1-20 of 367 Search Results for

metallic powder

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130395
EISBN: 978-1-62708-284-6
... analysis case hardening powder metal steel components POWDER METALLURGY (PM) technology provides a cost-effective method of producing near-net shape products, especially when a large number of the same or similar products are required. While the initial powder used is expensive compared to wrought...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000039
EISBN: 978-1-62708-312-6
... Abstract This chapter discusses the methods by which stainless steel powders are shaped and compacted prior to sintering, including rigid die compaction, metal injection molding, extrusion, and hot isostatic pressing. It explains where each process is used and how processing parameters...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980141
EISBN: 978-1-62708-342-3
... profiles, and the processing of composite materials, as well as the extrusion of metal powders, are discussed. The chapter ends with a discussion on the factors that define the extrudability of metallic materials and how these attributes are characterized. aluminum alloys billets casting defects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060085
EISBN: 978-1-62708-261-7
... the design and operation of melting furnaces as well as melting practices and the role of fluxing. It also discusses casting methods, nonferrous casting alloys, and atomization processes used to make metal powders. atomization foundry casting melting furnaces nonferrous casting alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000005
EISBN: 978-1-62708-312-6
... characteristics of austenitic, ferritic, martensitic, duplex, and precipitation hardening stainless steel powders and metal injection molding grades. alloy composition stainless steel stainless steel powder References 1. Kovach C.W. and Redmond J.D. , Austenitic...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290251
EISBN: 978-1-62708-319-5
... ceramics porous structures foams design criteria Powder-binder processing evolved by following advances in plastics technologies. Subsequently, ideas such as additive manufacturing developed for future opportunities in metallic, ceramic, and composite structures. Early success in ceramics shaping...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000223
EISBN: 978-1-62708-312-6
... Abstract This appendix is a compilation of terms and definitions associated with the processing, microstructure, and properties of powder metal stainless steels. microstructure powder metallurgy stainless steel ASM Materials Engineering Dictionary , ASM International, 1992...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000109
EISBN: 978-1-62708-312-6
... Abstract This chapter discusses the mechanical properties of powder metal stainless steels and the extent to which they can be controlled through appropriate alloying and processing steps. It describes how process-related factors, such as porosity, interstitial content, sintering atmosphere...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
..., and brazing. It also discusses powder consolidation, rolling, drawing and extrusion, and common forging methods. fabrication finishing forging forming joining material removal powder processing METAL PRODUCTS that are subjected to mechanical reduction operations subsequent to casting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230267
EISBN: 978-1-62708-298-3
... Abstract Powder metallurgy plays a central role in the production of nearly all beryllium components. This chapter describes the primary steps in the powder metal process and the work that has been done to improve each one. It explains how beryllium powders are made and how...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000167
EISBN: 978-1-62708-312-6
... Abstract This chapter describes secondary processes employed in the production of powder-metal stainless steel parts, including various machining operations, welding, brazing, sinter bonding, resin impregnation, re-pressing and sizing, and surface finishing. It also discusses the factors...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
..., and powder metals. It discusses their properties and applications as well as suitable equipment for extrusion. It further discusses the processes involved in the extrusion of semifinished products in exotic alloys and extrusion of semifinished products from metallic composite materials. extruded metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480161
EISBN: 978-1-62708-318-8
... Qian M. , Ed., Powder Metallurgy of Titanium , Trans Tech Publications, Durnten-Zurich , Switzerland , 2012 8.14 Froes F.H. , Titanium Powder Metallurgy: Developments and Opportunities in a Sector Poised for Growth , Powder Metall. Rev. , Vol 2 ( No. 4 ), Winter 2013 , p 29...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... and slurry casting, liquid metal infiltration, spray deposition, powder metallurgy, extrusion, hot rolling, and forging. The chapter also provides information on continuous-fiber aluminum and titanium composites as well as particle-reinforced titanium and fiber metal (glass aluminum) laminates...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550223
EISBN: 978-1-62708-307-2
..., and grades of commercially pure titanium and alpha and near-alpha, alpha-beta, and beta titanium alloys. It describes primary and secondary fabrication processes, including melting, forging, forming, heat treating, casting, machining, and joining as well as powder metallurgy and direct metal deposition...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000185
EISBN: 978-1-62708-312-6
...) industry as a whole. Parallel with this shift, ferritic stainless steels now account for the major volume of sintered stainless steels. Table 11.1 is an adaptation of the summary of applications of sintered stainless steels from Powder Metal Technologies and Applications , Volume 7, ASM Handbook...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740373
EISBN: 978-1-62708-308-9
... clutch races. (c) Sensor rings for anti-lock brakes. Source: Ref 1 – 3 References 1. P/M Parts Showcase , Met. Powder Rep. , Vol 50 ( No. 1 ), p 5 2. Johnson P.K. , Winning Parts Show High Strength and Cost Savings , Int. J. Powder Metall. , Vol 22...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000023
EISBN: 978-1-62708-312-6
.... , Gas and Water Atomization , Powder Metallurgy , Vol 7 , Metals Handbook , 9th ed. , American Society for Metals , 1984 , p 26 3. Dautzenberg N. and Gesell H. , Production Technique and Properties of Austenitic Cr-Ni Stainless Steel Powders , Powder Metall. Int. Vol 8...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000059
EISBN: 978-1-62708-312-6
... and are normally absent in properly finished wrought stainless steels. References 1. Lenel F.V. , Powder Metallurgy—Principles and Applications , Metal Powder Industries Federation , Princeton, NJ , 1980 , p 184 2. German R.M. , Powder Metallurgy Science , 2nd ed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.9781627083126
EISBN: 978-1-62708-312-6