... as ultrasonics or x-ray, thermographic inspection is a relatively fast, noncontact, single-sided process that has a wide coverage area. It can be used to detect delaminations, impact damage, water ingression into honeycomb, inclusions, and density variations. In thermography ( Fig. 12.17 ), it is first necessary...