Skip Nav Destination
Close Modal
Search Results for
particle interlayer-toughening
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-15 of 15
Search Results for particle interlayer-toughening
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Image
Published: 01 November 2010
Fig. 11.12 Fracture morphology in a particle interlayer-toughened thermoset-matrix composite. (a) Strain birefringence in the interlayer particles. Transmitted polarized light, 20× objective. (b) Some of the particles are found to bridge the formed cracks, and some particles are torn
More
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030177
EISBN: 978-1-62708-349-2
... in a variety of aircraft applications. To improve the damage tolerance of composite materials even further, an engineering approach to toughening was used to modify the highly stressed interlayer with either a tougher material or through the use of preformed particles, leading to the third generation...
Abstract
The second-generation composite materials were added to increase the strain to failure of the primary phase and/or create a dispersed second phase, thereby enhancing the fracture toughness of the thermosetting matrix. These matrices offered novel design capabilities for composites in a variety of aircraft applications. To improve the damage tolerance of composite materials even further, an engineering approach to toughening was used to modify the highly stressed interlayer with either a tougher material or through the use of preformed particles, leading to the third generation of composite materials. This chapter discusses the development, processes, application, advantages, and disadvantages of dispersed-phase toughening of thermoset matrices. Information on the processes of particle interlayer toughening of composite materials is also included.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030193
EISBN: 978-1-62708-349-2
... mechanisms, toughened thermoset-matrix composite failure mechanisms, particle interlayer-toughened composite failure mechanisms, and dispersed-phase, rubber-toughened thermoset-matrix composite failure mechanisms. brittle-matrix composites dispersed-phase toughening failure mechanisms fiber...
Abstract
As fiber-reinforced polymeric composites continue to be used in more damage-prone environments, it is necessary to understand the response of these materials when subjected to impact from foreign objects. This chapter provides an overview of the analysis methods for impact-damaged composites. It discusses the causes and effects of various failure mechanisms in composite materials. The failure mechanisms covered are brittle-matrix composite failure, tough-matrix composite failure, thermoplastic-matrix composite failure mechanisms, untoughened thermoset-matrix composite failure mechanisms, toughened thermoset-matrix composite failure mechanisms, particle interlayer-toughened composite failure mechanisms, and dispersed-phase, rubber-toughened thermoset-matrix composite failure mechanisms.
Image
in Introduction—Composite Materials and Optical Microscopy
> Optical Microscopy of Fiber-Reinforced Composites
Published: 01 November 2010
Fig. 1.12 Ultrathin section of a particle-modified interlayer-toughened composite material. Transmitted-light Hoffman modulation contrast, 20× objective
More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030001
EISBN: 978-1-62708-349-2
... optical microscopy particle interlayer toughening polymer matrices prepreg materials Composite Materials The unique and diverse characteristics of composite materials have caused an increase in their utilization worldwide. From featherweight fly fishing rods to high-performance airplane parts...
Abstract
This chapter provides a general description of materials and methods for manufacturing high-performance composites. The materials covered are polymer matrices and prepreg materials and the methods include infusion processes, composite-toughening methods, matrix-toughening methods, and dispersed-phase toughening. In addition, the chapter provides information on interlayer-toughened composites and honeycomb or foam structure composite materials. It also discusses the processes in optical microscopy of composite materials.
Image
in Toughening Methods for Thermoset-Matrix Composites
> Optical Microscopy of Fiber-Reinforced Composites
Published: 01 November 2010
in the interlayer region (i.e., light-gray circles). Slightly uncrossed polarized light, 50× objective. (b) Ultrathin section developed from a particle-modified toughened interlayer composite that was sectioned through the thickness. Transmitted light, Hoffman modulation contrast, 40× objective. (c) Ultrathin
More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.9781627083492
EISBN: 978-1-62708-349-2
Image
in Viewing the Specimen Using Reflected-Light Microscopy
> Optical Microscopy of Fiber-Reinforced Composites
Published: 01 November 2010
Fig. 5.9 Cross sections of an interlayer-toughened composite material. (a) Bright-field illumination, 25× objective. (b) Same view but after the addition of a solvent-based laser dye (Magnaflux Zyglo, Magnaflux Corp.) to the sample surface. The laser dye is preferentially absorbed
More
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870063
EISBN: 978-1-62708-314-0
... alteration, (2) rubber elastomer second phase toughening, (3) thermoplastic elastomer toughening, and (4) interlayering. Network Alteration Since the brittleness of thermosetting polymers is a direct consequence of their high crosslink densities, one method of toughening a thermoset polymer...
Abstract
This chapter discusses the use of thermoset and thermoplastic resins in polymer matrix composites. It begins by explaining how the two classes of polymer differ and how it impacts their use as matrix materials. It then goes on to describe the characteristics of polyester, vinyl ester, epoxy, bismaleimide, cyanate ester, polyimide, and phenolic resins and various toughening methods. The chapter also covers thermoplastic matrix materials and product forms and provides an introduction to the physiochemical tests used to characterize resins and cured laminates.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
... ZrO 2 particles in the elastic stress field of a crack. Source: Ref 10.7 Fig. 10.7 Strength/aging curves obtained by heat treatment at 1300 °C (2370 °F) for various compositions of CaO-partially stabilized zirconia materials. Source: Ref 10.7 Zirconia-toughened ceramics also show...
Abstract
Ceramics normally have high melting temperatures, excellent chemical stability and, due to the absence of conduction electrons, tend to be good electrical and thermal insulators. They are also inherently hard and brittle, and when loaded in tension, have almost no tolerance for flaws. This chapter describes the applications, properties, and behaviors of some of the more widely used structural ceramics, including alumina, aluminum titanate, silicon carbide, silicon nitride, zirconia, zirconia-toughened alumina (ZTA), magnesia-partially stabilized zirconia (Mg-PSZ), and yttria-tetragonal zirconia polycrystalline (Y-TZP). It also provides information on materials selection, design optimization, and joining methods, and covers every step of the ceramic production process.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030159
EISBN: 978-1-62708-349-2
... separated from the matrix as a result of the crack propagation. In this material, the microcracks were found to not propagate into the particle-toughened interlayer region of the composite. Fig. 9.15 Microcracks in the intraply region of an interlayer-toughened carbon fiber composite material...
Abstract
The formation of microcracks in composite materials may arise from static-, dynamic-, impact-, or fatigue-loading situations and also by temperature changes or thermal cycles. This chapter discusses the processes involved in the various methods for the microcrack analysis of composite materials, namely bright-field analysis, polarized-light analysis, contrast dyes analysis, and dark-field analysis. The analysis of microcracked composites using epi-fluorescence is also covered. In addition, the chapter describes the procedures for the determination and recording of microcracks in composite materials.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030089
EISBN: 978-1-62708-349-2
... ). Accordingly, for many composite materials that have been properly polished, the reflected-light DIC image will be similar to an image obtained using reflected-light bright-field illumination. Fig. 5.8 Cross section of a polished interlayer-toughened composite that was lightly etched showing height...
Abstract
The analysis of composite materials using optical microscopy is a process that can be made easy and efficient with only a few contrast methods and preparation techniques. This chapter is intended to provide information that will help an investigator select the appropriate microscopy technique for the specific analysis objectives with a given composite material. The chapter opens with a discussion of macrophotography and microscope alignment, and then goes on to describe various illumination techniques that are useful for specific analysis requirements. These techniques include bright-field illumination, dark-field illumination, polarized-light microscopy, interference and contrast microscopy, and fluorescence microscopy. The chapter also provides a discussion of sample preparation materials such as dyes, etchants, and stains for the analysis of composite materials using optical microscopy.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030115
EISBN: 978-1-62708-349-2
.... Dispersed particles, polymer phases, and short fibers embedded in a matrix or adhesive. A common feature of interest is a toughening phase or particle either dispersed throughout the matrix or in the interlayer region. Large, complex structures with an array of different materials. Frequently...
Abstract
Transmitted-light methods reveal more details of the morphology of fiber-reinforced polymeric composites than are observable using any other available microscopy techniques. This chapter describes the various aspects relating to the selection and preparation of ultrathin-section specimens of fiber-reinforced polymeric composites for examination by transmitted-light microscopy techniques. The preparation steps covered are a selection of the rough section, preparation of the rough section for preliminary mounting, grinding and polishing the primary-mount first surface, mounting the first surface on a glass slide, and preparing the second surface (top surface). The optimization of microscope conditions and analysis of specimens by microscopy techniques are also covered. In addition, examples of composite ultrathin sections that are analyzed using transmitted-light microscopy contrast methods are shown throughout.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390456
EISBN: 978-1-62708-459-8
... are high enough to prevent dynamic recrystallization and if there are no second-phase particles that could initiate microcracks. This means that shear cannot take place in an infinitely narrow plane; instead, a more diffused primary shear zone is found ( Fig. 13.3 ). The chip becomes thicker...
Abstract
In contrast to most plastic deformation processes, the shape of a machined component is not uniquely defined by the tooling. Instead, it is affected by complex interactions between tool geometry, material properties, and frictional stresses and is further complicated by tool wear. This chapter covers the mechanics and tribology of metal cutting processes. It discusses the factors that influence chip formation, including tool and process geometry, cutting forces and speeds, temperature, and stress distribution. It reviews the causes and effects of tool wear and explains how to predict and extend the life of cutting tools based on the material of construction, the use of cutting fluids, and the means of lubrication. It presents various methods for evaluating workpiece materials, chip formation, wear, and surface finish in cutting processes such as turning, milling, and drilling. It also discusses the mechanics and tribology of surface grinding and other forms of abrasive machining.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5
Abstract
This article describes key processing methods and related design, manufacturing, and application considerations for plastic parts and includes a discussion on materials and process selection methodology for plastics. The discussion covers the primary plastic processing methods and how each process influences part design and the properties of the plastic part. It also includes a brief description of functional requirements in process selection; an overview of various process effects and how they affect the functions and properties of the part; and the selection of processes for size, shape, and design detail factors.