Fig. 7.4 Stress, time, and temperature relationship for alloyed iron casting. Source: Ref 2 More
Image
Published: 01 December 1995
Fig. 10-11 Four in. (102 mm) cutter head converted from a malleable iron casting to a 0.65% carbon steel casting More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320103
EISBN: 978-1-62708-332-4
... Abstract This chapter covers mechanical properties, microstructures, chemical compositions, manufacturing processes, and engineering of gating practices for several applications of gray, white, and alloyed cast irons. It begins with a description of material standards, followed by a section...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320157
EISBN: 978-1-62708-332-4
... guidelines for malleable iron castings. composition iron castings malleabilization malleable iron tensile strength yield strength THE DEVELOPMENT OF MALLEABLE IRON in 1720 was a unique innovation because this new type of iron was strong, tough, machinable, and malleable for piercing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320163
EISBN: 978-1-62708-332-4
... Abstract Ductile iron has far superior mechanical properties compared to gray iron as well as significantly improved castability and attractive cost savings compared to cast steel. This chapter begins with information on graphite morphology and matrix type. It then discusses the advantages...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320195
EISBN: 978-1-62708-332-4
... ADI more widely and with improved success. austemperability austempered ductile iron austempering austenitizing iron castings retained austenite tensile properties UNLIKE CONVENTIONAL QUENCH and temper heat treatment, austempering is an iron and steel heat-treatment process...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320207
EISBN: 978-1-62708-332-4
... Abstract Compacted graphite iron (GCI) is a cast iron grade that is engineered through graphite morphology modifications to achieve a combination of thermal and mechanical properties that are in between those of flake graphite iron and ductile iron. This chapter discusses the advantages...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310331
EISBN: 978-1-62708-326-3
... Abstract Cast irons, like steels, are iron-carbon alloys but with higher carbon levels than steels to take advantage of eutectic solidification in the binary iron-carbon system. Like steel, heat treatment of cast iron includes stress relieving, annealing, normalizing, through hardening...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060247
EISBN: 978-1-62708-261-7
... Abstract The commercial relevance of cast irons is best understood in the context of the iron-carbon phase diagram, where their composition places them near the eutectic point, which sheds light on why they melt at lower temperatures than steel and why they can be cast into more intricate...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240453
EISBN: 978-1-62708-251-8
... Abstract The properties of cast iron are determined primarily by the form of carbon they contain, which in turn, is controlled by modifying compositions and cooling rates during casting. Certain alloys (such as Si, Al, Ni, Co, and Cu) promote graphite formation, while others (such as S, V, Cr...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220583
EISBN: 978-1-62708-259-4
... Abstract This chapter discusses the effect of composition and cooling rate on the microstructure and properties of cast irons and explains how they differ from steel. It describes the conditions under which white, gray, mottled (chilled), and nodular (ductile) cast irons are produced...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140175
EISBN: 978-1-62708-264-8
... Abstract This chapter discusses the composition, properties, microstructure, grain formation, and fracture behavior of gray, white, ductile, and malleable cast iron and how these critical factors are affected when iron is heated to different temperatures prior to or during solidification...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440207
EISBN: 978-1-62708-262-4
... Abstract This chapter is a detailed account of heat treating techniques for cast irons (gray and ductile), providing the reader with a basic understanding of the differences among various types of cast irons and the concept of carbon equivalent. The types of heat treatments discussed are stress...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300179
EISBN: 978-1-62708-323-2
... Abstract This chapter covers the friction and wear behaviors of cast irons. It describes the microstructure and metallurgy of gray, white, malleable, and ductile cast irons, their respective tensile properties, and their suitability for applications involving friction, various types of erosion...
Image
Published: 01 October 2011
Fig. 10.14 Typical carbon and silicon ranges for ductile iron castings More
Image
Published: 01 January 2022
Fig. 7.5 Stress-relieving cycles for iron castings. Source: Ref 2 More
Image
Published: 01 January 2022
Fig. 7.18 Pouring times of two grades of gray iron castings. Source: Ref 6 More
Image
Published: 01 January 2022
Fig. 9.14 Pouring times for ductile iron castings. Source: Ref 2 More
Image
Published: 01 January 2022
Fig. 9.47 Ferritic ductile iron castings for a (a) turbo charger housing and an (b) exhaust manifold More
Image
Published: 30 November 2023
Fig. 3.25 Ductile iron castings shakeout time guide. Source: Ref 15 More