Skip Nav Destination
Close Modal
Search Results for
laser dimpling
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 21 Search Results for
laser dimpling
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110323
EISBN: 978-1-62708-247-1
... Optical microscope images taken from a unit both before (left) and after (right) the dimpling process was performed. The contrast observed in these images is used to determine the endpoint for the dimpling process. Figure 8 A SEM image from the surface of a sample after the dimpling process...
Abstract
This article presents methods that enable one to consistently, uniformly and quickly remove substrate silicon from units without imparting damage to the structure of interest. It provides examples of electron beam probing and backside nano-probing techniques. The electron beam probing techniques are E-beam Logic State Imaging, Electron-beam Signal Image Mapping, and E-beam Device Perturbation. Backside nano-probing techniques discussed include: Electron Beam Absorbed Current, Electron Beam Induced Resistance Change, four terminal resistance measurements, resistive gate defect identification, and circuit editing. The article also presents methods to prepare electron beam probing samples where some remaining silicon is required for the transistor functions and transmission electron microscope samples from units where the substrate silicon has been partially or completely removed.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700177
EISBN: 978-1-62708-279-2
... ( Ref 12.13 ). Provided the welding parameters are adjusted, DP, complex-phase (CP), and TRIP steels can be welded using conventional resistance spot welding processes on commercial spot welding machines. Laser welding of the three steels showed no particular difficulties or problems ( Ref 12.14...
Abstract
This chapter describes the nature of the problems arising from using advanced high-strength steels (AHSS) and discusses potential remedies to minimize the adverse effects that may limit the adoption of AHSS in the automotive industry. The discussion provides information on press energy, springback, residual stress, die wear, hot forming, downgaging limits, welding, binders, draw beads, and tool material wear.
Book Chapter
Book: Systems Failure Analysis
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780093
EISBN: 978-1-62708-268-6
... test to determine if the material is of the specified hardness. The approach for testing hardness is straightforward and is called a Rockwell hardness test. A hardened or diamond-tipped punch is pressed against the specimen surface with a known force to form a dimple. Softer materials have bigger...
Abstract
After the fault-tree, a failure-cause identification method has identified potential failure causes and the failure analysis team has prepared a failure mode assessment and assignment (FMA&A). The team knows specifically what to search for when examining components and subassemblies from the failed system. There are numerous techniques and technologies available for examining and analyzing components and subassemblies, which are categorized as follows: optical approaches, dimensional inspection and related approaches, nondestructive test approaches, mechanical and environmental approaches, and chemical and composition analysis for assessing material characteristics. This chapter is a detailed account of the working principle and the steps involved in these techniques and technologies.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700071
EISBN: 978-1-62708-279-2
... is to increase its second moment of inertia through corrugating or dimpling of the sheet metal. Corrugation or dimpling allows the reduction of thickness for weight savings without compromising stiffness ( Ref 4.2 ). Advanced high-strength steels offer greater design flexibility to optimize the stiffness...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270031
EISBN: 978-1-62708-301-0
... be derived ( Ref 7 ). The true length of a feature is the measured length multiplied by R L , and the true area is the measured projected area multiplied by R S . A typical application is quantitative measurement of dimple size from SEM photomicrographs. Measurements made directly on the SEM picture...
Abstract
This chapter discusses some of the more advanced methods and procedures used in failure analysis, including in-service material sampling, in situ microstructure analysis, and a form of punch testing that can determine the fracture toughness of any material from a tiny specimen. The chapter also covers quantitative fractography, fracture surface topography analysis, and the use of oxide dating as well as fault tree and failure modes and effects analysis (FMEA) and computational techniques.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610209
EISBN: 978-1-62708-303-4
...: Ref 4 Fig. 6 Scanning electron microscopy view of the surface of the tensile test fracture in 18% Ni, grade 300 maraging steel, showing a portion of the central zone of the fracture, close to the origin. The surface here is composed of equiaxed dimples of two sizes. The large dimples...
Abstract
This chapter provides information and data on the fatigue and fracture properties of steel, aluminum, and titanium alloys. It explains how microstructure, grain size, inclusions, and other factors affect the fracture toughness and fatigue life of these materials and the extent to which they can be optimized. It also discusses the effect of metalworking and heat treatment, the influence of loading and operating conditions, and factors such as corrosion damage that can accelerate crack growth rates.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110563
EISBN: 978-1-62708-247-1
.... Figure 20 a) Reflected light and b) LSIM image using a 5mW, 540nm laser. A bottom level comb finger from a stack of three shown shorting to the ground plane is identified. Figure 21 Bump structure in a MEMS microphone. Figure 22 a) Cross section of a CMUT; b) Magnification...
Abstract
This chapter discusses the various failure analysis techniques for microelectromechanical systems (MEMS), focusing on conventional semiconductor manufacturing processes and materials. The discussion begins with a section describing the advances in integration and packaging technologies that have helped drive the further proliferation of MEMS devices in the marketplace. It then shows some examples of the top MEMS applications and quickly discusses the fundamentals of their workings. The next section describes common failure mechanisms along with techniques and challenges in identifying them. The chapter also provides information on the testing of MEMS devices. It covers the two common challenges in sample preparation for MEMS: decapping, or opening up the package, without disturbing the MEMS elements; and removing MEMS elements for analysis. Finally, the chapter discusses the aspects of failure analysis techniques that are of particular interest to MEMS.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630035
EISBN: 978-1-62708-270-9
... significant feature is that the compressive residual stresses force the grains of metal in the indentation to squeeze together, exactly as the stones of the arch are pressed together by the weight of the stone blocks above. If the entire surface is mechanically dimpled with many small indentations...
Abstract
Residual, or locked-in internal, stresses are regions of misfit within a metal part or assembly that can cause distortion and fracture just as can the more obvious applied, or service, stresses. This chapter describes the fundamental facts about residual stresses and discusses the basic mechanisms of residual stress formation: thermal, transformational, mechanical, and chemical.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.9781627083164
EISBN: 978-1-62708-316-4
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
..., plasma, laser, electron beam Furnace, induction, flame, infrared, chemical reaction, flame Soldering iron, ultrasonic, infrared, flame, resistance, oven Furnace, resistance, pressure deformation, exploration, friction, flame Chemical reaction, oven, or not applicable Usually not required Typical...
Abstract
This chapter describes the processes involved in the fabrication of wrought and cast metal products. It discusses deformation processes including bending and forming, material removal processes such as milling, cutting, and grinding, and joining methods including welding, soldering, and brazing. It also discusses powder consolidation, rolling, drawing and extrusion, and common forging methods.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460253
EISBN: 978-1-62708-285-3
... treatments were performed using a tube furnace with an argon atmosphere. A wide range of characterization methods was employed, including, among others, powder size as measured by laser diffraction; powder flowability by Metal Powder Industries Federation standard 03; chemical analysis by inert gas fusion...
Abstract
The Nuclear Waste Management Organization (NWMO) investigates approaches for managing Canada's used nuclear fuel. As part of a larger program investigating concepts of copper coatings, NWMO has begun exploring copper cold spray in collaboration with the National Research Council. Within the coating program, a large variety of copper coating sizes have been investigated, from small corrosion coupons to full-scale used-fuel containers/canisters (UFCs). This chapter demonstrates the successful application of copper coating technology to full-scale geometric representative Mark II UFC mock-up configurations through activities involving powder selection, general coating development, UFC coating optimization, and prototyping.
Book Chapter
Book: Principles of Brazing
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230001
EISBN: 978-1-62708-351-5
... to joining. 1.1.4 Welding Welding involves the fusion of the joint surfaces by controlled melting through heat being directed specifically toward the joint. Commonly used heating sources are plasma arcs, electron beams, lasers, and electrical current that is passed through the components and across...
Abstract
Brazing and soldering jointly represent one of several methods for joining solid materials. This chapter summarizes the principal characteristics of the various joining methods. It then discusses key parameters of brazing including surface energy and tension, wetting and contact angle, fluid flow, filler spreading characteristics, surface roughness of components, dissolution of parent materials, new phase formations, significance of the joint gap, and the strength of metals. The chapter also describes issues in processing aspects that must be considered when designing a joint, and the health, safety, and environmental aspects of brazing.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.9781627083515
EISBN: 978-1-62708-351-5
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000059
EISBN: 978-1-62708-313-3
Abstract
This chapter discusses the typical compositional ranges of superalloys, the role of major base metals (iron, cobalt, and nickel), and the effects of common alloying additions. It describes how chromium, aluminum, and titanium as well as refractory elements, grain-boundary elements, reactive elements, and oxides influence mechanical properties and behaviors. It also discusses the effect of trace elements.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.9781627083003
EISBN: 978-1-62708-300-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.9781627083041
EISBN: 978-1-62708-304-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130177
EISBN: 978-1-62708-284-6
... Peening, Conference Proceedings of ICSP-2 , 194 , p 208 – 214 60. Herring D.H. , A Tutorial on Shot Blasting and Shot/Laser Peening , Ind. Heat. , Vol 73 ( No. 8 ), Aug 2006 , p 20 – 22 61. “ Shot Peening and Shot Blasting ,” OSKKiefer GmbH , Oberflächen and Strahltechnik...
Abstract
This chapter provides information on various contributors to failure of carburized and carbonitrided components, with the primary focus on carburized components. The most common contributors covered include component design, selection of proper hardenability, increased residual stress, dimensional stability, and generation of quenching and grinding cracks. They also include insufficient case hardness and improper core hardness, influence of surface carbon content and grain size, internal oxidation, structure of carbides, and inclusion of noncarbide. Details on micropitting, macropitting, case crushing, pitting corrosion, and partial melting are also provided.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
Abstract
This chapter provides details on powder-binder processing for three materials, namely precipitation-hardened 17-4 PH stainless steel, cemented carbides, and alumina. The types of powders, binders, feedstock, shaping processes, debinding, sintering cycles, compositions, microstructure, distortion, postsintering treatments, and mechanical properties are presented for each. The shaping options include powder-binder approaches such as binder jetting, injection molding, extrusion, slip and slurry casting, centrifugal casting, tape casting, and additive manufacturing. Sintering options are outlined with respect to attaining high final properties.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.9781627082532
EISBN: 978-1-62708-253-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.9781627082600
EISBN: 978-1-62708-260-0