1-7 of 7 Search Results for

isopleth plots

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420191
EISBN: 978-1-62708-310-2
...-D ternary plot, the information from the diagrams can be plotted in two dimensions by any of several methods, including the liquidus plot, the isothermal plot, and a vertical section called an isopleth. Fig. 10.2 Hypothetical ternary phase diagram. Binary phase diagrams are present along...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310281
EISBN: 978-1-62708-286-0
... plotted and attributed to a software package called Thermo-Calc. The purpose of this appendix is to give a brief introduction to Thermo-Calc, explain what it is, and what are its uses. Also provided are instructions for accessing a demonstration version of the software. What is Thermo-Calc? Thermo...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420263
EISBN: 978-1-62708-310-2
... of the Zr-Cu-Ni-Al-Ti system, the liquidus temperature was found to decrease rapidly from the quaternary alloy Zr 56.28 Cu 31.3 Ni 4.0 Al 8.5 (at.%) due to the addition of titanium. Further calculation of several isopleths revealed that the liquidus temperature decreased the fastest when zirconium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310091
EISBN: 978-1-62708-286-0
... steels. Without being able to computer model the thermodynamics of the system, it would be impossible to project the partitioning of the various potential alloying elements. Figure 3 shows isopleth diagrams for a basic 2205 composition in which nickel is varied. Fig. 3 The iron-nickel diagram...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440145
EISBN: 978-1-62708-352-2
.... The linear expansion coefficient, α, plotted against the thermal conductivity, λ. The contours show the thermal distortion parameter λ/α. Fig. 4.9 General relationship between coefficient of thermal expansion, or CTE (between 273 and 373 K), and melting point for metals, T m . Adapted from Li...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230047
EISBN: 978-1-62708-351-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0