Fig. 10 Corrosion losses of hot-dip coatings in the industrial environment of Bethlehem, PA More
Image
Published: 01 March 2001
Fig. 4 Corrosion losses of hot dip coatings in the industrial environment of Bethlehem, PA. Source: Ref 18 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... Abstract This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use of weld...
Image
Published: 01 March 2002
Fig. 8.49 Hot dipped Galvalume coating on steel. 1% amyl nital. 1000× More
Image
Published: 01 November 2013
Fig. 7 Typical hot dip galvanized coating. Note the gradual transition from layer to layer, which results in a strong bond between base metal and coating. Source: Ref 4 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... protective linings barrier protection chemical inhibition galvanic protection surface preparation inspection quality assurance electroplating electroless plating hot dipping thermal spraying cladding pack cementation vapor deposition ion implantation laser processing COATINGS are the most...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700059
EISBN: 978-1-62708-279-2
... table of the hot mill (for hot rolled products) or in the cooling section of the continuous annealing furnace (for continuously annealed or hot dip coated products). Steels are produced based on annealing the material in the two-phase intercritical temperature region where the carbon content...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
... from alkali hydroxides and such al- kaline salts as borates, carbonates, phosphates, or silicates. The clean- ing action may be enhanced by the addition of surface-active agents and special solvents. aluminizing. Forming of an aluminum or aluminum alloy coating on a metal by hot dipping, hot spraying...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700095
EISBN: 978-1-62708-279-2
... or from the two-phase austenite and ferrite for continuously annealed cold rolled and hot dip coated products. In cold rolled and hot dipped sheets, this microstructure develops by intercritical annealing of the cold rolled sheets followed by quenching to room temperature. Quenching transforms...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040067
EISBN: 978-1-62708-300-3
... such as light upsetting may be completed without lubrication or with a simple mineral oil. In the zinc phosphate coating lubrication system, the basic workpiece material is first cleaned to remove grease and scales and then dipped in a zinc phosphate solution. Through chemical reaction, a zinc phosphate layer...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... resistance and heat resistance Hot-dip galvanizing (zinc coatings) Improved corrosion resistance via sacrificial protection of steel substrate Hot-dip aluminizing Improved corrosion and oxidation resistance of steel substrate Hot-dip lead-tin alloy-coatings (terne coatings) Improved corrosion...
Image
Published: 01 January 2000
Fig. 11 Service life (time to 5% rusting of steel surface) versus thickness of hot dip galvanized (zinc) coating for selected atmospheres Atmosphere Description Heavy industrial atmospheres These contain general industrial emissions such as sulfurous gases, corrosive mists More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
... Corrosion With light loads or low-cycle fatigue, the effects of fatigue will usually be small, and the preferred solution is to reduce the tendency to oxidation by applying an inert coating. Consider the following treatments: Hot dip galvanizing Heavy electrolytic nickel or copper plating...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280079
EISBN: 978-1-62708-267-9
... geometry. The resulting tree is invested (coated) with ceramic of various sizes by dipping the assembled tree in a slurry, applying ceramic granules, and then drying the assembly under controlled conditions. The investing process is carried out for as many times as needed to build up a satisfactory ceramic...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390100
EISBN: 978-1-62708-459-8
... lubricants (emulsions, synthetics, solutions); and a wide range of coatings and carriers. It also discusses solid-film lubricants (oxide films, polymer films, layer-lattice compounds) and environmental and safety concerns. aqueous lubricants coatings compounded lubricants greases metalworking...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030380
EISBN: 978-1-62708-282-2
... (1670 F). alternate-immersion test. A corrosion test in which the specimens are intermittently exposed to a liquid medium at de nite time intervals. aluminizing. Forming of an aluminum or aluminum alloy coating on a metal by hot dipping, hot spraying, or diffusion. amalgam. An alloy of mercury with one...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030165
EISBN: 978-1-62708-282-2
... a barrier between the metal substrate and the environment. In addition, metallic coatings can sometimes provide cathodic protection when the coating is compromised. Metallic coatings and other inorganic coatings are produced using a variety of techniques, including hot dipping, electroplating, cladding...