... may act to diminish the amount (and the effect) of water absorption. Water absorption may be viewed as an osmotic phenomenon; that is, the amount of water absorption is governed by the thermodynamic activity of water either in solution or in the vapor phase ( Ref 1 – 3 ). Examples of this behavior are...