Published: 30 September 2023
Figure 12.22: Schematic illustration of the ironing process. Ironing is commonly done in two or three passes using multiple rings. Arrows indicate directions of friction stresses acting on cup. More
Image
Published: 01 August 2012
Fig. 2.35 Ironing. Source: Ref 2.4 More
Image
Published: 01 August 2012
Fig. 7.12 Schematic of ironing test. F a , F r , F t , F n = forces in axial, radial, tangential to die surface, and normal to surface directions, respectively. Source: Ref 7.19 More
Image
Published: 01 August 2012
Fig. 7.13 Comparison of sidewall thinning distributions obtained from the ironing tests with different lubricants (Lub); curvilinear length (C.L.). Source: Ref 7.19 More
Image
Published: 01 August 2012
Fig. 8.8 Schematic of the ironing process. Source: Ref 8.4 More
Image
Published: 01 August 2012
Fig. 8.9 Punch force/punch stroke diagram: ironing process combined with forming. Source: Ref 8.3 More
Image
Published: 01 November 2013
Fig. 39 Drawing with a moving mandrel (the ironing process). Source: Ref 12 More
Image
Published: 01 February 2005
Fig. 2.15 Ironing operation More
Image
Published: 30 September 2023
Figure 2.3: Examples of the beneficial effects of friction. (a) On the punch in ironing; (b) entraining a new billet in rolling; (c) on the roll surface during steady state rolling. More
Image
Published: 30 September 2023
Figure 12.23: Effect of lubrication on reduction obtainable in ironing with dies of different half angles. More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320005
EISBN: 978-1-62708-347-8
... Abstract The properties of steel are affected markedly as the percentage of carbon varies. This chapter describes the properties of alloys of iron and carbon, including a review of the iron-carbon phase diagram and, in particular, the portion of the diagram relevant to carbon steels...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220583
EISBN: 978-1-62708-259-4
... Abstract This chapter discusses the effect of composition and cooling rate on the microstructure and properties of cast irons and explains how they differ from steel. It describes the conditions under which white, gray, mottled (chilled), and nodular (ductile) cast irons are produced...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240453
EISBN: 978-1-62708-251-8
... Abstract The properties of cast iron are determined primarily by the form of carbon they contain, which in turn, is controlled by modifying compositions and cooling rates during casting. Certain alloys (such as Si, Al, Ni, Co, and Cu) promote graphite formation, while others (such as S, V, Cr...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730069
EISBN: 978-1-62708-283-9
... Abstract This chapter discusses ferrous metals, including low-carbon steels, stainless steels, and cast irons. It also provides information on hardening and hardenability and the tempering process. hardening tempering ferrous metals hardenability Jominy end-quench testing WHILE...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170021
EISBN: 978-1-62708-297-6
... Abstract This article covers the metallurgy and properties of gray irons. It describes the classes or grades of gray iron, the types of applications for which they are suited, and the corresponding compositional ranges. It discusses the role of major, minor, and trace elements, how...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170062
EISBN: 978-1-62708-297-6
... Abstract This article discusses the metallurgy and properties of ductile cast iron. It begins with an overview of ductile or spheroidal-graphite iron, describing the specifications, applications, and compositions. It then discusses the importance of composition control and explains how various...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170100
EISBN: 978-1-62708-297-6
... Abstract This article explains how malleable iron is produced and how its microstructure and properties differ from those of gray and ductile iron. Malleable iron is first cast as white iron then annealed to convert the iron carbide into irregularly shaped graphite particles called temper...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060247
EISBN: 978-1-62708-261-7
... Abstract The commercial relevance of cast irons is best understood in the context of the iron-carbon phase diagram, where their composition places them near the eutectic point, which sheds light on why they melt at lower temperatures than steel and why they can be cast into more intricate...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140001
EISBN: 978-1-62708-264-8
... Abstract Steels are over 95% Fe, so a good starting point for understanding steel is to study the nature of solid iron. This chapter provides information on the composition, phase transformation, and associated changes in the crystal structure of pure iron at varying temperatures...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140175
EISBN: 978-1-62708-264-8
... Abstract This chapter discusses the composition, properties, microstructure, grain formation, and fracture behavior of gray, white, ductile, and malleable cast iron and how these critical factors are affected when iron is heated to different temperatures prior to or during solidification...