1-20 of 864 Search Results for

metals-based additive manufacturing

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000009
EISBN: 978-1-62708-313-3
... elements in the composition, with the three base metals being nickel, cobalt, and iron. The entire superalloy family shares a common basic microstructure, which is a face-centered cubic (fcc) matrix with a number of dispersed secondary strengthening phases. In elemental form, nickel is the only superalloy...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300391
EISBN: 978-1-62708-323-2
... Extreme pressure Proprietary Emulsifiers Proprietary Some equipment manufacturers have gone a step further and specify the use of their brand oil: “Use only Dexos 5W-20 oil.” This ensures that a certain viscosity base oil with certain additives is used in that tribosystem. Thus, oil users do...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930179
EISBN: 978-1-62708-359-1
... Metals for Gas-Shielded Arc Welding”), and A5.29 (“Low Alloy Steel Electrodes for Flux Cored Arc Welding”). Cast Irons Cast irons are a family of high-carbon iron-base alloys containing from 2 to 4% C, 0.50 to 2% Si, and varying amounts of added manganese and chromium strengtheners, in addition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230189
EISBN: 978-1-62708-351-5
... carat gold solders. brazing carat filler metals gold alloys gold jewelry gold solders silver jewelry silverware BRAZES FOR JEWELRY, silverware, and objets d’art merit separate consideration from industrial brazing alloys because, in addition to providing joints that are mechanically...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290251
EISBN: 978-1-62708-319-5
... combinations, and processing ideas, such as binder jetting and extrusion-based additive manufacturing, including bound-metal deposition and fused-filament fabrication. 11.1 Introduction Science fiction is a great resource for looking forward to where technology advances may take us. The ideas of flying...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
... Radial forge processing of nickel-base superalloy into round billet. Courtesy of Allvac ATI Fig. 6.2 Multilevel gears produced by powder metallurgy. Courtesy of Metal Powder Industries Federation (MPIF) Fig. 6.3 Ultrasonic welding of aluminum foil. Courtesy of Sonobond Ultrasonics Inc...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390100
EISBN: 978-1-62708-459-8
.... The development of a lubricant represents substantial effort, involving laboratory evaluation of candidate base lubricants and additives, testing for toxicity and other nontribological properties, field testing, and establishment of a lubricant manufacturing process. 6.2 Mineral Oils Mineral oil...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320003
EISBN: 978-1-62708-332-4
... Abstract This chapter provides a brief overview of iron and steel manufacturing and the major equipment involved in the process as well as identifying where casting fits into the overall process. In addition, it provides an overview of cast iron manufacturing, including the processes involved...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230493
EISBN: 978-1-62708-298-3
... residuals are liberated during the manufacturing process of beryllium and beryllium oxide ceramics. When plausible, these by-products are collected without additional contamination and recycled directly back into the manufacturing process. When these by-products are contaminated with other metals...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170550
EISBN: 978-1-62708-297-6
... tableware. Less obvious, but equally pervasive, are the use of platinum-group metals as catalysts in automotive pollution-control equipment and for making the spinnerettes used in the manufacture of synthetic fibers for clothing; the use of silver for photographic processes; the use of gold, palladium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220281
EISBN: 978-1-62708-341-6
..., as on the handles of hand tools, scissors, etc., the heat and thus the coating can be restricted to a specific area. Thermosetting materials can also be applied electrostatically to the base metal, as is done in the manufacture of coated anchor chains. Unlike the methods described above, the dry powder is given...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280339
EISBN: 978-1-62708-267-9
... the understanding and adaptation of chromium as an additive to the transition metals iron, nickel, and cobalt, with marvelous bene cial effects on the corrosion resistance, both aqueous and gaseous. From nickel-base resistance wires and cobalt-base wear- and temperature-resistant alloys, it was a short jump in time...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170528
EISBN: 978-1-62708-297-6
... of copper are added to increase hardness for some applications. Compositions of type metals in present commercial use are given in Table 3 . The lead base provides low cost, a low melting point, and ease of casting—properties that are desirable for all type metals. Additions of antimony harden the alloy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
...-pressure cold spray. 8.1 Additive Manufacturing for the Automotive Industry Using Cold Gas Dynamic Spraying Until recently, the needs for the manufacturing of brittle material components in the industrial field and the development of metal powders and processes have expanded the application...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200369
EISBN: 978-1-62708-354-6
... has been in service. Most of the cast grades are readily weldable, however, the ease with which they can be welded depends on their chemical composition, heat treatment, and to some degree, the section thickness involved. Base metal preparation and details of welding, defect removal, and some...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290261
EISBN: 978-1-62708-319-5
... All rights reserved www.asminternational.org APPENDIX Glossary A acicular powder. Needle-shaped particles good for debinding strength but generally detrimental to the forming process because they resist ow in molding. additive manufacturing (AM). A process of joining materials to make components from...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440049
EISBN: 978-1-62708-352-2
... zinc is for joining aluminum and its alloys [ Finch 1985 ]. This metal plays an additional role in helping to disrupt alumina surface layers and so helps to promote wetting by the solder. A flux-cored, zinc-base solder that is intended for joining aluminum is available commercially [ Rubin 1982...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320323
EISBN: 978-1-62708-332-4
... additions. The databases include: Average core sand added for each part Average bond burnt for each part Computer programs are generated based on this information to guide the new sand addition on a daily basis based on the parts produced. Weekly tests are run for sand distribution correction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400089
EISBN: 978-1-62708-316-4
... they are applied and removed and how their pressure and temperature ranges can be extended by performance enhancing additives. The chapter also explains how sheet metal forming lubricants are evaluated in the laboratory as well as on the production floor and how tribological tests are conducted to simulate...