1-20 of 437 Search Results for

mater

Sort by
Image
Published: 01 December 2003
Fig. 17 Radial features thought to be crystallites in the matrix of the APC-2 material, indicative of the crystalline nature of the carbon/thermoplastic (AS4/APC-2) resin system, following failure due to mode I tension loading. 5000× More
Image
Published: 01 June 1983
Figure 6.16 The effect of ferro- and antiferromagnetic transitions on a number of material properties. More
Image
Published: 01 June 1983
Figure 14.2 Thermal conductivity vs. temperature for frequently used thermocouple materials. The alloys corresponding to the standard thermocouple types (i.e., KP, KN, TP, TN, and JP) are discussed in 14.3.3. More
Image
Published: 01 November 2013
Fig. 16 Approximate speed ranges and applications of various cutting and tool materials. Courtesy GTE Valenite Corp. Source: Ref 8 More
Image
Published: 01 January 2015
Fig. 6.26 Effect of oxygen content on fracture toughness. Extralow interstitial material contains less than 0.13 wt% O. More
Image
Published: 30 April 2021
Fig. 10.15 Average volume loss plus and minus two standard deviations of various materials tested in a loop abrasion test against 30 μm aluminum oxide finishing tape (200 g, 8 h test) More
Image
Published: 01 November 2010
Fig. 6.2 Photograph of an ultrathin section made from a glass fabric composite material. In this sample, the backing pieces are made from carbon fiber composite to provide contrast with the glass fabric composite samples in the center of the section (which cannot be seen due to the ultrathin di... More
Image
Published: 01 December 1995
Fig. 6-47 Schematic diagrams of probability of occurrence of applied stress and material yield strength More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280365
EISBN: 978-1-62708-267-9
... International , 1997 • Rohrbach K.P. , Trends in High-Temperature Alloys , Adv. Mater. Process. , Vol 148 ( No. 10 ), 1995 , p 37 – 40 • ASM Handbook , 10th ed. , ASM International , various dates, with a wide range of information on all facets of heat-resistant materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120345
EISBN: 978-1-62708-269-3
... • Gilbert J.R.B. , The Uses of Titanium , Mater. Sci. Technol. , Vol 1 ( No. 4 ), 1985 , p 257 – 262 10.1179/mst.1985.1.4.257 • Hanson B H. , Present and Future Use of Titanium in Engineering , Mater. Des. , Vol 7 ( No. 6 ), 1986 , p 301 – 307 10.1016/0261-3069(86)90099-3...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2022
DOI: 10.31399/asm.tb.mbheaktmse.t56030001
EISBN: 978-1-62708-418-5
.... , and Lu A.P. , Microstructures and Properties of High-Entropy Alloys , Prog Mater Sci , Vol 61 , 2014 , p 1 – 93 10.1016/j.pmatsci.2013.10.001 2. Cantor B. , Chang I.T.H. , Knight I. P. , and Vincent A.J.B. , Microstructural Development in Equiatomic Multicomponent...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2022
DOI: 10.31399/asm.tb.mbheaktmse.t56030021
EISBN: 978-1-62708-418-5
... S.Y. , Nanostructured High‐Entropy Alloys with Multiple Principal Elements: Novel Alloy Design Concepts and Outcomes , Adv Eng Mater , Vol 6 , 2004 , p 299 – 303 10.1002/adem.200300567 2. Lu Z. , Wang H. , Chen M. , Baker I. , Yeh J. , Liu C.T. , and Nieh...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2022
DOI: 10.31399/asm.tb.mbheaktmse.9781627084185
EISBN: 978-1-62708-418-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230485
EISBN: 978-1-62708-298-3
.... , and Jepson W.B. , 1960 . The High Temperature Oxidation of Beryllium, Part I: In Dry Oxygen , J. Nucl. Mater. , Vol 2 , p 169 – 175 10.1016/0022-3115(60)90044-1 Aylmore D.W. , Gregg S.J. , and Jepson W.B. , 1961 . The High Temperature Oxidation of Beryllium, Part IV...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030200
EISBN: 978-1-62708-282-2
... Control in Enhanced Oil Recovery Wells , Mater. Perform. , Vol 27 ( No. 2 ), Feb 1987 , p 16 – 22 4. Hausler R.H. , Corrosion Inhibition in the Presence of Corrosion Product Layers , Proceedings of the Sixth European Conference on Corrosion Inhibitors (Ferrara), 1985 , p 41 – 65...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230523
EISBN: 978-1-62708-298-3
.../08827509408914114 Aitken E.A. , and Smith J.P. , 1962 . Oxidation of Beryllium Intermetallic Compounds in Moist Atmospheres : J. Nucl. Mater. , Vol 6 , p 119 10.1016/0022-3115(62)90220-9 Akishin P.A. , Spiridonov V.P. , and Sobolev G.A. , 1958 . Electron Diffraction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.9781627082983
EISBN: 978-1-62708-298-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130285
EISBN: 978-1-62708-284-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2016
DOI: 10.31399/asm.tb.ascaam.t59190001
EISBN: 978-1-62708-296-9