1-20 of 659 Search Results for

metallurgical effect

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030062
EISBN: 978-1-62708-282-2
... Abstract This chapter is dedicated mostly to the metallurgical effects on the corrosion behavior of corrosion-resistant alloys. It begins with a section describing the importance of alloying elements on the corrosion behavior of nickel alloys. The chapter considers the metallurgical effects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030074
EISBN: 978-1-62708-282-2
... Abstract This chapter is dedicated mostly to the metallurgical effects on the corrosion behavior of corrosion-resistant alloys. It begins with a section describing the importance of alloying elements on the corrosion behavior of nickel alloys. The chapter considers the metallurgical effects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030070
EISBN: 978-1-62708-282-2
... Abstract This chapter describes the effects of metallurgical variables on the corrosion of aluminum alloys. Emphasis is placed on the effect of constituent particles on pitting corrosion of aluminum. corrosion aluminum alloys aluminum THE METALLURGICAL EFFECTS on corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030082
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses the effects of metallurgical variables on dealloying corrosion. It begins by describing the processes involved in dealloying of metal alloys in aqueous environments. This is followed by a discussion on the morphology of porous dealloyed structures below and above...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860269
EISBN: 978-1-62708-348-5
... contributing to the fracture behavior of materials at cryogenic temperatures. Three approaches of elastic-plastic fracture mechanics are covered, namely the crack opening displacement, the J-integral, and the R-curve methods. The chapter also discusses the influence of thermal and metallurgical effects...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730011
EISBN: 978-1-62708-283-9
... of the metallurgical effects of freezing or solidification, including the segregation of solutes and the formation of metal glasses. freezing interstitial solid solutions metal glasses phase diagrams phase relations phases substitutional solid solutions Phases A DISTINCT STATE of aggregation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060083
EISBN: 978-1-62708-343-0
... there to describe how fatigue life can be estimated from ductility measurements when cyclic data are unavailable or are likely to change. It also explains how cyclic life is influenced by the time-dependent nature of creep-plasticity and the physical and metallurgical effects of environmental exposure. creep...
Image
Published: 01 January 2017
Fig. 10.21 Effects of halide addition and alloy metallurgical condition on SCC behavior of Ti-8Al-1Mo-1V (double cantilever beam specimens, DCB) in methanol at 24 °C (75 °F). Source: Ref 10.22 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030003
EISBN: 978-1-62708-282-2
... elements, grain boundaries, second phases, and inclusions often have a dominant effect. Finally, welded structures almost always corrode first at the welds because of metallurgical heterogeneities that exist in and near welds. In general, the most susceptible site or defect on a metal surface...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060115
EISBN: 978-1-62708-355-3
... of the factors that influence the test results. This chapter provides a metallurgical perspective for such interpretation. The topics covered include elastic behavior, anelasticity, damping, proportional limit, yield point, ultimate strength, toughness, ductility, strain hardening, and yielding and the onset...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820013
EISBN: 978-1-62708-339-3
.... Corrosion of carbon steel weldments can be due to metallurgical effects, such as preferential corrosion of the HAZ or weld metal, or it can be associated with geometrical aspects, such as stress concentration at the weld toe, or creation of crevices due to joint design. Additionally, specific environmental...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030172
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses the effects of metallurgical factors on the corrosion resistance of magnesium alloys. The factors are chemical composition, heat treating, grain size, and cold-work effects. The chapter describes the causes of corrosion failures in magnesium alloys, namely heavy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440009
EISBN: 978-1-62708-262-4
... Abstract Steel is an important material because of its tremendous flexibility in metal working and heat treating to produce a variety of mechanical, physical, and chemical properties. The purpose of this chapter is to present the metallurgical principles of heat treatment of steel...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860133
EISBN: 978-1-62708-348-5
... Abstract This chapter presents basic principles and the theoretical results of heat transport in solids. Thermal conductivity and thermal diffusivity are the principal properties discussed. Discussions are also included on the effects of temperature, magnetic field, and metallurgical variations...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080005
EISBN: 978-1-62708-304-1
... of weight gain, metal loss, depth of attack, and oxidation rate. It also discusses the effect of metallurgical and environmental factors such as oxygen concentration, high-velocity combustion gas streams, chromium depletion and breakaway, component thickness, and water vapor. austenitic stainless...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770001
EISBN: 978-1-62708-337-9
... in the best way possible every time. Laboratory Tests Laboratory tests to determine the effect of metallurgical variables, for example, carbides, retained austenite, and core strength, are very useful and have contributed appreciably to the understanding of the influences of metallurgical features...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030167
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses the factors influencing the corrosion resistance of bulk materials, namely alloying, metallurgical factors, and mechanical treatments. corrosion resistance bulk materials alloying metallurgical factors mechanical treatments THE CORROSION RESISTANCE...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410017
EISBN: 978-1-62708-265-5
... This chapter describes the iron-carbon phase diagram, its modification by alloying elements, and the effect of carbon on the chemistry and crystallography of austenite, ferrite, and cementite found in Fe-C alloys and steels. It also lays the groundwork for understanding important metallurgical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030096
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses various factors that affect corrosion of stainless steel weldments. It begins by providing an overview of the metallurgical factors associated with welding. This is followed by a discussion on preferential attack associated with weld metal precipitates...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
... Abstract Stainless steels and nickel-base alloys are recognized for their resistance to general corrosion and other categories of corrosion. This chapter examines the effects of specific alloying elements, metallurgical structure, and mechanical conditioning on the corrosion resistance...