Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270180
EISBN: 978-1-62708-301-0
... vulnerability because of the way they were mounted. A sketch showing the correct mounting configuration is included in the report. fatigue failure nose undercarriage retraction jack SEM fractography An aircraft had an incident when the nose landing gear got retracted on landing roll. Two...