... of compositions MBe 13 , MBe 12 , and M 2 Be 17 have unique combinations of properties that include high-temperature strength, good thermal conductivity, excellent oxidation resistance, and low density. For example, the strength (modulus of rupture) of Ta 2 Be 17 at 1060 °C is 420 MPa, and its density is 4.99 g...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780185
EISBN: 978-1-62708-281-5
... strength, MPa (ksi) Elongation, % Modulus of elasticity, GPa (10 6 psi) Compressive strength, MPa (ksi) Modulus of rupture, MPa (ksi) Hardness Thermosets EP, reinforced with glass cloth 350 (51) … 175 (25) 410 (39) 485 (70) MF, alpha-cellulose filler 50–90 (7–13) 0.6–0.9 9 (1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060049
EISBN: 978-1-62708-261-7
... to measure other mechanical properties as well. Additional examples of such properties include the elastic modulus, hardness, fatigue resistance, and fracture toughness. These are described subsequently in more detail. A short list of the important types of mechanical properties includes: Hardness...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.9781627083096
EISBN: 978-1-62708-309-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280211
EISBN: 978-1-62708-267-9
... at the conclusion of a test is recorded. Static modulus generally is not measured, at least in tests designed to produce strength data. Creep-rupture properties are determined by longer-time, sometimes long-time, tests of metal under load, where the elongation generally is measured with time. Failure elongation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870373
EISBN: 978-1-62708-314-0
... mechanical properties for unidirectional composites made from E-glass/epoxy, aramid/epoxy, high-strength carbon/epoxy, and intermediate modulus carbon/epoxy are summarized in Table 14.1 . With regard to this table, there are two words of caution: (1) the properties shown are for unidirectional composites...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240583
EISBN: 978-1-62708-251-8
..., primarily for niobium alloys in aerospace applications, to enable their use in high-temperature oxidizing environments. Table 31.1 Comparative properties of refractory metals Metal Crystal structure (a) Specific gravity Melting point Modulus of elasticity Coefficient of thermal expansion...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290193
EISBN: 978-1-62708-319-5
.... , Tanaka S.I. , Tanaki T. , and Asami J. , Influence of Measuring Method on Young’s Modulus and Comparison with Young’s Modulus and Mechanical Properties of Sintered Irons , J. Jpn. Soc. Powder Powder Metall. , Vol 50 , 2003 , p 96 – 103 10.2497/jjspm.50.96 • Latella B.A...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780146
EISBN: 978-1-62708-281-5
... can be quite tough. However, the short-term tensile strength and modulus of the hydrated nylon will be somewhat reduced, as will the long-term (creep rupture) strength of the material. Creep deformation of the hydrated nylon will proceed more rapidly than that in the dry material at the same level...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610415
EISBN: 978-1-62708-303-4
... Abstract This chapter compares and contrasts the high-temperature behaviors of metals and composites. It describes the use of creep curves and stress-rupture testing along with the underlying mechanisms in creep deformation and elevated-temperature fracture. It also discusses creep-life...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280339
EISBN: 978-1-62708-267-9
..., but the nickel-base and iron-nickel-base products were wrought and relatively weak in creep rupture by today’s standards. Nevertheless, many of the alloys of the 1940s time frame (Vitallium, Inconel X) still have use today. From the 1940s to the 1960s, major advances occurred. The need for high-strength...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.9781627082563
EISBN: 978-1-62708-256-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280011
EISBN: 978-1-62708-267-9
... for the most demanding applications in high-pressure turbine (HPT) sections should be SCDS materials. In addition to maximizing creep-rupture strength, thermal mechanical fatigue (TMF) strength is optimized by the reduction in modulus achieved by orienting a particular direction of the superalloy crystal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540047
EISBN: 978-1-62708-309-6
... they reveal about the load-carrying characteristics of engineering materials. It then discusses the use of failure criteria and the determination of yielding and fracture limits. It goes on to describe the mechanisms and appearances of brittle and ductile fractures and stress rupture, providing detailed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610327
EISBN: 978-1-62708-303-4
... 3 Poisson’s ratio Transverse rupture strength, MPa (ksi) Fracture toughness, MPa m   ( ksi in. ) Young’s modulus, GPa (10 6 psi) Glass-ceramics Variable 2.4–5.9 0.24 70–350 (10–51) 2.4 (2.2) 83–138 (12–20) Pyrex glass Amorphous 2.52 0.2 69 (10) 0.75...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.9781627082709
EISBN: 978-1-62708-270-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540297
EISBN: 978-1-62708-309-6
... Material Crystal structure Theoretical density, g/cm 3 Poisson’s ratio Transverse rupture strength, MPa (ksi) Fracture toughness, MPa m (ksi in . ) Young’s modulus, GPa (10 6 psi) Glass-ceramics Variable 2.4–5.9 0.24 70–350 (10–51) 2.4 (2.2) 83–138 (12...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280323
EISBN: 978-1-62708-267-9
... temperatures. At ordinary temperatures, the strengths of most metals are measured in terms of short-time static properties such as yield strength or ultimate strength, but at high temperatures, creep extension occurs and will lead to rupture if sufficient time elapses under the environment and mechanical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000221
EISBN: 978-1-62708-312-6
... Charpy impact energy, ft-lbf Strength, 10 3 psi Hardness, Rockwell Fatigue strength 90% survival, 10 3 psi Density, g/cm 3 Strength, 10 3 psi Elongation (in 1 in.), % Young’s modulus, 10 6 psi Poisson’s ratio Macro (apparent) Micro (converted) Yield Ultimate Ultimate Yield (0.2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
...-dominated laminates of aramid composites exhibit very little creep. In general, creep strain increases with increasing temperature, increasing stress, and decreasing fiber modulus. However, under long-term loading, aramid composites, similar to glass-fiber composites, are subject to stress rupture...