Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120148
EISBN: 978-1-62708-269-3
...Abstract Abstract This appendix provides datasheets describing the chemical composition, processing characteristics, mechanical and fabrication properties, and heat treating of commercially pure and modified titanium. The datasheets address four grades of unalloyed titanium (ASTM Grade 1, UNS...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000025
EISBN: 978-1-62708-313-3
...Abstract Abstract The microstructure of superalloys is highly complex, with a large number of dispersed intermetallics and other phases that modify alloy behavior through their composition, morphology, and distribution. This chapter provides an overview of the most notable phases, including...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240453
EISBN: 978-1-62708-251-8
...Abstract Abstract The properties of cast iron are determined primarily by the form of carbon they contain, which in turn, is controlled by modifying compositions and cooling rates during casting. Certain alloys (such as Si, Al, Ni, Co, and Cu) promote graphite formation, while others (such as S...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870123
EISBN: 978-1-62708-344-7
... prior to crack initiation and the other after the crack has started. Although the method accounts somewhat better for loading-order effects, the transition in behavior that the rules presume to model occurs prior to any signs of cracking. Two modified versions of the double linear damage rule method...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2016
DOI: 10.31399/asm.tb.ascaam.t59190001
EISBN: 978-1-62708-296-9
... Partially modified Fine plates, partial fragmentation 4 Rods, no plates, some needles are accepted 5 Completely modified Rods, no needles 6 Fine rods, invisible under light microscope Source: Ref 72 Morphological effects of eutectic silicon modification Table 1.7 Morphological...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2016
DOI: 10.31399/asm.tb.ascaam.t59190089
EISBN: 978-1-62708-296-9
... in the interdendritic eutectic. SEM, deep etch Fig. 3.1 Schema of the examined cast part, showing cutting points of the metallography specimens Abstract Abstract This chapter is an atlas of microstructures observed in AlSi7Mg, AlSi11, and Al21CuNiMg modified with either eutectic (strontium, sodium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270080
EISBN: 978-1-62708-301-0
... appears to be a brittle fracture that initiated from a zone of poor-quality weld. It also provides photographic evidence of a weld crack in the heat-affected zone and includes a drawing of a modified weld design that passed subsequent testing. fractography metallography tie rod visual examination...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250245
EISBN: 978-1-62708-345-4
...Abstract Abstract Carbonitriding is a modified form of gas carburizing. It is performed in a closed furnace chamber with an atmosphere enriched with a gaseous compound of carbon and nitrogen. This chapter provides information on the carbonitriding of steels, the applications of carbonitriding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060173
EISBN: 978-1-62708-343-0
... damage 8.83 A TCF Time- + Cycle-Fraction Rule 8.35 A LFA Life fraction approach 8.75 AD TPR 10% Rule 8.12 ABD LCD Linear creep damage for therma1 fatigue 8.84 ABD MLF Modified-Life Fraction Rule 8.26 ABD LFR Life Fraction Rule 8.85 ABD TCD Turbine...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420073
EISBN: 978-1-62708-310-2
... diagrams can be constructed from time-temperature cooling curves and how they can be used to predict the phases present, their chemical compositions, and relative amounts. It also shows how phase diagrams can be modified to account for nonequilibrium cooling conditions. binary isomorphous systems...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030177
EISBN: 978-1-62708-349-2
... for composites in a variety of aircraft applications. To improve the damage tolerance of composite materials even further, an engineering approach to toughening was used to modify the highly stressed interlayer with either a tougher material or through the use of preformed particles, leading to the third...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320171
EISBN: 978-1-62708-347-8
... to room temperature that produces the desired properties. Carbonitriding is generally regarded as a modified gas carburizing process, rather than a form of nitriding. This chapter briefly describes the case depth that can be achieved with carbonitriding, how case depth is measured, and the materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780105
EISBN: 978-1-62708-281-5
... in characterizing thermoplastics, whether they are homogeneous resins, alloyed or blended compositions, or highly modified thermoplastic composites. It begins with a description of various approaches used for the determination of molecular weight (MW) by viscosity measurements. This is followed by a discussion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780336
EISBN: 978-1-62708-281-5
... and amylose films, starch-based polyethylene films, films with modified starch additives, poly(3-hydroxybutyrate-valerate)-biodegradable plastic, and biodisintegration and biodegradation studies of plastic-starch blends, are also presented. microbial degradation plastics biodeterioration plastic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220241
EISBN: 978-1-62708-341-6
... Abstract To a large extent, the induction coil and its coupling to the workpiece determine the precise heating pattern that is developed. However, it is often desirable to modify this pattern in order to produce a special heating distribution or to increase energy efficiency. At other times, the high...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140039
EISBN: 978-1-62708-335-5
... of Directionally Solidified Aluminum Foundry Alloys , AFS Trans. , 1987 • Shamsuzzoha M. and Hogan L. , The Crystal Morphology of Fibrous Silicon in Strontium Modified Al-Si Eutectic , Philos. Mag. , Vol 54 , 1986 10.1080/01418618608243605 • Sigworth G. , Observations...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030001
EISBN: 978-1-62708-349-2
... Inclusions , Org. Coat. Plast. Preprints , Vol 39 , 1978 , p 164 14. Verchere D. , Sautereau H. , Pascault J.-P. , Moschiar C.C. , Richardi S.M. , and Williams R.J.J. , Rubber-Modified Epoxies: Analysis of the Phase-Separation Process , Toughened Plastics I...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.9781627083492
EISBN: 978-1-62708-349-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000101
EISBN: 978-1-62708-312-6
... from Fig. 5.33 in Chapter 5 Fig. 6.3 Effect of pitting resistance equivalent on corrosion resistance (5% NaCl by immersion) of standard (▭)and tin- and copper- ( o ) modified austenitic stainless steels (unpublished data) Fig. 6.4 Auger composition-depth profile of 1.5% Sn...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430376
EISBN: 978-1-62708-253-2
.... Mazur, J. Melicharek, N. and Schmittdiel M. , “ Erosion, Cavitation and Fretting .” Last modified 2014 , http://www.lettsvankirk.com/index.php?option=com_docman&task=doc_download&gid=35&Itemid= 6.23 Chen Y. M. , Cavitation Erosion , Failure Analysis...