-related causes of a given behavior or performance of an item It is very important to clearly understand the differences between these objectives so that the metallographic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110634
EISBN: 978-1-62708-247-1
... is that the defected flaws may be “nuisances” that never cause functional failure. Performing physical failure analysis on IDDQ-only fails provides insight into their nature. Figure 2 shows physical failure analysis results for two IDDQ-only failing chips. Results such as these demonstrate that indeed the IDDQ test...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870489
EISBN: 978-1-62708-314-0
... testing, evaluation, and control of these characteristics are necessary to ensure that the prepreg materials’ handling characteristics are optimal and final part structural performance is obtained. Woven fabric is the most common continuous dry material form. A woven fabric consists of interlaced warp...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430409
EISBN: 978-1-62708-253-2
..., creep, various forms of corrosion, erosion, fatigue, manufacturing, and operational issues. Any such failure ultimately affects the performance of the plant due to unscheduled forced shutdowns. Therefore, the condition of the tubes needs to be checked periodically by RLA tests. Remaining life assessment...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930039
EISBN: 978-1-62708-359-1
..., hardness, and impact or fracture toughness. Corrosion testing is often employed in situations where a welding operation is performed on a corrosion-resistant material, or in a structure exposed to a hostile environment. Although absolute corrosion performance is important, a major concern is to ensure...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250311
EISBN: 978-1-62708-345-4
... Layout of Lewis parabola for tooth-bending stress calculation Fig. 1 Kinematics of a gear mesh Abstract Mechanical tests are performed to evaluate the durability of gears under load. The chapter first discusses the processes involved in the computations of stress for test parameters...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780159
EISBN: 978-1-62708-281-5
..., and it is difficult to develop meaningful laboratory simulations. Both the relatively simple tests performed on basic polymers and their compounds and the larger-scale tests performed on fabricated structures are criticized for their lack of ability to predict real-life performance ( Ref 8 ). In spite...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390456
EISBN: 978-1-62708-459-8
... performance testing rake angle tool life Chapters 8 to 12 were devoted to processes where fracture is undesirable – with the exception of the process of shearing – and the shape of the part is produced by plastic flow. Machining differs in that the material is intentionally separated and the shape...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930163
EISBN: 978-1-62708-359-1
... is one of the major roadblocks to the development of testing and evaluation methodologies for applying fracture mechanics to weldments. Failure-Assessment Diagrams The concept of performing fitness-for-service assessments using a failure-assessment diagram (FAD) was first proposed in 1975...