Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170193
EISBN: 978-1-62708-297-6
...Abstract Abstract This article discusses the effect of alloying on high-strength low-alloy (HSLA) steels. It explains where HSLA steels fit in the continuum of commercial steels and describes the six general categories into which they are divided. It provides composition data for standard types...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170587
EISBN: 978-1-62708-297-6
...Abstract Abstract This article discusses the role of alloying in the production and use of low-expansion alloys such as iron-nickel (Invar), iron-nickel-chromium (Elinvar), and iron-nickel-cobalt (Super-Invar and Kovar). It explains how the coefficient of thermal expansion varies with nickel...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820013
EISBN: 978-1-62708-339-3
...Carbon steels classified according to carbon content Table 1 Carbon steels classified according to carbon content Carbon, % Low-carbon steel Mild steel Medium-carbon steel High-carbon steel Ref ≤0.15 0.15–0.30 0.30–0.50 0.50–1.00 1 ≤0.15 0.15–0.35 0.35–0.60 0.60...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140211
EISBN: 978-1-62708-335-5
... with ASTM E 8 and E 21, with 0.5 in. (12.5 mm) diam tensile specimens per Appendix 3, Fig. A3.1 . In most cases, the specimens were as-cast test bars. Yield strengths were measured at 0.2% offset using autographic extensometers; in the tests at high and low temperatures, the extensometers were used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270067
EISBN: 978-1-62708-301-0
...Abstract Abstract A low-pressure turbine rotor blade failed in service, causing extensive engine damage. A section of the blade broke off around 25 mm from the root platform, producing a flat fracture surface that appeared smooth on one end and grainy elsewhere. Based on their examination...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270143
EISBN: 978-1-62708-301-0
...Abstract Abstract A low-pressure turbine rotor blade failed during a test run, causing extensive damage to an aircraft engine. Visual examination showed that the nickel-base superalloy blade broke above the root platform in the airfoil section, leaving a fracture surface with two distinct...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
...Abstract Abstract This appendix is a collection of tables listing coefficients of linear thermal expansion for carbon and low-alloy steels, presenting a summary of thermal expansion, thermal conductivity, and heat capacity; and listing thermal conductivities and specific heats of carbon and low...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090043
EISBN: 978-1-62708-266-2
...Abstract Abstract This chapter addresses the issue of stress-corrosion cracking (SCC) in carbon and low-alloy steels. It discusses crack initiation, propagation, and fracture in aqueous chloride, hydrogen sulfide, sulfuric acid, hydroxide, ammonia, nitrate, ethanol, methanol, and hydrogen gas...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.9781627083485
EISBN: 978-1-62708-348-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140055
EISBN: 978-1-62708-264-8
...Abstract Abstract Steels contain a wide range of elements, including alloys as well as residual processing impurities. This chapter describes the chemical composition of low-alloy AISI steels, which are classified based on the amounts of chromium, molybdenum, and nickel they contain...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410233
EISBN: 978-1-62708-265-5
... This chapter discusses various alloying and processing approaches to increase the strength of low-carbon steels. It describes hot-rolled low-carbon steels, cold-rolled and annealed low-carbon steels, interstitial-free or ultra-low carbon steels, high-strength, low-alloy (HSLA) steels, dual-phase...