1-20 of 604 Search Results for

mechanical plating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780216
EISBN: 978-1-62708-281-5
... with their associated results. A brief discussion on the linear elastic fracture mechanics method is presented, along with an example of its effectiveness as a predictive tool for impact performance. Various issues with a bearing on impact performance, such as processing, chemical attack, and aging, are also described...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... mechanisms: barrier protection, chemical inhibition, and galvanic (sacrificial) protection. This chapter begins with a section on organic coating and linings, providing a detailed account of the steps involved in the coating process, namely, design and selection, surface preparation, application...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140021
EISBN: 978-1-62708-264-8
..., with the pearlite distributed in various forms. Wrought steels often show a banded microstructure, with alternating bands of ferrite grains and pearlite grains aligned in the direction of the prior mechanical deformation ( Fig. 4.9 ). The cementite in slow-cooled steels generally is contained as thin plates...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... (nickel-phosphorus) and wear resistance (nickel-phosphorus and nickel-boron) Mechanical plating Improved corrosion resistance Weld overlays Improved wear resistance (hardfacing alloys) and corrosion resistance (stainless steel or nickel-base overlays) and dimensional restoration (buildup alloys...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290207
EISBN: 978-1-62708-306-5
... content of 0.50 to 0.80%. Fasteners are generally formed in the annealed stage and then hardened and tempered to a hardness of 45 to 50 Rc. Zinc or cadmium electroplating is specified for certain applications. Other applications may use a zinc mechanical plating to eliminate hydrogen embrittlement...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630035
EISBN: 978-1-62708-270-9
... the basic mechanisms of residual stress formation: thermal, transformational, mechanical, and chemical. residual stress thermal residual stresses transformational residual stresses mechanical residual stresses IT IS LITERALLY a shattering experience to witness a metal part suddenly split...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540169
EISBN: 978-1-62708-309-6
.... and Sih G.C. , On the Crack Extension in Plates Under Plane Loading and Transverse Shear , J. Basic Eng. (Trans. ASME), Ser. D , Vol 85 , 1963 , p 519 – 527 10.1115/1.3656897 4.55. Sih G.C. and MacDonald B. , Fracture Mechanics Applied to Engineering Problems—Strain Energy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.9781627083164
EISBN: 978-1-62708-316-4
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110144
EISBN: 978-1-62708-247-1
.... It also presents a case study illustrating the application of CNC milling to isolate MCM leakage failure. chemical etching CNC machining flat lapping frontside sample preparation laser decap method laser etching mechanical milling multi-chip module plasma reactive ion etching...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420303
EISBN: 978-1-62708-310-2
... Abstract This chapter examines two important strengthening mechanisms, martensitic and bainitic transformations, both of which occur under nonequilibrium cooling conditions. It explains how time-temperature-transformation diagrams are constructed and how they are used to understand and control...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780055
EISBN: 978-1-62708-281-5
... for design and material selection. Engineering plastics are now used in applications where their mechanical performance must meet increasingly demanding requirements. Because the marketplace is more competitive, companies cannot afford overdesigned parts or lengthy, iterative product-development cycles...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220353
EISBN: 978-1-62708-259-4
.... It describes the effect of hot working on nonmetallic inclusions and the many properties influenced by them. It discusses the recrystallization mechanism by which hot working produces microstructural changes and explains how to control it by adjusting temperature, degree of reduction, and cooling rates...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540397
EISBN: 978-1-62708-309-6
...: Ref A7.11 Sheet and plate mechanical properties data for the low-density 8090 and 2090 Al-Li alloys are presented in Table A7.5 . Table A7.6 lists the test results for extrusions. Fatigue and fatigue crack growth rate data for the 8090-TU51 extrusion are shown in Fig. A7.9 to A7.11...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410113
EISBN: 978-1-62708-265-5
... grain boundaries or as Widmanstätten side plates and grow into austenite grain interiors, rejecting carbon until there is sufficient carbon to nucleate pearlite. The latter process produces the ferrite-pearlite microstructures of low- and medium-carbon steels cooled in air after hot rolling or after...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2016
DOI: 10.31399/asm.tb.ascaam.t59190001
EISBN: 978-1-62708-296-9
... interface. The eutectic silicon plate grows through the TPRE mechanism developed in the groove at the twin boundary ( Ref 35 , 53 – 58 ). The fluctuations of the actual growth conditions force its branching or overgrowth. The branching of the silicon plate is strongly determined by the cooling rate...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410099
EISBN: 978-1-62708-265-5
... drag on bainite formation mechanisms. It also discusses the development of ferrite-carbide bainites and their effect on toughness, hardness, and ductility. bainite bainitic transformation ferrite mechanical behavior References 6.1 Davenport E.S. and Bain...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870099
EISBN: 978-1-62708-299-0
... Abstract Environmentally assisted cracking is a generic term that includes various cracking phenomena such as stress-corrosion cracking (SCC), corrosion fatigue cracking, and liquid-metal embrittlement. This chapter describes these cracking mechanisms beginning with SCC and the factors...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410063
EISBN: 978-1-62708-265-5
... representation of the slip (a) and twinning (b) modes of lattice invariant deformation with martensite plates. These sketches, of course, are idealized to demonstrate the concept of the lattice invariant shear. In actual crystals, when slip is the mechanism of accommodation, not only are dislocations introduced...