Published: 01 November 2011
Fig. 4.14 Hybrid laser arc welding variations. Source: Ref 4.9 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290079
EISBN: 978-1-62708-306-5
... Abstract This chapter discusses the fusion welding processes, namely oxyfuel gas welding, oxyacetylene braze welding, stud welding (stud arc welding and capacitor discharge stud welding), high-frequency welding, electron beam welding, laser beam welding, hybrid laser arc welding, and thermit...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
... assembly is used to bond metal and plastic parts after the individual production of each metal and plastic part. Here, welding, gluing, or screwing is used as a bonding process. In in-mold assembly, the prefabricated metal parts are overmolded with the plastic components. However, such hybrid plastic-metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230001
EISBN: 978-1-62708-351-5
... of holding time at 820 °C (1500 °F). Four distinct stages are observed, demonstrating the complexity of the wetting process. [ Weirauch, Jr., and Krafick 1996 ] Fig. 1.6 Schematic showing fundamental steps in the frictional welding process (involving rotational movement). (a) One part or workpiece...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290251
EISBN: 978-1-62708-319-5
...-wattage laser beam (8 W) was able to cut the paper or sinter the plastic particles. Stacking of the layers gave the desired three-dimensional component. Now, additive manufacturing is pushing for similar extensions into metals and ceramics. Also, ideas such as rotational molding and foamed structures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.9781627083515
EISBN: 978-1-62708-351-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390039
EISBN: 978-1-62708-459-8
..., yet virgin surfaces are exposed, partly because of the generation of new surfaces and partly because of asperity plowing. Depending on the material pairing, adhesion may then lead to cold or solid-state welding ; further relative movement (sliding or normal separation of the surfaces) then destroys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... Abstract This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use of weld...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
... also include gravity permanent molding, low-pressure permanent molding, counter pressure, squeeze casting, investment casting, rapid prototype casting, cast forge hybrid, and semisolid metal processes. green sand casting no-bake molding vacuum molding evaporative foam casting gravity...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460227
EISBN: 978-1-62708-285-3
... correctly. The actuator bodies have a long lead time, making a viable repair process essential. Traditional repair processes, such as tungsten inert gas welding, metal inert gas welding, and laser cladding, were possible repair options. These methods are able to produce strengths and porosities that would...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.9781627084598
EISBN: 978-1-62708-459-8
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290261
EISBN: 978-1-62708-319-5
... designed to deliver properties that are a hybrid of the constituent properties. compression. The removal of air from melting feedstock by applying heat and pressure. In a reciprocating screw molding operation, this is achieved by tapering the screw to reduce the space for the feedstock during metering...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
..., and laser processing. The last section focuses on nonmetallic inorganic coatings including ceramic coating materials, conversion coatings, and anodized coatings. corrosion control protective coatings corrosion inhibitors organic coatings metallic coatings nonmetallic inorganic coatings...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440001
EISBN: 978-1-62708-352-2
... slide, sputter metallized with 0.1 μm (4 μin.) of chromium overlaid with 0.1 μm (4 μin.) of gold. Spread ratio is defined in Appendix A1.2 . Fig. 1.5 The strength of pressure-welded joints as a function of the deformation induced during the bonding process. Below the threshold deformation...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.9781627082679
EISBN: 978-1-62708-267-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.9781627083522
EISBN: 978-1-62708-352-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480161
EISBN: 978-1-62708-318-8
... melting, electron beam hearth melting, rammed graphite mold casting, sand casting, investment casting, hot isostatic pressing, weld repair, and heat treatment -- along with related equipment, process challenges, and achievable properties and microstructures. It also explains how titanium parts...