Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780131
EISBN: 978-1-62708-268-6
...Abstract Abstract Leaks can occur as the result of several failure causes. This chapter reviews the causes, features, and impact of various types of leaks, namely gasket leaks, O-ring leaks, bond-joint leaks, weld leaks, polyvinyl chloride leaks, valve leaks, and structural leaks. bond...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270126
EISBN: 978-1-62708-301-0
...Abstract Abstract A test flight was cut short after a fire warning came on indicating a problem with one of the four engines on an aircraft. A visual examination following the precautionary landing revealed several burned hoses, a melted bolt, and fuel leaking from the base of the main burner...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720293
EISBN: 978-1-62708-305-8
..., and dimensional inspection. Casting defects including porosity, oxide films, inclusions, hot tears, metal penetration, and surface defects are reviewed. Liquid penetrant inspection, magnetic particle inspection, eddy current inspection, radiographic inspection, ultrasonic inspection, and leak testing for castings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720411
EISBN: 978-1-62708-305-8
... of nondestructive inspection of weldments including visual inspection, liquid penetrant inspection, magnetic particle inspection, radiographic inspection, ultrasonic inspection, leak testing, and eddy current and electric current perturbation inspection. The chapter also describes the properties of brazing filler...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860515
EISBN: 978-1-62708-348-5
... and auxiliary materials. Areas of frequent concern, such as thermal contact, heat leak, thermal anchoring, thermal conductivity of greases, insulators, lead wires, ground loops, and feedthroughs are also reviewed. The chapter provides an overview and historical development of temperature scales because...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900039
EISBN: 978-1-62708-350-8
... configuration and design. It also covers the processes involved in the construction and maintenance of retorts, methods for sealing a retort to prevent ammonia leaks, and safety precautions to be taken while using ammonia. Further, the chapter provides information on the factors for choosing a heating medium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030089
EISBN: 978-1-62708-282-2
... • Lampman S. , Ed., Weld Integrity and Performance , ASM International , 1997 SCC in Oil Refineries Leaking Carbon Steel Weldments in a Sulfur Recovery Unit Corrosion of Welds in Carbon Steel Deaerator Tanks Weld Cracking in Oil Refinery Deaerator Vessels Investigation Preventive...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050293
EISBN: 978-1-62708-311-9
... supply is beneficial. The examination should include inspection for water leaks from hose connections and signs of discoloration on copper bus, tube connections in oscillator sets, and any signs of oil leaks from capacitors. The studs and taps on any heat station component, such as capacitors...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870101
EISBN: 978-1-62708-314-0
... duplicate tools. On the downside, there has been a lot of negative experience with composite tools that are subject to 350 °F (175 °C) autoclave cure cycles: The matrix has a tendency to crack, and with repeated thermal cycles it can develop leaks. Another consideration when specifying composite tools...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780093
EISBN: 978-1-62708-268-6
..., leak paths, and other conditions not readily apparent using visual or other assessment techniques. Techniques in this area include x-ray and n-ray radiography, dye penetrant inspection, fluorescent dye pressure testing, and magnafluxing. Mechanical and environmental approaches for evaluating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780193
EISBN: 978-1-62708-268-6
... Visual examination, microscopic examination, x-ray Leaking X-ray inspection for porosity, dimensional inspection, tolerance analysis for adequate seal/gasket squeeze, visual and microscopic examination for presence of contaminants or cuts on seals, materials analysis to confirm correct seal/ gasket...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820013
EISBN: 978-1-62708-339-3
... Chromium-Molybdenum Steels Welding Processes SCC Due to Welding Residual Stresses Stress-Corrosion Cracking of C-Mn Steel in a CO<sub>2</sub> Absorber in a Chemical Plant <xref ref-type="bibr" rid="t51820013-ref19">(Ref 19)</xref> SCC Due to Nitrates SCC in Oil Refineries Leaking Carbon...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630211
EISBN: 978-1-62708-270-9
... surface of a 12-in.-diameter crude oil pipeline that experienced an in-service leak. (b) Metallographic cross section of the leak location showing undercutting within the pit, a pitting morphology that is typically associated with MIC. Fig. 6 Stress-corrosion crack in thin neck of a cartridge...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820077
EISBN: 978-1-62708-339-3
... Considerations Corrosion Behavior Group I Alloys Group II Alloys Group III Alloys Mechanical Properties Corrosion Resistance Hydrogen Embrittlement Intergranular Corrosion Avoiding Intergranular Corrosion Example 1: Leaking Welds in a Ferritic Stainless Steel Wastewater Vaporizer...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110563
EISBN: 978-1-62708-247-1
...-633 8235/Helium-kill-iPhone-Hospital-finds-gas-leaks-completely-disabled-Apple-phones-watches.html , Oct. 31 , 2018 . [65] Huang C-A. , Fang SK , Hsu K. , “ The integration metrology analysis tools of MEMS multi-bonding interface inspection solution ”, 2017 IEEE 24th Int'l...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500157
EISBN: 978-1-62708-317-1
... defects in SHF-P include: Excessive thinning leading to fracture Flange wrinkles leading to leaking of the pressurizing medium Sidewall wrinkles Excessive bulging leading to fracture ( Fig. 8.18a ) Surface marks ( Fig. 8.18b ). Fig. 8.18 Bulge formation in sheet hydroforming...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000185
EISBN: 978-1-62708-312-6
... after 10 years and/or 100,000 miles, with only minor amounts of rust and no loss of mechanical strength ( Ref 10 ). For aesthetic purposes, these rings can be nickel or chrome plated to give them a rust-free appearance. Because of stricter environmental regulations (no-leak exhaust systems...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910427
EISBN: 978-1-62708-250-1
... temperature pattern as indicator of physical state of object Used most effectively on refractory and insulation furnace tube inspection. Requires specialized skill. Instrumentation is costly. Infrequent Acoustic emission Leaks, collapse of cavitation, bubbles, by vibration level in equipment. Cracks...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270059
EISBN: 978-1-62708-301-0
... of inquiry concluded that when the leaking reactor No. 5 was replaced by a dog-leg pipe with bellows at the two ends, to bridge reactors 4 and 6, there was no proper design study, no proper consideration for the need for a support, no safety testing, no reference to the relevant standards, and no reference...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430351
EISBN: 978-1-62708-253-2
... of a tube at a few millimeters distance from the leak indicating metal wastage on outer surface. (b) Poor quality of welding with porosities and deep ripples, 6× Fig. 6.170 (a) ID microstructure away from puncture location consisting of fine-grained ferrite and pearlite with shallow pits, 100×. (b...