EISBN: 978-1-62708-260-0
... determines that a certain standard will not scratch the sample but the next harder standard will. Scratch tests can also be performed with an indenter that is run across a sample, producing a plowing action. The scratch width is the measure of hardness. Static indentation tests A ball, cone, or pyramid...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610025
EISBN: 978-1-62708-303-4
... indentor that then penetrates the surface of the specimen. The size of the resulting indentation, a measure of the permanent deformation that the material undergoes during the test, relates to the material hardness. A small indentation indicates high hardness. When the load is divided by the indentation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110563
EISBN: 978-1-62708-247-1
... identifying them. The chapter also provides information on the testing of MEMS devices. It covers the two common challenges in sample preparation for MEMS: decapping, or opening up the package, without disturbing the MEMS elements; and removing MEMS elements for analysis. Finally, the chapter discusses the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090341
EISBN: 978-1-62708-266-2
.... and Wiederhorn S.M. , Proof Testing of Ceramic Materials—An Analytical Basis for Failure Prediction , Int. J. Fract. Mech. , Vol 10 , 1974 , p 379 10.1007/BF00035499 14.19 Freiman S.W. , Baker T.L. , and Wachtman J.B. Jr. , A Computerized Fracture Mechanics Data...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.9781627082914
EISBN: 978-1-62708-291-4
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.9781627082617
EISBN: 978-1-62708-261-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.9781627082600
EISBN: 978-1-62708-260-0
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630035
EISBN: 978-1-62708-270-9
... Electric, 1977 7. Control of Shrinkage and Distortion , Design of Welded Structures , James F. Lincoln Arc Welding Foundation , 1966 , section 7.7 8. Barrett C. and Massalski T.B. , Structure of Metals , 3rd ed. , McGraw-Hill , 1966 9. “ Test Strip, Holder, and Gage for...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480265
EISBN: 978-1-62708-318-8
.... Soft-vacuum techniques have been used, and there is some contamination, but the extent is uncertain. Electron beam welds have high depth-to-width ratios. Such narrow welds cause less distortion than is obtained with GMAW, GTAW, and PAW. Conventional equipment is used to weld titanium and its alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500019
EISBN: 978-1-62708-317-1
...). Source: Ref 2.12 Table 2.3 Test conditions for V-die bending tests (geometry in Fig. 2.14 ) Testing parameters Description Sheet material DP780 Sheet thickness, width and length, mm (in.) 1 × 60 × 210 (0.04 × 2.4 × 8.3) Sheet orientation Rolling and transverse direction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290137
EISBN: 978-1-62708-306-5
... weld zone. When metallurgical reactions occur, they can either benefit or adversely affect the properties of the joint. From a metallurgical perspective, the application of both fusion welding and solid-state welding processes must be evaluated using appropriate weldability testing methods for their...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.9781627083164
EISBN: 978-1-62708-316-4
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870099
EISBN: 978-1-62708-299-0
... Stress-Corrosion Cracking of Metals, American Society for Testing and Materials and American Institute of Mining and Metallurgical Engineers , 1945 , p 323 10.1520/STP42581S 7. Sprowls D.O. and Brown R.H. , Stress-Corrosion Mechanisms for Aluminum Alloys , Fundamental Aspects of...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.9781627082587
EISBN: 978-1-62708-258-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110067
EISBN: 978-1-62708-247-1
... signature analysis and GHz-SAM. GHz -SAM integrated circuit inspection scanning acoustic microscope semiconductor packages spectral signature analysis References [1] Moore T. M. , in International Symposium of Test and Failure Analysis , A. International, Ed...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540121
EISBN: 978-1-62708-309-6
... McGaw M.A. , Fatigue, Creep Fatigue, and Thermomechanical Fatigue Life Testing , ASM Handbook , Vol 8 , Mechanical Testing and Evaluation , ASM International , 2000 , p 686 – 716 10.31399/asm.hb.v08.a0003314 3.28. Socie D.F. , Morrow J. , and Chen W.C. , A Procedure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560125
EISBN: 978-1-62708-291-4
... ferrite in the pearlite colony is etched to a lower level than the cementite and because the cementite lamellae are usually inclined to the section plane, as illustrated in Fig. 6.6 (Part 1) (d) . The result is that the observed width of the cementite plates is a projected width much greater than the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130177
EISBN: 978-1-62708-284-6
... that are four pitch and coarser. Use hot oil quenching on fine pitch gears. Case hardness of the finished gear should be 60 HRC or greater. If possible, test each gear for partial decarburization and/or upper transformation products. To minimize distortion and to permit quieter operation...