Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290165
EISBN: 978-1-62708-306-5
... Abstract Brazing and soldering processes use a molten filler metal to wet the mating surfaces of a joint, with or without the aid of a fluxing agent, leading to the formation of a metallurgical bond between the filler and the respective components. This chapter discusses the characteristics...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230105
EISBN: 978-1-62708-351-5
... Abstract This chapter discusses joining atmospheres that are used for brazing, along with their advantages and disadvantages. It discusses the processes, advantages, and disadvantages of chemical fluxing, self-fluxing, and fluxless brazing. Information on stop-off compounds that are considered...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
... zirconia polycrystalline (Y-TZP). It also provides information on materials selection, design optimization, and joining methods, and covers every step of the ceramic production process. brazing ceramic processing diffusion bonding structural ceramics toughened ceramics weibull analysis...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290279
EISBN: 978-1-62708-306-5
... by mechanical fastening, adhesive bonding, and, for thermoplastic composites, welding; the making of glass-to-metal seals; and joining of oxide and nonoxide ceramics to themselves and to metals by solid-state processes and by brazing. The classification, types, applications, and the mechanism of each...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440049
EISBN: 978-1-62708-352-2
... then extends to consider the less common solders, arranged in rough order of usage and decreasing melting point. To readers familiar with brazing technology, one important difference of solders will soon be apparent. That is, solders are largely based on unique eutectic compositions. The addition of other...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
... or 2490 °F). Other than microwave sintering, almost any furnace is successful in sintering 17–4 PH. Most common is vacuum or hydrogen sintering. Continuous pusher-plate or walking beam hydrogen furnaces are used to sinter millions of cell telephone parts every day, while batch vacuum or hydrogen...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440145
EISBN: 978-1-62708-352-2
... an activated solder or braze, capable of providing a solderable surface, to wet and spread over the component surfaces. The “tinned” surface is then usually mechanically dressed to present a flat metal surface for the actual joining step, which is performed at a temperature below the solidus point...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440103
EISBN: 978-1-62708-352-2
... reduce the oxides of less refractory metals, it will remove this surface film, enabling wetting to proceed in a conventional manner through alloying. Reactive solders are described in Chapter 4, section 4.1.2.2 . Active brazes, which are much more common, are discussed separately in the planned...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480353
EISBN: 978-1-62708-318-8
... and Testing of Titanium Alloys,” in this book). Titanium sheet metal components are generally riveted to supporting structures. However, brazing, diffusion bonding, and welding by resistance, fusion, electron beam, and laser have also been used to fabricate titanium sheet metal structures. When properly...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390241
EISBN: 978-1-62708-459-8
... source can be due to electrical resistance [ 21 ], microwaves [ 22 ] or laser heating [ 23 ]. As the bar is stretched, deformations are restricted to the hot section. Obviously, this eliminates lubrication and cleaning, as well as die wear considerations. However, the process is slow, and determined...
Book Chapter

By A. F. Clark
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860075
EISBN: 978-1-62708-348-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.9781627083485
EISBN: 978-1-62708-348-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0