1-20 of 25 Search Results for

ndt

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050245
EISBN: 978-1-62708-311-9
... and Abnormal Characteristics of Induction Hardened Components , Induction Heating and Heat Treatment , Vol 4C , ASM Handbook , ASM International , 2014 , p 228 – 240 10.31399/asm.hb.v04c.a0005871 Standards Test Equipment Nondestructive Testing (NDT) Inspection for Induction Hardness...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720001
EISBN: 978-1-62708-305-8
... requirements and standards for determining whether the item or activity is in line with these targets. Some inspection methods are destructive; however, inspections are usually nondestructive. Nondestructive examination (NDE), or nondestructive testing (NDT), are a number of technologies used to analyze...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060149
EISBN: 978-1-62708-261-7
... of Metallic Materials , ASTM E 399 , ASTM International 7.10 Standard Practice for Strain-Controlled Fatigue Testing , ASTM E 606 , ASTM International 7.11 Cartz L. , Quality Control and NDT , Nondestructive Testing , ASM International , 1995 Stress-Life Fatigue Testing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050281
EISBN: 978-1-62708-311-9
... Cooling water Pressure switch for low pressure if pressure boosting pump is used Workpiece position correct in coil Fixture Rotation detection Means of lubrication Machine shutdown on fault and part rejection process NDT quality verification if possible Verification...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490021
EISBN: 978-1-62708-340-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430409
EISBN: 978-1-62708-253-2
.... The results of these tests are systematically analyzed and based on the findings and calculations, the remaining life of the tubes is calculated. During RLA, a wide range of destructive and nondestructive tests are carried out for health assessment of the tubes. Nondestructive testing (NDT) techniques...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130043
EISBN: 978-1-62708-284-6
... criterion for the transition temperature is the nil-ductility temperature (NDT). The NDT is the temperature where fracture becomes 100% cleavage, and there is essentially no plastic deformation. Changes in the NDT can be produced by changes in microstructure and chemistry. The largest change can...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
... expensive Structural adhesives somewhat expensive Production rate Can be very fast Automatic processes quite fast Manual processes slow. Automated processes can be very fast. Seconds to hours depending on type Quality assurance Nondestructive testing (NDT) methods well established NDT...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820203
EISBN: 978-1-62708-339-3
...) Electrochemical Impedance Spectroscopy (EIS) Electrochemical Noise (EN) Corrosion Potential Ultrasonic Thickness Measurements Ultrasonic Testing of Welds in the ByPass Lines of a Boiling Water Reactor Other NDT Techniques Tests for Stainless Steels and Nickel-Base Alloys ASTM G 48 ASTM G...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120047
EISBN: 978-1-62708-269-3
..., and fairly complex shapes are produced. Limited machining envelopes are incorporated in the design of the cans or dies used, but the requirements of NDT limit the extent to which near net shape (NNS) can be approached. Practical considerations of component complexity also affect the final compact volume...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130351
EISBN: 978-1-62708-284-6
.... 66 Ultrasonic signal responses from the manufactured reference standards Fig. 67 Ultrasonic signal responses for each bolt inspected Fig. 68 Ultraviolet light photographs of magnetic particle indications for each bolt inspected. NDT, nondestructive testing Fig. 69...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610263
EISBN: 978-1-62708-303-4
... of different improvement techniques. Source: Ref 16 Fig. 27 Pellini’s fracture analysis diagram. NDT, nil-ductility temperature. Source: Ref 16 Fig. 28 Ductile-to-brittle transition curves for a variety of materials. Source: Ref 16 Fig. 16 Geometry parameters that affect...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030360
EISBN: 978-1-62708-282-2
...—Ultrasonic Examination of Welded Joints ,” 1998 18. BS EN 473, “ Non-Destructive Testing—Qualification and Certification of NDT Personnel: General Principles ,” DIN EN 473, 2000 19. “ PANI Programme for the Assessment of NDT in Industry ,” AEA Technology, Health and Safety Executive (UK) HSE...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870201
EISBN: 978-1-62708-314-0
... fabrication, overbleeding can and does occur because of leaky damming systems or leaky matched die molds. The analysis of these cured laminates included nondestructive testing (NDT), thickness measurements, resin content determinations, and materiallographic cross sections. The resin contents and thickness...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120039
EISBN: 978-1-62708-269-3
... of conventional risering is virtually impossible. Therefore, in the interest of maximum product integrity and mechanical properties, virtually all aerospace castings are hot iso-statically pressed. HIP enables castings to meet aerospace nondestructive inspection standards (NDT). Gross section defects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720393
EISBN: 978-1-62708-305-8
... manufacturing for part acceptance and process control. The various types of tests included are: Dimensional evaluation Density measurements Hardness testing Mechanical testing NDT Dimensional Evaluation Density Measurement Apparent Hardness and Microhardness Mechanical Testing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.t51180151
EISBN: 978-1-62708-256-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110067
EISBN: 978-1-62708-247-1
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720267
EISBN: 978-1-62708-305-8
... in nondestructive testing (NDT) are listed in Table 3 . Common ultrasonic testing frequency ranges and applications Table 3 Common ultrasonic testing frequency ranges and applications Frequency range Applications 200 kHz–1 MHz Coarse-grain castings: gray iron, nodular iron, copper, and stainless...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220143
EISBN: 978-1-62708-341-6