... chapter also covers quantitative fractography, fracture surface topography analysis, and the use of oxide dating as well as fault tree and failure modes and effects analysis (FMEA) and computational techniques. fault tree analysis fracture surface topography analysis oxide dating quantitative...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410009
EISBN: 978-1-62708-265-5
... This chapter traces the history of steelmaking over three millennia, from the discovery of martensite in a mining tool dating from the twelfth century B.C. to the nineteenth century development of the Bessemer and Siemens processes. It also describes the work of early metallographers who...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230131
EISBN: 978-1-62708-298-3
... Abstract This chapter discusses the properties and applications of beryllium intermetallic compounds. It describes the crystal structure of key beryllides, the metals they contain, and important properties such as high-temperature strength, thermal conductivity and expansion, oxidation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090317
EISBN: 978-1-62708-266-2
... Abstract Uranium alloys are used in applications requiring dense metals, but they have little resistance to oxidation and corrosion and are susceptible to environmentally assisted cracking, particularly when processed to high strength levels. This chapter describes the conditions under which...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090271
EISBN: 978-1-62708-266-2
... composition, designation, and grade of nearly two dozen commercial titanium alloys and the different types of media (including oxidizers, organic compounds, hot salt, and liquid metal) in which SCC has been observed. It discusses the mechanical and metallurgical factors that influence SCC behavior and...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
..., continuous fiber ceramic composites, and carbon-carbon composites. It also describes a number of ceramic-matrix composite processing methods, including cold pressing and sintering, hot pressing, reaction bonding, directed metal oxidation, and liquid, vapor, and polymer infiltration. ceramic-matrix...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000147
EISBN: 978-1-62708-312-6
... Abstract This chapter describes a number of corrosion testing methods for sintered stainless steels, including immersion, salt spray, and electrochemical tests, ferric chloride and ferroxyl tests, and elevated-temperature oxidation resistance tests. It also provides corrosion resistance and...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290251
EISBN: 978-1-62708-319-5
... additive manufacturing, including bound-metal deposition and fused-filament fabrication: oxidation-resistant high-temperature alloys, anisotropic structures, submicrometer-scale structures, surface hard materials, and artist metallic clays. Some of the advances discussed include the developments in process...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
... corrosion resistance of aluminum oxide/aluminum composites is highly dependent on the bonding compound formed at the fiber/matrix interface. To date, no severe corrosion problems have been identified with Al 2 O 3 /Al-Li composites. The corrosion behavior of cast Al-2%Mg, Al-2%Mg-3.5% mica and Al-4%Cu...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030096
EISBN: 978-1-62708-282-2
... austenitic stainless steels as well as several forms of corrosion associated with welding. The effects of gas-tungsten arc weld shielding gas composition and heat-tint oxides on corrosion resistance are then covered. Microbiological corrosion of butt welds in water tanks is also illustrated. In addition, the...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280135
EISBN: 978-1-62708-267-9
... desired objectives of quenching, annealing, and aging along with the associated risks of surface damage caused by oxidation, carbon pickup, alloy depletion, intergranular attack, and environmental contaminants. It also discusses heat treatment atmospheres, furnace and fixturing requirements, and practical...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720293
EISBN: 978-1-62708-305-8
... inspection. Casting defects including porosity, oxide films, inclusions, hot tears, metal penetration, and surface defects are reviewed. Liquid penetrant inspection, magnetic particle inspection, eddy current inspection, radiographic inspection, ultrasonic inspection, and leak testing for castings are...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870573
EISBN: 978-1-62708-314-0
... and pyrolysis, chemical vapor infiltration, directed metal oxidation, and liquid silicon infiltration. ceramic matrix composites chemical vapor infiltration directed metal oxidation liquid silicon infiltration polymer infiltration and pyrolysis slurry infiltration MONOLITHIC CERAMIC...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110351
EISBN: 978-1-62708-247-1
... tools for first silicon debug. The etching capabilities of circuit edit FIB tools are then discussed, providing information on chemistry assisted etching in silicon oxides and low-k dielectrics. The chapter also discusses the requirements and procedures involved in edit operation: high aspect ratio...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.9781627082617
EISBN: 978-1-62708-261-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110447
EISBN: 978-1-62708-247-1
... root cause of a physical failure and implement, when possible early detection methods. One example is solderability failure investigated with Auger found to correlate with oxide thickness on the solder ball. A faster screening method with SEM-EDX to determine oxide thickness is proposed as a more...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060073
EISBN: 978-1-62708-261-7
...) to realize that iron could be produced in simple furnaces by direct carbon reduction of the oxide ore. The exact date of this first intentional reduction of iron cannot be established, but it is certain that the making and shaping of iron was widespread in Egypt by 1500 B.C. For the next 3000 years...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240583
EISBN: 978-1-62708-251-8
... vapor pressures, and relatively low thermal expansions compared to other metals. Unfortunately, despite their high-temperature resistance, all of them oxidize severely at relatively low temperatures and therefore require oxidation-resistant coatings for elevated-temperature use. Protective coating...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310147
EISBN: 978-1-62708-286-0
... stabilizing alloy, titanium, is too readily oxidized for normal foundry practice to avoid the loss of this essential element. Thus, the casting alloys listed in Tables 1 and 2 ( Ref 1 ) are recognizable as approximate counterparts of the co-listed wrought alloys (AISI grade). This cross reference to...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730081
EISBN: 978-1-62708-283-9
... fullerenes glasses graphite nanotubes Portland cement CERAMICS ARE NONMETALLIC, inorganic materials. Most ceramics can be grouped into several distinct groups. One group consists of crystalline compounds such as magnesium oxide, aluminum oxide, and boron nitride. Glasses form a second group. There...