1-20 of 287 Search Results for

mold steels

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170210
EISBN: 978-1-62708-297-6
...Abstract Abstract This article provides an overview of tool steels, discussing their composition, properties, and behaviors. It covers all types and classes of wrought and powder metal tool steels, including high-speed steels, hot and cold-work steels, shock-resisting steels, and mold steels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440191
EISBN: 978-1-62708-262-4
...-purpose tool steels L2 T61202 0.50–1.10 (a) 1.00 0.20 … … … … … … L6 T61206 0.70 0.75 … … … 0.25 (b) … … 1.50 Mold steels P2 T51602 0.07 … … 2.00 … … 0.20 … 0.50 P4 T51604 0.07 … … 5.00 … … 0.75 … … Chromium hot-work tool steels H11...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310285
EISBN: 978-1-62708-326-3
...Abstract Abstract The possible classification for tool steels is their division into four groups according to their final application: hot-worked, cold-worked, plastic mold, and high-speed tool steels. This chapter mainly follows such division by application, but the grade nomenclatures used...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240411
EISBN: 978-1-62708-251-8
... work tool steels, low-alloy special-purpose tool steels, mold tool steels, high-speed tool steels, and powder metallurgy tool steels. This chapter provides discusses the manufacturing process, composition, properties, types, and applications of these tool steels and other cutting tool materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130311
EISBN: 978-1-62708-284-6
... mold, and high-speed tool steels. chemical composition tool steel failure analysis heat treatment TOOL STEELS are an important class of steels due to their distinct applications and, especially, their specific heat treating issues. Tool steels are used in various industrial applications...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060273
EISBN: 978-1-62708-261-7
... composition coatings heat treatment high-speed steel wrought tool steel TOOL STEELS BELONG to a special category of steel alloys that have been developed to manufacture the tools, dies, and molds that shape, form, and cut other steel alloys. They are also used to process many nonferrous metals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000005
EISBN: 978-1-62708-312-6
... (350 °F). Chemical compositions of metal injection molding (MIM) grades of stainless steels Table 2.5 Chemical compositions of metal injection molding (MIM) grades of stainless steels Grade Standard/Nonstandard Fe C Cr Ni Mo Cu Si Mn Other Source/Ref 316L MPIF bal 0.03...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410151
EISBN: 978-1-62708-280-8
... that the mold constant C is the same for both the feeder and the casting, M f > M c where Assuming a 20 percent safety factor in the modulus ratios, M f = 1.2 × M c This simplified equation proposed for steel castings cast in sand molds...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
.... , Ahn S. , and Chang Y.W. , Powder Injection Molding of a 17-4 PH Stainless Steel and the Effect of Sintering Temperature on Its Microstructure and Mechanical Properties , J. Mater. Process. Technol. , Vol 130 , 2002 , p 321 – 327 10.1016/S0924-0136(02)00739-2 3. Julien B...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000039
EISBN: 978-1-62708-312-6
... and Expo. ( Detroit, MI ), 1998 10.4271/980334 4. Phillips R. , “ Tooling for Molding Stainless Steel Parts ,” presented at PM Stainless Steel Seminar , March 1–2, 2000 ( Durham, NC ), MPIF, Princeton, NJ 5. Reinshagen J.H. and Mason R.P. , An Evaluation of Methods...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300199
EISBN: 978-1-62708-323-2
..., and large forged shapes. In the United States, they are mostly made by specialty steel suppliers, and tool steel suppliers often offer large blocks of various tool steels for dies and molds. The difference between an alloy steel and a tool steel is not that straightforward, but a practical definition...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410621
EISBN: 978-1-62708-265-5
... Materials for Molds and Dies , Colorado School of Mines Press , Golden, CO , 1987 24.10 Properties and Selection: Irons, Steels, and High-Performance Alloys , Vol 1 , ASM Handbook , ASM International , 1990 24.11 Harvey P.D. , Ed., Heat Treatment of Tool Steels , Metals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
... tool steel 11–13 6.2–7.0 High manganese carbon steel 10–14 5.6–7.6 Malleable cast iron 12 6.6 Mold tool steel 8.8–15 4.9–8.4 Nonresulfurized carbon steel 11–14 5.9–7.5 Chromium molybdenum alloy steel 9.4–15 5.2–8.2 Chromium alloy steel 12–13 6.5–7.0 Molybdenum...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290139
EISBN: 978-1-62708-319-5
... between particles is filled by binder to ensure particle flow during shaping. (a) General view showing many particles. (b) Close-up view of binder filling the pore between contacting particles Fig. 7.2 Photograph of an injection-molded steel component with blisters due to trapped binder during...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040277
EISBN: 978-1-62708-300-3
..., high-chromium cold work tool steels D Mold steels P Hot work tool steels, chromium, tungsten, and molybdenum H Tungsten high-speed tool steels T Molybdenum high-speed tool steels M Table 21.2 provides a good summary of certain material properties of dies for hot forging...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060085
EISBN: 978-1-62708-261-7
... by continuous casting, although ingot casting is still the preferred method for certain specialty, tool, forging, and remelted steel grades. In foundry casting, metals parts are cast by pouring molten metal into a mold with complex cavities to make component shapes (hence the term, shape casting ). Molds...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130151
EISBN: 978-1-62708-284-6
... components already inserted during molding for the casting, for example, in tool steel components. Another possibility during heat treatment is to fill the holes from casting with any material that can totally inhibit contact with the quenching fluid that would result in hardening of this region. Regarding...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
... Molding Process for Fabrication of Micro Machine Parts from Stainless Steel Powder , Adv. Eng. Mater. , Vol 11 , 2009 , p 202 – 205 10.1002/adem.200800165 • Jenni M. , Schimmer L. , Zauner R. , Stampf J. , and Morris J. , Quantitative Study of Powder Binder Separation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
... Shell molds assembled before pouring. Source: Ref 1 Fig. 3.6 Alloy 224.0 impellers produced by low-pressure plaster casting Fig. 3.8 Permanent mold machined from steel. Source: Ref 1 Fig. 3.14 Semisolid formed alloy A357.0 landing gear component Fig. 3.15 One...