Skip Nav Destination
Close Modal
Search Results for
laser deposition
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 156 Search Results for
laser deposition
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410551
EISBN: 978-1-62708-265-5
... laser and electron beams. The chapter compares methods and includes several example applications. chemical vapor deposition electron beam melting ion implantation laser melting low-pressure carburizing physical vapor deposition plasma carburizing plasma nitriding salt bath coating surface...
Abstract
This chapter describes surface modification processes that go beyond conventional heat treatments, including plasma nitriding, plasma carburizing, low-pressure carburizing, ion implantation, physical and chemical vapor deposition, salt bath coating, and transformation hardening via high-energy laser and electron beams. The chapter compares methods and includes several example applications.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 1998
DOI: 10.31399/asm.tb.ts5.t65900305
EISBN: 978-1-62708-358-4
... Abstract Surface modification technologies improve the performance of tool steels. This chapter discusses the processes involved in oxide coatings, nitriding, ion implantation, chemical and physical vapor deposition processing, salt bath coating, laser and electron beam surface modification...
Abstract
Surface modification technologies improve the performance of tool steels. This chapter discusses the processes involved in oxide coatings, nitriding, ion implantation, chemical and physical vapor deposition processing, salt bath coating, laser and electron beam surface modification, and boride coatings that improve the performance of hot-work and high-speed tool steels.
Image
Published: 01 October 2012
Fig. 5.20 Laser-additive manufacturing process. (a) Powder feed stock is added by gas jets to the melt pool formed by laser. (b) Direct metal deposition of titanium foil shape. Courtesy of S. Kelly, Pennsylvania State University. Source: Ref 5.11
More
Image
in Melting, Casting, and Powder Metallurgy[1]
> Titanium: Physical Metallurgy, Processing, and Applications
Published: 01 January 2015
Fig. 8.51 Ultimate tensile strength (UTS), yield strength (YS), and elongation of Ti-6Al-4V alloy produced using various additive manufacturing processes. DMD, direct-metal deposition; HIP, hot isostatic pressing; HT, heat treatment; LENS, laser-engineered net shaping ( Ref 8.16 ); DMLS
More
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290079
EISBN: 978-1-62708-306-5
... can have an effect on the deposited GMAW bead. In the laser-leading configuration, the GMAW torch is traveling behind the laser beam, positioned at a “push angle.” In the arc-leading configuration, the torch is at a “drag angle,” traveling in front of the laser beam. This difference in torch angle can...
Abstract
This chapter discusses the fusion welding processes, namely oxyfuel gas welding, oxyacetylene braze welding, stud welding (stud arc welding and capacitor discharge stud welding), high-frequency welding, electron beam welding, laser beam welding, hybrid laser arc welding, and thermit welding.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500317
EISBN: 978-1-62708-317-1
... hardening, case (surface) hardening, and nitriding as well as hard chrome plating, vapor deposition, and thermal diffusion coating. It explains how to measure wear resistance using various tests and provides guidelines for selecting tool materials, treatments, and coatings. chemical vapor deposition...
Abstract
This chapter discusses the types of failures that can occur in sheet metal forming tools and explains how to mitigate their effects. It describes the factors that influence galling and wear and the benefits of special treatments and coatings. It provides information on through hardening, case (surface) hardening, and nitriding as well as hard chrome plating, vapor deposition, and thermal diffusion coating. It explains how to measure wear resistance using various tests and provides guidelines for selecting tool materials, treatments, and coatings.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
... deposition. The precipitation or plating-out of a metal from so- lutions of its salts through the introduction of another metal or reagent to the solution. chemical polishing. A process that produces a polished surface by the ac- tion of a chemical etching solution. The etching solution is com- pounded so...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... Localized surface hardening (flame, induction, laser, and electron-beam hardening) Improved wear resistance through the development of a hard martensitic surface Laser melting Improved wear resistance through grain refinement and the formation of fine dispersions of precipitates Shot peening...
Abstract
This chapter begins with a brief review of the different types of surface treatments and coatings used in industry and their effect on properties and performance. It then discusses the importance of corrosion and wear treatments and the consequences of failing to properly implement them in critical industries such as mining, energy production, transportation, and mineral and chemical processing. The chapter also describes basic approaches to dealing with corrosion and wear in steel.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... protective linings barrier protection chemical inhibition galvanic protection surface preparation inspection quality assurance electroplating electroless plating hot dipping thermal spraying cladding pack cementation vapor deposition ion implantation laser processing COATINGS are the most...
Abstract
Organic coatings (paints and plastic or rubber linings), metallic coatings, and nonmetallic inorganic coatings (conversion coatings, cements, ceramics, and glasses) are used in applications requiring corrosion protection. These coatings and linings may protect substrates by three basic mechanisms: barrier protection, chemical inhibition, and galvanic (sacrificial) protection. This chapter begins with a section on organic coating and linings, providing a detailed account of the steps involved in the coating process, namely, design and selection, surface preparation, application, and inspection and quality assurance. The next section discusses the methods by which metals, and in some cases their alloys, can be applied to almost all other metals and alloys: electroplating, electroless plating, hot dipping, thermal spraying, cladding, pack cementation, vapor deposition, ion implantation, and laser processing. The last section focuses on nonmetallic inorganic coatings including ceramic coating materials, conversion coatings, and anodized coatings.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120131
EISBN: 978-1-62708-269-3
... alloy components. A related process is the laser forming of titanium components, which is claimed to reduce lead times for the fabrication of complex titanium structures by 50 to 75%. Lasform is the name for a direct metal deposition process that combines high-power laser cladding technologies...
Abstract
This chapter discusses some of the promising developments in the use of titanium, including titanium aluminides, titanium matrix composites, superplastic forming, spray forming, nanotechnology, and rapid solidification rate processing. It also reports on efforts to increase the operating temperature range of conventional titanium alloys and reduce costs.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... heating, laser heating, and radiation). The depositing species (clusters of atoms or molecules) have relatively low energies (less than five electron volts, or eV). Relatively high deposition rates are attainable. The process is generally performed in vacuum, typically at 10 –3 to 10 –4 Pa (10 –5 to 10...
Abstract
This chapter discusses coating technologies that are applicable to beryllium, including physical and chemical vapor deposition, thermal evaporation, electroplating, sputtering, ion plating, and plasma arc spraying. It describes the advantages and disadvantages of each method and the effect of temperature, pressure, and other process variables on the microstructures and properties developed.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460173
EISBN: 978-1-62708-285-3
... spray powders. Due to the nature of the cold spray process, there are several properties that the powder must have. In general, powder properties have a strong influence on two process phenomena: powder feeding/spraying and layer deposition. Powder feeding/spraying is mainly influenced...
Abstract
Increasing growth of high-pressure cold spraying applications on the industrial scale have forced global powder producers to face this challenge and develop specific powders for cold spray applications. This chapter provides information on the properties, classification, characteristics, manufacturing, and procedures for packaging of powders specific to cold spray applications.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110524
EISBN: 978-1-62708-247-1
... structure is determined by the masks used during wafer processing. The first step in making a laser is epitaxial growth, usually in a high-temperature reactor with metal-organic chemical vapor deposition (MOCVD) depositing a few microns of material on a GaAs or InP substrate. In this step, cladding...
Abstract
Optoelectronic components can be readily classified as active light-emitting components (such as semiconductor lasers and light emitting diodes), electrically active but non-emitting components, and inactive components. This chapter focuses on the first category, and particularly on semiconductor lasers. The discussion begins with the basics of semiconductor lasers and the material science behind some causes of device failure. It then covers some of the common failure mechanisms, highlighting the need to identify failures as wearout or maverick failures. The chapter also covers the capabilities of many key optoelectronic failure analysis tools. The final section describes the common steps that should be followed so as to assure product reliability of optoelectronic components.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110379
EISBN: 978-1-62708-247-1
... layers of material in order to locate and identify the area of interest. Several of the top-down delayering techniques include wet chemical etching, dry reactive ion etching, top-down parallel lapping (including chemical-mechanical polishing), ion beam milling and laser delayering techniques...
Abstract
With semiconductor device dimension continuously scaling down and increasing complexity in integrated circuits, delayering techniques for reverse engineering is becoming increasingly challenging. The primary goal of delayering in semiconductor failure analysis is to successfully remove layers of material in order to locate and identify the area of interest. Several of the top-down delayering techniques include wet chemical etching, dry reactive ion etching, top-down parallel lapping (including chemical-mechanical polishing), ion beam milling and laser delayering techniques. This article discusses the general procedure, types, advantages, and disadvantages of each of these techniques. In this article, two types of different semiconductor die level backend of line technologies are presented: aluminum metallization and copper metallization.
Book Chapter
Book: Systems Failure Analysis
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780141
EISBN: 978-1-62708-268-6
... subtle. This chapter summarizes a few commonly encountered contaminant sources to stimulate the reader's thinking about potential contaminant sources. A case study of titanium component washing at Litton Lasers is presented to illustrate how the presence of contaminants leads to a system failure...
Abstract
Contaminants can be a cause of numerous types of system failures. There are numerous techniques for confirming contaminant presence. When the presence of a contaminant is suspected, the failure analysis team must find and eliminate the contaminant source, which can be obvious or quite subtle. This chapter summarizes a few commonly encountered contaminant sources to stimulate the reader's thinking about potential contaminant sources. A case study of titanium component washing at Litton Lasers is presented to illustrate how the presence of contaminants leads to a system failure.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930365
EISBN: 978-1-62708-359-1
..., oxyacetylene. Filler rods 3.5C-3Si-0.6P Ferritic gray irons are readily welded but complex irons are difficult to weld. Increasing silicon above 2% also decreases weldability. Preheat to 400–600 °C or to 1000 °C with 60/40 brass filler (bronze welding). Preheat to avoid hard brittle deposit. Difficult...
Abstract
This appendix provides reference tables listing weldability of cast irons, steels, and nonferrous metals. A process selection table for arc welding carbon steels is included, and recommended preheat and interpass temperature tables are also presented. This appendix includes information on qualification codes and standards.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... recently developed coatings or surface modifications—such as chemical vapor deposition (CVD), physical vapor deposition (PVD), ion implantation, and laser melting, alloying, or cladding—are also performed by companies that specialize in these processes/coatings. For example, most cutting tool manufacturers...
Abstract
This chapter compares and contrasts surface-engineering processes based on process availability, corrosion and wear performance, distortion effects, penetration depth or attainable coating thickness, and cost. It provides both quantitative and qualitative information as well as measured property values.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.9781627083591
EISBN: 978-1-62708-359-1
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... carbon; PVD, physical vapor deposition; HVOF, high-velocity oxyfuel; PAS, plasma arc spraying; EB, electron beam; SMAW, shielded metal arc welding; OAW, oxyacetylene welding Figure 12.1 is also an estimate of the relative size of the technology components that comprise the material-modification...
Abstract
This chapter covers coatings and treatments that are used to improve the friction and wear behaviors of materials. It describes modifications that work by hardening contacting surfaces, including heat treating, vacuum coating, thermal spray, and plating, and those that separate or lubricate surfaces, including solid film, chemical conversion, and vacuum coatings, surface oiling and texturing, and lubricating platings. It compares and contrasts methods based on thickness and depth and their relative effect on friction, erosion, and wear.