... quenches, can operate at a high efficiency. An increase of 80 to 90% efficiency is expected with optimization of workpiece production flow. Example 2 involves static heating. Scanners are used when progressive heating is required. Scanners are built for both vertical and horizontal hardening...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050191
EISBN: 978-1-62708-311-9
... speeds and output power may need to be changed as the part moves from the larger diameter to the smaller diameter. Finally, there is substantial application of horizontal scanners to full-length induction hardening of full-length bars and for ball screws. Fig. 10.18 Shaft with changes in diameter...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050025
EISBN: 978-1-62708-311-9
... and current regulation tend to the output power better when there are wide variations in impedance during the heating cycle, such as when a scanner passes over different diameters of a workpiece when heating. Regulation of the power supply is important so that the total power produced into the workpiece...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220253
EISBN: 978-1-62708-341-6
..., individual workpieces are placed on a loading vee by a hydraulic pusher, magazine, or other means. A second device then loads the billet or bar onto the walking beam, where it is “walked” through the line by a series of lifting, horizontal transfer, and lowering motions into consecutive vees in the guidance...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050057
EISBN: 978-1-62708-311-9
... are designed to locate horizontally on the workpiece so that current is induced in the longitudinal direction. Round workpieces are rotated at high speed so that a case can be produced around the diameter. Coils for single-shot heating generally require characterization and usually have flux concentrators...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110485
EISBN: 978-1-62708-247-1
... showing the basic elements and reference axes. In operation, the probe is rastered across the sample surface using piezoelectric actuators to control the fine movements of the system. Two common scanner configurations are: The flexure stage scanner system in which the stage moves in x and y...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050001
EISBN: 978-1-62708-311-9
... could run 2,500 bolts/h for a 14.3 mm ( 9 16 in.) diameter, 3,500 bolts/h for 12 mm (½ in.), and 5,000 bolts/h for 11 mm ( 7 16 in.). Case hardening of full length bars for a steel company was developed in the early 1960s. A horizontal scanning system for case hardening of 38...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050139
EISBN: 978-1-62708-311-9
... more system versatility. The mass of a workpiece is used to self-quench the part ( Fig. 6.10g ). A 4340 steel will quench very effectively in some applications using this technique. Workpieces are pushed horizontally through an induction coil, dropping into a quench tank to be brought out...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400149
EISBN: 978-1-62708-258-7
... is simply a light microscope equipped with a moving specimen stage and a video scanner that records the image of a particular location or field in the specimen. Information obtained from the scanned image is digitized, and many analytical functions are performed by a computer. A typical image analyzer setup...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110228
EISBN: 978-1-62708-247-1
... that is faster than the test loop. The data is smeared in the horizontal scan direction, and the background is averaged into the LADA site data reducing its contrast. In [7] , the authors demonstrated a method of resolving the time of a LADA interaction by measuring the shift of the LADA site when...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980009
EISBN: 978-1-62708-342-3
.... They are produced on horizontal presses and drawn, coiled, or wound to the customers’ desired finished sizes on multispindle wire drawing machines as shown in Fig. 2.1 . The production processes are described in section 5.3 . Other extruded products are anodes used for electrochemical plating with tin...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
...) Continuous weld for horizontal stiffeners prevents traps and crevices from forming. (j) Square sections formed from two L-shape members need to be continuously welded to seal out the external environment. Fig. 1 (Part 2) Examples of how design and assembly can affect localized corrosion by creating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220185
EISBN: 978-1-62708-341-6
.... The simpler of the two employs a simple single-turn or multiturn coil with a separate quench ring which can be mounted on the scanner ( Fig. 8.29a ). For larger production runs, on the other hand, a double-chamber coil which incorporates both coil cooling and quenching capabilities is often the preferred...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090367
EISBN: 978-1-62708-266-2
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2