- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 189 Search Results for
nondestructive evaluation methods
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720393
EISBN: 978-1-62708-305-8
... evaluation methods to flaw detection in P/M parts. The nondestructive evaluation methods covered are mechanical proof testing, metallography, liquid penetrant crack detection, filtered particle crack detection, magnetic particle crack inspection, direct current resistivity testing, x-ray radiography...
Abstract
Fabricated powder metallurgy (P/M) parts are evaluated and tested at several stages during manufacturing for part acceptance and process control. The various types of tests included are dimensional evaluation, density measurements, hardness testing, mechanical testing, and nondestructive testing. This chapter is a detailed account of these testing methods. It describes the four most common types of defects in P/M parts, namely ejection cracks, density variations, microlaminations, and poor sintering. The chapter discusses the capabilities and limitations of various nondestructive evaluation methods to flaw detection in P/M parts. The nondestructive evaluation methods covered are mechanical proof testing, metallography, liquid penetrant crack detection, filtered particle crack detection, magnetic particle crack inspection, direct current resistivity testing, x-ray radiography, computed tomography, gamma-ray density determination, and ultrasonic techniques.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910475
EISBN: 978-1-62708-250-1
... Abstract This chapter discusses the techniques applicable to the diagnosis of corrosion failures, including visual and microscopic examination of corroded surfaces and microstructure; chemical analysis of the metal, corrosion products, and bulk environment; nondestructive evaluation methods...
Abstract
This chapter discusses the techniques applicable to the diagnosis of corrosion failures, including visual and microscopic examination of corroded surfaces and microstructure; chemical analysis of the metal, corrosion products, and bulk environment; nondestructive evaluation methods; corrosion testing techniques; and mechanical testing techniques. A guide to investigative techniques used in corrosion failure analysis is provided in a table, describing the advantages and limitations of each technique. The principal stages of the investigation and analysis of corrosion failures discussed in the chapter are: collection of background information and sampling; preliminary laboratory examination; detailed metallographic and fractographic examinations; chemical analysis of corrosion products and bulk materials; corrosion testing for quality control; mechanical testing for quality control; and analysis of results and report writing.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720001
EISBN: 978-1-62708-305-8
... (Philadelphia, Pennsylvania), and in Nondestructive Evaluation and Quality Control , Volume 17, ASM Handbook. The relative uses and merits of various nondestructive testing methods Table 2 The relative uses and merits of various nondestructive testing methods  Test method Ultrasonics X-ray...
Abstract
This chapter provides an overview of the various inspection methods used with metals and alloys, namely visual inspection, coordinate measuring machines, machine vision, hardness testing, tensile testing, chemical analysis, metallography, and nondestructive testing. The nondestructive testing methods discussed are liquid penetrant inspection, magnetic particle inspection, eddy current inspection, radiographic inspection, and ultrasonic testing.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930085
EISBN: 978-1-62708-359-1
... Abstract Welded joints in any component or structure require a thorough inspection. The role of nondestructive evaluation (NDE) in the inspection of welds is very important, and the technology has become highly developed as a result. This article describes the applications, methods, evaluation...
Abstract
Welded joints in any component or structure require a thorough inspection. The role of nondestructive evaluation (NDE) in the inspection of welds is very important, and the technology has become highly developed as a result. This article describes the applications, methods, evaluation procedures, performance, and limitations of NDE. It provides information on the training and certification of NDE operators, evaluation of test results, and guidance to method selection. Typical examples of various NDE methods for welds are also described.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270019
EISBN: 978-1-62708-301-0
..., and pressure vessels. 3.8.1 Conventional Nondestructive Evaluation Techniques Visual Examination Visual examination is an easy and widely used method for detecting surface flaws in a variety of components. Visual examination is carried out with the naked eye and with instruments such as borescopes...
Abstract
This chapter discusses the basic steps of a failure investigation. It explains that the first step is to gather and document information about the failed component and its operating history. It advises investigators to visit the failure site as soon as possible to record damages and collect test specimens for subsequent examination and chemical analysis. It also discusses the role of mechanical property testing, the use of nondestructive evaluation, and the final step of generating a report.
Book Chapter
Book: Corrosion of Weldments
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820203
EISBN: 978-1-62708-339-3
... Abstract This chapter addresses in-service monitoring and corrosion testing of weldments. Three categories of corrosion monitoring are discussed: direct testing of coupons, electrochemical techniques, and nondestructive testing techniques. The majority of the test methods for evaluating...
Abstract
This chapter addresses in-service monitoring and corrosion testing of weldments. Three categories of corrosion monitoring are discussed: direct testing of coupons, electrochemical techniques, and nondestructive testing techniques. The majority of the test methods for evaluating corrosion of weldments are used to assess intergranular corrosion of stainless steels and high-nickel alloys. Other applicable tests evaluate pitting and crevice corrosion, stress-corrosion cracking, and microbiologically influenced corrosion. Each of these test methods is reviewed in this chapter.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930039
EISBN: 978-1-62708-359-1
... Abstract This article reviews nondestructive and destructive test methods used to characterize welds. The first process of characterization discussed involves information that may be obtained by direct visual inspection and measurement of the weld. An overview of nondestructive evaluation...
Abstract
This article reviews nondestructive and destructive test methods used to characterize welds. The first process of characterization discussed involves information that may be obtained by direct visual inspection and measurement of the weld. An overview of nondestructive evaluation is included that encompasses techniques used to characterize the locations and structure of internal and surface defects, including radiography, ultrasonic testing, and liquid penetrant inspection. The next group of characterization procedures discussed is destructive tests, requiring the removal of specimens from the weld. The third component of weld characterization is the measurement of mechanical and corrosion properties. Following the discussion on the characterization procedures, the second part of this article provides examples of how two particular welds were characterized according to these procedures.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090359
EISBN: 978-1-62708-266-2
... Abstract This chapter describes how ultrasonic testing came to be a viable method for evaluating intergranular stress-corrosion cracking (SCC) in large-diameter stainless steel pipe welds in boiling water reactor service. Intergranular SCC can be difficult to detect using nondestructive...
Abstract
This chapter describes how ultrasonic testing came to be a viable method for evaluating intergranular stress-corrosion cracking (SCC) in large-diameter stainless steel pipe welds in boiling water reactor service. Intergranular SCC can be difficult to detect using nondestructive evaluation (NDE) techniques because of its treelike branching pattern and its location in the heat-affected zone within the weld. As the chapter explains, by optimizing excitation and reflected waveforms, switching to dual-element sensing, properly orienting the scanning path, and using crack-tip diffraction and amplitude-drop techniques, the height, length, and location of intergranular cracks can be accurately determined anywhere along the walls of the pipe as well as in weld areas.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720345
EISBN: 978-1-62708-305-8
... Abstract Wrought tubular products are nondestructively inspected chiefly by eddy current techniques (including the magnetic flux leakage technique) and by ultrasonic techniques. The methods discussed in this chapter include eddy current inspection, flux leakage inspection, ultrasonic inspection...
Abstract
Wrought tubular products are nondestructively inspected chiefly by eddy current techniques (including the magnetic flux leakage technique) and by ultrasonic techniques. The methods discussed in this chapter include eddy current inspection, flux leakage inspection, ultrasonic inspection, magnetic particle inspection, liquid penetrant inspection, and radiographic inspection of resistance welded tubular products, seamless steel tubular products, and nonferrous tubular products. This chapter discusses the fundamental factors that should be considered in selecting a nondestructive inspection method and in selecting from among the commercially available inspection equipment. The factors covered are product characteristics, nature of the flaws, extraneous variables, rate of inspection, end effect, mill versus laboratory inspection, specification requirements, equipment costs, and operating costs.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870333
EISBN: 978-1-62708-314-0
... Abstract This chapter discusses the use of nondestructive inspection methods, including visual, ultrasonic, radiographic, and thermographic techniques, and the types of flaws and damages they can reveal in composite parts and assemblies. It describes the basic principles behind each method...
Abstract
This chapter discusses the use of nondestructive inspection methods, including visual, ultrasonic, radiographic, and thermographic techniques, and the types of flaws and damages they can reveal in composite parts and assemblies. It describes the basic principles behind each method along with best practices and procedures.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090419
EISBN: 978-1-62708-266-2
... Abstract This chapter describes nondestructive evaluation (NDE) test methods and their relative effectiveness for diagnosing the cause of stress-corrosion cracking (SCC) service failures. It discusses procedures for analyzing various types of damage in carbon and low-alloy steels, high-strength...
Abstract
This chapter describes nondestructive evaluation (NDE) test methods and their relative effectiveness for diagnosing the cause of stress-corrosion cracking (SCC) service failures. It discusses procedures for analyzing various types of damage in carbon and low-alloy steels, high-strength low-alloy steels, hardenable stainless steels, austenitic stainless steels, copper-base alloys, titanium and titanium alloys, aluminum and aluminum alloys, and nickel and nickel alloys. It identifies material-environment combinations where SCC is known to occur, provides guidelines on how to characterize cracking and fracture damage, and explains what to look for during macroscopic and microscopic examinations as well as chemical and metallographic analyses. It also includes nearly a dozen case studies investigating SCC failures in various materials.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060149
EISBN: 978-1-62708-261-7
... Abstract This chapter explains how metallography and hardness testing are used to evaluate the quality and condition of metal products. It also discusses the use of tensile testing, fracture toughness and impact testing, fatigue testing, and nondestructive test methods including ultrasonic, x...
Abstract
This chapter explains how metallography and hardness testing are used to evaluate the quality and condition of metal products. It also discusses the use of tensile testing, fracture toughness and impact testing, fatigue testing, and nondestructive test methods including ultrasonic, x-ray, and eddy current testing.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720321
EISBN: 978-1-62708-305-8
... Abstract This chapter focuses on the inspection of steel bars for the detection and evaluation of flaws. The principles involved also apply, for the most part, to the inspection of steel wire. The nondestructive inspection methods discussed include magnetic particle inspection, liquid penetrant...
Abstract
This chapter focuses on the inspection of steel bars for the detection and evaluation of flaws. The principles involved also apply, for the most part, to the inspection of steel wire. The nondestructive inspection methods discussed include magnetic particle inspection, liquid penetrant inspection, ultrasonic inspection, and electromagnetic inspection. Eddy current and magnetic permeability are also covered.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050245
EISBN: 978-1-62708-311-9
... Abstract This chapter discusses the methods and procedures used for inspecting induction-hardened parts. It provides information on hardness and case depth measurements, nondestructive testing and surface analysis, the effect of various hardening errors, and relevant test standards. case...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720411
EISBN: 978-1-62708-305-8
... to be inspected, the detection capabilities of the inspection method, the level of joint quality required, and economic considerations. Regardless of the method selected, established standards must be followed to obtain valid inspection results. In general, nondestructive inspection (NDI) methods...
Abstract
Weldments made by the various welding processes may contain discontinuities that are characteristic of that process. This chapter discusses the different welding processes as well as the discontinuities typical of each process. It provides a detailed discussion on the methods of nondestructive inspection of weldments including visual inspection, liquid penetrant inspection, magnetic particle inspection, radiographic inspection, ultrasonic inspection, leak testing, and eddy current and electric current perturbation inspection. The chapter also describes the properties of brazing filler metals and the types of flaws exhibited by brazed joints.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720365
EISBN: 978-1-62708-305-8
... by the forging operation and the principal factors that influence the selection of a nondestructive inspection method for forgings. eddy current inspection forgings liquid penetrant inspection magnetic particle inspection radiographic inspection ultrasonic inspection visual inspection...
Abstract
In forgings of both ferrous and nonferrous metals, the flaws that most often occur are caused by conditions that exist in the ingot, by subsequent hot working of the ingot or the billet, and by hot or cold working during forging. The inspection methods most commonly used to detect these flaws include visual, magnetic particle, liquid penetrant, ultrasonic, eddy current, and radiographic inspection. This chapter provides a detailed discussion on the characteristics, process steps, applications, advantages, and limitations of these methods. It also describes the flaws caused by the forging operation and the principal factors that influence the selection of a nondestructive inspection method for forgings.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430409
EISBN: 978-1-62708-253-2
... a vital role in RLA. Measurement of oxide scale thickness is an indirect method of evaluating the status of creep damage. Oxide scale thickness can be determined destructively or nondestructively. A destructive method of scale thickness measurement is based on the deposit weight density approach...
Abstract
The power generating industry has become proficient at predicting how long a component will last under a given set of operating conditions. This chapter explains how such predictions are made in the case of boiler tubes. It identifies critical damage mechanisms, progressive failure pathways, and relevant test and measurement procedures. It describes life assessment methods based on hardness, wall thickness, scale formation, microstructure, and creep. It also includes a case study on the determination of the residual life of a secondary superheater tube.
Book Chapter
Book: Systems Failure Analysis
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780093
EISBN: 978-1-62708-268-6
... inspection environmental approaches failure mode assessment and assignment material characteristics mechanical approaches nondestructive test approaches optical approaches AFTER THE FAULT-TREE, a failure-cause identification method has identified potential failure causes and the failure analysis...
Abstract
After the fault-tree, a failure-cause identification method has identified potential failure causes and the failure analysis team has prepared a failure mode assessment and assignment (FMA&A). The team knows specifically what to search for when examining components and subassemblies from the failed system. There are numerous techniques and technologies available for examining and analyzing components and subassemblies, which are categorized as follows: optical approaches, dimensional inspection and related approaches, nondestructive test approaches, mechanical and environmental approaches, and chemical and composition analysis for assessing material characteristics. This chapter is a detailed account of the working principle and the steps involved in these techniques and technologies.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200065
EISBN: 978-1-62708-354-6
... and brazing qualifications MSS-SP-55 Quality standard for steel castings for valves, flanges and fittings and other piping components-visual method ASNT SNT-TC-1A Recommended practice for nondestructive testing personnel qualification and certification MIL-STD-410 Nondestructive testing personnel...
Abstract
This chapter discusses the role of standards and specifications for steel castings. It defines specifications and discusses how certification, testing, examination, methods, practices, procedures, compositions, properties, facilities, statistical process control, and documentation relate to codes and standards. The chapter describes processes involved in the selection of specifications for steel castings. Further, it provides information on the cost of specifications.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720293
EISBN: 978-1-62708-305-8
... Discontinuities The principal nondestructive methods used for detecting internal discontinuities in castings are radiography, ultrasonic inspection, and eddy current inspection. Of these methods, radiography is the most highly developed technique for detailed inspection; it can provide a pictorial...
Abstract
The inspection of castings normally involves checking for shape and dimensions, coupled with aided and unaided visual inspection for external discontinuities and surface quality. This chapter discusses methods for determining surface quality, internal discontinuities, and dimensional inspection. Casting defects including porosity, oxide films, inclusions, hot tears, metal penetration, and surface defects are reviewed. Liquid penetrant inspection, magnetic particle inspection, eddy current inspection, radiographic inspection, ultrasonic inspection, and leak testing for castings are discussed. The chapter provides information on the procedures involved in the inspection of castings that are limited to visual and dimensional inspections, weight testing, and hardness testing. It also discusses the use of computer equipment in foundry inspection operations.