... starboard side pin also gave way, fracturing at its tack welded joint. As per specifications, the connecting flanges were made of EN 1A material, and the connecting pins were made of EN 19 “R” material. Subsequent to machining, these parts are to be cadmium plated. The flange and the hinge pin are...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290207
EISBN: 978-1-62708-306-5
... system. The chapter then describes important structural fasteners, namely bolts, screws, pins, collar fasteners, rivets, blind fasteners, machine pins, and spring clip fasteners. The following sections describe the process involved in presses, shrink fits, hole generation, and fastener installation. The...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280189
EISBN: 978-1-62708-267-9
... Abstract The qualities that make superalloys excellent engineering materials also make them difficult to machine. This chapter discusses the challenges involved in machining superalloys and the factors that determine machinability. It addresses material removal rates, cutting tool materials...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870307
EISBN: 978-1-62708-314-0
... machined or rolled. Some nuts are self-locking and others are not; cotter pins and safety wire are used to secure those that are not. Self-aligning nuts (up to eight degrees) are also available for situations in which the structural members are not parallel. There are also nuts designed specifically for...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130351
EISBN: 978-1-62708-284-6
... the vendor for rework, while others were reworked in-house. The pins were machined from 300M steel. The pins were then heat treated to a strength range of 1930 to 2070 MPa (280 to 300 ksi). The pin was ground and chromium plated. Figure 9 shows the main landing gear (MLG) lever attach pin as...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050191
EISBN: 978-1-62708-311-9
... into various types of tools and track pins manufactured for off-highway equipment. camshaft lobes gears induction surface hardening shafts through hardening SINCE ITS INTRODUCTION in the 1930s, induction heat treatment has been applied to a large variety of mass-produced commercial...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540001
EISBN: 978-1-62708-309-6
... on to analyze the stress state of load-bearing members, pressurized tubes, and pin-loaded lugs, accounting for the effect of geometric discontinuities, such as cutouts, fillets, and holes, as well as cracks. It also explains how finite element methods are used to solve problems involving complex...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860065
EISBN: 978-1-62708-338-6
... machine system and a vertical winding machine. The chapter provides information on in-plane (polar) winders and several types of creels, namely stationary and no twist, rotating, braking, and combinations thereof. Comprehensive descriptions of mandrel designs used in filament winding are presented in text...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040277
EISBN: 978-1-62708-300-3
... not been hardened, and a very high resistance to wear in the hardened state. They are used to form very large cold forgings [ ICFG, 1992 ]. Forging dies or inserts are machined from solid blocks or forged die steels. By using standard support components such as die holders and guide pins...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310095
EISBN: 978-1-62708-326-3
..., free-machining carbon steels, low-alloy manganese steels, low-alloy molybdenum steels, low-alloy chromium-molybdenum steels, low-alloy nickel-chromium-molybdenum steels, low-alloy nickel-molybdenum steels, low-alloy chromium steels, and low-alloy silicon-manganese steels. The chapter provides...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000167
EISBN: 978-1-62708-312-6
... Abstract This chapter describes secondary processes employed in the production of powder-metal stainless steel parts, including various machining operations, welding, brazing, sinter bonding, resin impregnation, re-pressing and sizing, and surface finishing. It also discusses the factors that...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110652
EISBN: 978-1-62708-247-1
... Device Model (CDM) and the so-called Machine Model (MM). Four EOS simulations were developed and applied: (1) programming over-stress (variation of the programming voltage applied to special high voltage pins); (2) forced I/O reverse breakdown (actually BV DSS ); (3a) reverse insertion for dual in-line...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610263
EISBN: 978-1-62708-303-4
... Abstract This chapter discusses the fatigue behavior of bolted, riveted, and welded joints. It describes the relative strength of machined and rolled threads and the effect of thread design, preload, and clamping force on the fatigue strength of bolts made from different steels. It explains...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860035
EISBN: 978-1-62708-338-6
... Abstract This chapter discusses the ways in which the evolution of filament winding software systems has capitalized on the inherent flexibility of computer numerical controlled winding machines and enhanced their productivity. It provides a detailed discussion on different types of geometries...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170003
EISBN: 978-1-62708-297-6
... easier to cast, weld, form, and machine. It also discusses some of the alloying techniques that have been developed to address problems stemming from dissimilarities between the base metal and alloying or inoculate material. alloying mechanical properties Metals are...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.t51180029
EISBN: 978-1-62708-256-3
... latent factors. Failures may also involve multiple parts, entire machines, or processes of any size and shape. The chapter examines the unique aspects of many failures and explains how they can sometimes be traced to systemic issues. It also covers the reasons why products fail, including improper...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
... high-temperature and corrosion behaviors are determined by the orientation, shape, and spacing of fibers, the number of plies, resin properties, and consolidation and forming methods. The chapter also covers secondary fabrication processes, such as thermoforming, machining, and joining, as well as...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720117
EISBN: 978-1-62708-305-8
... Abstract This chapter is a detailed account of the tensile testing procedure used for evaluating metals and alloys. The discussion covers the stress-strain behavior of metals determined by tensile testing, properties determined from testing, test machines for measuring mechanical properties...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850334
EISBN: 978-1-62708-260-0
... Equotip hardness tests, and microindentation tests. It describes the equipment and procedures used, discusses the factors that influence accuracy, and provides hardness conversion equations for different types of materials. It also explains how hardness testing sheds light on anisotropy, machinability...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560165
EISBN: 978-1-62708-291-4
... Abstract A spheroidized structure, which consists of spherically shaped cementite in a matrix of ferrite, is often desired in the production of steel, whether to improve properties, such as machinability and ductility, or accommodate subsequent hardening treatments. This chapter discusses the...