1-20 of 1066 Search Results for

metallic materials

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
... enable a wide spectrum of materials to be extruded. This chapter focuses on the processes involved in the extrusion of semifinished products in various metals and their alloys, namely tin, lead, lead-base soft solders, tin-base soft solders, zinc, magnesium, aluminum, copper, titanium, zirconium, iron...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720117
EISBN: 978-1-62708-305-8
... properties, and general procedures of tensile testing. Three distinct aspects of standard test methods for tension testing of metallic materials are discussed: test piece preparation, geometry, and material condition; test setup and equipment; and test procedure. mechanical properties metallic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980141
EISBN: 978-1-62708-342-3
... profiles, and the processing of composite materials, as well as the extrusion of metal powders, are discussed. The chapter ends with a discussion on the factors that define the extrudability of metallic materials and how these attributes are characterized. aluminum alloys billets casting defects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820013
EISBN: 978-1-62708-339-3
... vessel chemical analysis results Table 8 Absorber vessel chemical analysis results Material Composition, % C Mn Si S P As Sn Pb Sb Weld 0.049 0.62 0.56 0.028 0.017 0.0014 0.0025 0.001 nil Parent metal 0.18 1.47 0.35 0.022 0.018 0.0021 0.0030 0.001 nil...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060209
EISBN: 978-1-62708-355-3
...Abstract Abstract This chapter focuses on short-term tensile testing at high temperatures. It emphasizes one of the most important reasons for conducting hot tensile tests: the determination of the hot working characteristics of metallic materials. Two types of hot tensile tests are discussed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540357
EISBN: 978-1-62708-309-6
...Abstract Abstract Deformation within a crystal lattice is governed principally by the presence of dislocations, which are two-dimensional defects in the lattice structure. Slip from shear stress is the most common deformation mechanism within crystalline lattices of metallic materials, although...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060101
EISBN: 978-1-62708-355-3
... of the formability of a material in all situations. However, as discussed in this chapter, the uniaxial tensile test is one of the most widely used tests for determining sheet metal formability. This chapter describes the effect of material properties and temperature on sheet metal formability. Information...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
... interest both as engineering materials and as alloying agents. This chapter addresses both roles, discussing the properties, processing characteristics, and applications of several categories of nonferrous metals, including light metals, corrosion-resistance alloys, superalloys, refractory metals, low...