1-20 of 78 Search Results for

particulate-filled composites

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780276
EISBN: 978-1-62708-281-5
...Abstract Abstract This article briefly reviews abrasive and adhesive wear failure of reinforced polymers and polymer composites, namely particulate-filled polymers, short-fiber-reinforced polymers, polymers with continuous fibers, and mixed reinforcements and fabrics. It includes scanning...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550457
EISBN: 978-1-62708-307-2
..., aluminum oxide (Al 2 O 3 ), and refractory metals. Discontinuous reinforcements consist mainly of SiC in whisker (w) form, particulate (p) types of SiC, Al 2 O 3 , and titanium diboride (TiB 2 ), and short or chopped fibers (c) of Al 2 O 3 or graphite. A relative comparison of composite performance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
... filling. The improvement in soundness results in degrees of acceptability for welding and heat treatment. Most cast aluminum motor rotors are produced in specialized compositions by smaller vertical die casting machines. The objective is consistent electrical performance. Alloys 100.0, 150.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.9781627083126
EISBN: 978-1-62708-312-6
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
.... , Messer P.F. , and Ellis B. , Preparation of Feedstock for PIM by Using a New Binder System , Advances in Powder Metallurgy and Particulate Materials—1995 , Vol 2 , Metal Powder Industries Federation , Princeton, NJ , 1995 , p 6.37 – 6.43 • Ashby M.F. , Evans A. , Fleck N.A...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... Fig. 20.7 Properties of silicon carbide particulate (SiC p ) discontinuously reinforced aluminum composites. CTE, coefficient of thermal expansion; International Annealed Copper Standard (IACS). Source: Ref 2 Fig. 20.8 Elevated-temperature properties of silicon carbide (SiC) particulate...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000039
EISBN: 978-1-62708-312-6
... the Green Properties of PM Stainless Steels , Advances in Powder Metallurgy and Particulate Materials , ed. Eisen W. , Kassam S. , Vol 7 , MPIF , Princeton, NJ , 2001 , p 7 - 121 to 7 - 134 6. Bergkvist A. , Stainless Steel Powders for High Density Applications , Advances...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290085
EISBN: 978-1-62708-319-5
.... , Particulate Composites: Fundamentals and Applications , Springer International , Switzerland , 2016 10.1007/978-3-319-29917-4_11 • Hackley V.A. and Ferraris C.F. , “ Guide to Rheological Nomenclature: Measurements in Ceramic Particulate Systems ,” NIST Special Publication 946, National...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290251
EISBN: 978-1-62708-319-5
... Fig. 11.7 The filling time is shown on a finite-element simulation of molding for copper feedstock, showing isolation of the proper gate location to avoid defects and weld line placement in a high-stress region. Fig. 11.2 Two examples of alignment in powder-binder systems...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290009
EISBN: 978-1-62708-319-5
... reaction Powders are fabricated to meet requirements of composition, particle size, particle shape, and interparticle friction. Ways to identify a powder include size distribution and packing density as measured using standardized tests. Powder production is done through several approaches. The main...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870573
EISBN: 978-1-62708-314-0
.... In a manner similar to that used for monolithic ceramic materials, powder processing can be used to fabricate discontinuously reinforced ceramic matrix composites. While this process works well for very small reinforcements such as whiskers and particulates, longer discontinuous fibers are broken into shorter...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290067
EISBN: 978-1-62708-319-5
... Bodies , J. Am. Ceram. Soc. , Vol 84 , 2001 , p 1405 – 1410 10.1111/j.1151-2916.2001.tb00851.x • Carreno-Morelli E. and Bidaux J.E. , Processing of Titanium Based Materials for Low Cost Titanium Hydride Powders: PIM and Tape Casting , Advances in Powder Metallurgy and Particulate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260187
EISBN: 978-1-62708-336-2
.... , Further Developments in the Extrusion of Aluminum-Based Metal Matrix Composites , Proc. Sixth International Aluminum Extrusion Technology Seminar , Vol 1 , Aluminum Association and Aluminum Extruders Council , 1996 23. Dixon W. , Extrusion of Particulate-Reinforced Aluminum-Based Metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610377
EISBN: 978-1-62708-303-4
..., the reinforcement is harder, stronger, and stiffer than the matrix. The reinforcement is usually a fiber or a particulate. Particulate composites have dimensions that are approximately equal in all directions. They may be spherical, platelets, or any other regular or irregular geometry. Particulate composites tend...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870285
EISBN: 978-1-62708-314-0
...Glass-filled epoxy and nylon strength and stiffness Table 10.1 Glass-filled epoxy and nylon strength and stiffness Property Unfilled epoxy Glass-filled epoxy, 35% Unfilled nylon Glass-filled nylon, 35% Glass-filled nylon, 60% Density, g/cc 1.25 1.90 1.15 1.62 1.95...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
...Nominal 17-4 PH composition for wrought and powder alloys Table 10.1 Nominal 17-4 PH composition for wrought and powder alloys Alloy form Composition, wt% Cr Ni Cu Si Mn Nb + Ta C Wrought 15.5 4.5 3.5 0.5 0.4 0.3 0.04 Powder 16.5 4.0 4.0 1 max 1 max 0.3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140047
EISBN: 978-1-62708-335-5
... requirements of the casting in order to promote superficial soundness. The following rules describe the tendency for hydrogen pore formation ( Fig. 5.2 to 5.5 ) ( Ref 1 ): There is a critical or threshold hydrogen value for any composition that must be exceeded for hydrogen porosity to occur...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
... for molten aluminum holding furnaces made from a filament-wound continuous fiber ceramic-matrix composite. Courtesy of Textron Systems. Source: Ref 11.3 Both particulate-reinforced and whisker-reinforced Al 2 O 3 have found use as cutting tool inserts. The incorporation of SiC whiskers (20 to 45...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250139
EISBN: 978-1-62708-345-4
... compositions formulated for specific mechanical and physical properties. Commonly used metal powder grades Table 3 Commonly used metal powder grades MPIF designation Chemistry Applications F-0000 Pure Fe Low strength at high density, soft magnetic properties F-0005 Fe + 0.5% C...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
... to repair than metallic structure. The reinforcing phase provides the strength and stiffness. In most cases, the reinforcement is harder, stronger, and stiffer than the matrix. The reinforcement is usually a fiber or a particulate. Particulate composites have dimensions that are approximately equal...