1-20 of 1270 Search Results for

mechanical property

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870351
EISBN: 978-1-62708-314-0
... the grips through shear to the test specimen without failing. Mechanical properties are usually reported in terms of the volume fraction of fibers or fiber volume percent. However, it is much easier to determine weights using laboratory analysis techniques. For example, a cured sample is first weighed...
Image
Published: 01 December 1996
Fig. 5-38 Tensile mechanical property data for the tempered condition of a 1040 (plain carbon) steel and a 4140 (alloy) steel. (From Modern Steels and Their Properties , Handbook 3310, Bethlehem Steel Corporation, Bethlehem, PA, Ref 8 ) More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140039
EISBN: 978-1-62708-264-8
... Abstract Metals are used in many engineering applications because of their mechanical properties, particularly strength and ductility. This chapter explains how mechanical properties are measured and how to interpret the results. It describes the most widely used tests, including tensile tests...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630013
EISBN: 978-1-62708-270-9
... Abstract This chapter focuses on some of the facts of mechanical properties of metals that must be understood to successfully undertake the task of failure analysis. The discussion begins by describing the causes and effects of elastic and plastic deformation followed by a section describing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000109
EISBN: 978-1-62708-312-6
... Abstract This chapter discusses the mechanical properties of powder metal stainless steels and the extent to which they can be controlled through appropriate alloying and processing steps. It describes how process-related factors, such as porosity, interstitial content, sintering atmosphere...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860237
EISBN: 978-1-62708-348-5
... Beryllium a Other phases may be present. References on background material for low-temperature mechanical properties of materials. Table 7.2 References on background material for low-temperature mechanical properties of materials. § 7.2 Temperature dependence of strengthening...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060049
EISBN: 978-1-62708-261-7
... Abstract This chapter introduces the concepts of mechanical properties and the various underlying metallurgical mechanisms that can be used to alter the strength of materials. The mechanical properties discussed include elasticity, plasticity, creep deformation, fatigue, toughness, and hardness...