Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110563
EISBN: 978-1-62708-247-1
...-L , Lin J. , “ A novel non-destructive approach to deprocess the sealing cap from MEMS device for failure analysis ”, ISTFA 2010 Proc 36th Int'l Symp. for Testing and Failure Analysis , Addison, Texas , 2010 . [77] Tan H. , Moyal E. , Yap H.H. , Zhao Y.Z. , He...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110447
EISBN: 978-1-62708-247-1
... is a destructive technique this means that the contribution of those secondary ions to the spectrum originating from already bombarded surface areas to the spectrum must be negligible. This quasi non-destructive surface analysis can be achieved by the application of very low primary ion dose densities. Surface...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820203
EISBN: 978-1-62708-339-3
... Abstract This chapter addresses in-service monitoring and corrosion testing of weldments. Three categories of corrosion monitoring are discussed: direct testing of coupons, electrochemical techniques, and nondestructive testing techniques. The majority of the test methods for evaluating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090221
EISBN: 978-1-62708-266-2
.... , Evaluation of Stress Corrosion Cracking of Alpha-Brass in Non-Ammoniac Environments , Corrosion , Vol 46 ( No. 9 ), 1990 , p 717 10.5006/1.3585173 7.16 Pugh E.N. and Westwood A.R.C. , Complex Ions and Stress-Corrosion Cracking in Alpha Brass , Philos. Mag. , Vol 13 ( No. 121...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030005
EISBN: 978-1-62708-282-2
... Image Analysis with Weight Change Measurements for Assessing Non-Uniform Attack during Corrosion Testing of Aluminum , Br. Corros. J. , Vol 28 ( No. 2 ), 1993 , p 103 – 106 10.1179/000705993798268115 129. Dean W.S. , Classifying Atmospheric Corrosivity—A Challenge for ISO , Mater...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870075
EISBN: 978-1-62708-299-0
... alloy. The thickness of the cladding layer is usually less than 10% of the overall thickness of the product. Cladding alloys are generally of the non-heat-treatable type, although heat-treatable alloys are sometimes used for higher strength. For mechanical design calculations, such sacrificial...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110545
EISBN: 978-1-62708-247-1
... very well with other techniques for measuring carrier lifetime. [5] Figure 9 Carrier lifetime measurements obtained with conductivity (left) and photoluminescence (right). Variations in carrier lifetime occur from the non-uniform distribution of impurities. From Berman et al. [5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090367
EISBN: 978-1-62708-266-2
.... , Statistical Treatment of Non-normally Distributed Stress-Corrosion Data , Handbook on Corrosion Testing and Evaluation , Ailor W.H. , Ed., John Wiley and Sons , 1971 , p 87 – 100 17.76 Brown B.F. , Chapter 1, Stress Corrosion Cracking in High Strength Steels and in Titanium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870045
EISBN: 978-1-62708-299-0
...) and the advanced electrochemical techniques. The electrochemical techniques used to investigate pitting corrosion include the simple monitoring of corrosion potential and its fluctuation with time due to pitting attack, potentiostatic tests, potentiodynamic tests (at relatively slow scan rates of a few millivolts...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110587
EISBN: 978-1-62708-247-1
..., confirming the reported failure mode (i.e. leakage or short, open circuit, etc.) is the next important step. Next non-destructive internal and external examinations by optical microscopy, X-ray, C-mode Scanning Acoustic Microscopy (C-SAM) and so on, should be performed. Performing basic electrical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... conversion coating corrosion monitoring corrosion prevention methods electrochemical methods electroplated coating organic coating porcelain enameling THE INCREASE IN COST attributed to corrosion problems in the United States has been significant—from $5.5 billion in 1947 to a more recent estimate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.9781627082617
EISBN: 978-1-62708-261-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030074
EISBN: 978-1-62708-282-2
... , 1990 2. Gleeson B. , High-Temperature Corrosion of Metallic Alloys and Coatings , Corrosion and Environmental Degradation , Vol II , Wiley-VCH , 2000 , p 173 10.1002/9783527619306.ch14 3. Rebak R.B. , Corrosion of Non-Ferrous Alloys, Part I: Nickel-, Cobalt-, Copper...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030045
EISBN: 978-1-62708-282-2
.... , and White D.C. , The Role of Oceanospirillium Exopolymer in Marine Copper Corrosion , Proc. 1995 Intl. Conf. on MIC , Angel P. et al. , Ed., NACE International , 1995 , p 74 – 1 102. Videla H.A. , Biocorrosion of Non-Ferrous Metal Surfaces , Biofouling and Biocorrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870135
EISBN: 978-1-62708-299-0
.... McKee A.B. and Binger W.W. , Corrosion , Vol 13 , 1957 , p 786t 10.5006/0010-9312-13.12.20 Selected References Atmospheric Corrosion • STP 175 , Symposium on Atmospheric Corrosion of Non-ferrous Metals , ASTM , 1956 10.1520/STP175-EB • STP 435 , Metal...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290009
EISBN: 978-1-62708-319-5
... area may not flow. Accordingly, these are labeled non-free-flowing. For smaller powders, the funnel diameter is enlarged to 5 mm (0.2 in.) (Carney funnel). However, even with this larger opening, submicrometer-sized powders still do not flow. Therefore, the Scott device is applied to cascade powders...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460185
EISBN: 978-1-62708-285-3
... Metallic and Non-Metallic Substrates ,” University of Nottingham , 2005 7.8 Bala N. , Singh H. , and Prakash S. , High-Temperature Oxidation Studies of Cold-Sprayed Ni-20Cr and Ni-50Cr Coatings on SAE 213-T22 Boiler Steel , Appl. Surf. Sci. , Vol 255 ( No. 15 ), 2009 , p 6862...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
... compromises. The importance of assembly as a design constraint has resulted in a greatly increased emphasis on assembly in the design process. Design and manufacturing practice now focuses on ensuring that parts conform to specifications and that variability and randomness are minimized, and on making non...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230523
EISBN: 978-1-62708-298-3
... Alloy Powders , Surf. Interface Anal. , Vol 31 ( No. 7 ), p 599 – 608 10.1002/sia.1087 Anisimov A. , Frolov V. , Komarov V. , Mazul I. , Moszherin S. , Pepekin G. , and Pirogov A. , 1997 . Beryllium Armour Produced by Evaporation-Condensation Technique...