...–3800 2–150 49–71 (C, N) Average to good No 480–1040 900–1900 40–>100 300–>760 10–100 No, except for C Reheat treatment Ion nitriding 51–640 2–25 60–72 Average, poor on stainless steel No 400–570 750–1050 0.027–0.40 0.2–3 10–50 No Grinding (sometimes) TRD process 2.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
..., application, and inspection and quality assurance. The next section discusses the methods by which metals, and in some cases their alloys, can be applied to almost all other metals and alloys: electroplating, electroless plating, hot dipping, thermal spraying, cladding, pack cementation, vapor deposition, ion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240323
EISBN: 978-1-62708-251-8
... charged hydroxyl ions (OH − ) in equal amounts. The metal undergoing electrochemical corrosion need not be immersed in a liquid but may be in contact with moist soil or may just have moist areas on the metal surface. The cathode is the electrode of an electrolytic cell at which reduction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.9781627083027
EISBN: 978-1-62708-302-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610501
EISBN: 978-1-62708-303-4
... metal ions entering the crack solution from the crack walls; and M T + indicates metal ions entering the crack solution from the crack tip. Source: Ref 10 Fig. 19 Experimental crack growth rate as a function of stress intensity for a high-strength steel in humid air. Source: Ref 14...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940271
EISBN: 978-1-62708-302-7
... ferrous ions (Fe 2+ ) to ferric ions (Fe 3+ ) Fe 3+ Manganese oxidizing bacteria Aerobic Oxidize manganous ions (Mn 2+ ) to manganic ions (Mn 3+ ) Mn 3+ Aerobic slime formers (e.g., Pseudomonas ) Aerobic Produce extracellular polymers referred to as “slime.” Slime can prevent oxygen from...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... N10665) is highly resistant to hydrochloric acid (HCl) up to the atmospheric boiling point. However, the presence of small quantities of oxidizing metal ions, such as ferric ion (Fe 3+ ), will result in severe corrosion. Other operating conditions that require definition, especially for equipment used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
... Fig. 2 (a) Pitting and underdeposit attack on underground storage tank. (b) Close-up view of area at left in (a) Abstract Abstract This chapter outlines the step-by-step processes by which materials are selected in order to prevent or control corrosion and includes information on materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
... is a function of concentration and ranges from moderately reducing for dilute acids to more strongly oxidizing for concentrated acids. Deaerated hydrochloric acid is a strongly reducing environment, and the addition of oxidizing species such as dissolved oxygen or ferric (Fe 3+ ) ions will significantly...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
...Selected applications for wrought aluminum alloys Table 2.1 Selected applications for wrought aluminum alloys Alloy Description and selected applications 1100 Commercially pure aluminum highly resistant to chemical attack and weathering. Low cost, ductile for deep drawing, and easy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030292
EISBN: 978-1-62708-282-2
...Abstract Abstract This chapter presents the primary considerations and mechanisms for corrosion and how they are involved in the selection of materials for process equipment in petroleum refineries and petrochemical plants. In addition, specific information on mechanical properties, corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.9781627082532
EISBN: 978-1-62708-253-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
.... References 1 to 4 are general references describing specimen preparation. 2-2 Sample Selection Because sample preparation is time-consuming and involves some expense, adequate attention and thought must be given to the selection of samples with respect to the number, location, and orientation within...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.9781627082600
EISBN: 978-1-62708-260-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490265
EISBN: 978-1-62708-340-9
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6