... Abstract This article describes the general aspects of and practical problems of failure analysis of creep, stress relaxation, and yielding for homogeneous polymers. The effect of temperature and strain rate on the relationship between yield point and elastic modulus and the aging effect...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780105
EISBN: 978-1-62708-281-5
... Abstract This article addresses some established protocols in characterizing thermoplastics, whether they are homogeneous resins, alloyed or blended compositions, or highly modified thermoplastic composites. It begins with a description of various approaches used for the determination...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290085
EISBN: 978-1-62708-319-5
... Abstract This chapter is a detailed account of various attributes related to mixing and testing of powder-binder feedstocks. Mixing parameters and their effects on feedstock properties is discussed. The attributes reviewed include mixture homogeneity, wetting, powder-binder ratio, feedstock...
Image
Published: 01 August 2005
Fig. 7.12 Tensile engineering stress-strain behavior as a function of temperature. (a) Schematic stress-strain curves for a typical polymer tested at four temperatures while the strain rate is kept constant. 1, Low temperature, brittle behavior; 2, intermediate temperature, somewhat ductile; 3 More
Image
Published: 01 November 2012
Fig. 24 Tensile engineering stress-strain behavior as a function of temperature. (a) Schematic stress-strain curves for a typical polymer tested at four temperatures while the strain rate is kept constant. 1, low temperature, brittle behavior; 2, intermediate temperature, somewhat ductile; 3 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540297
EISBN: 978-1-62708-309-6
... mechanics and fracture mechanics tools used for metals are believed to be equally applicable to nonmetals, as long as the substance is homogeneous and isotropic. This chapter briefly discusses the essential features associated with ceramics, glasses, and polymers. Special attention is paid...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290261
EISBN: 978-1-62708-319-5
... as the feedstock is pushed through a small capillary tube. It is useful in determining feedstock ow and homogeneity. carbon control. A measure of the ability to remove the binder polymer without contamination of the powder. Carbon control is quanti ed by the nal carbon level and the uniformity of that level...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050301
EISBN: 978-1-62708-311-9
... furnished in the United States is 60 cycles, or 60 Hz. high frequency. When discussing power supply frequencies, frequencies greater than 100 kHz. homogeneous. Uniform. A homogeneous microstructure is desired in parts for induction hardening. hot-­rolled steel. Hot rolling first reduces all steel bars...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.9781627083119
EISBN: 978-1-62708-311-9
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290001
EISBN: 978-1-62708-319-5
... Abstract This chapter provides an introduction to powder processing of binders and polymers. It sets the context for the remainder of the book by providing an overview of the topics discussed in the subsequent chapters and by providing introduction to powder-binder fabrication and customization...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610327
EISBN: 978-1-62708-303-4
... applicable to nonmetals, as long as the substance is homogeneous and isotropic. This chapter briefly discusses the essential features associated with ceramics and polymers. Special attention is paid to the characteristics of these materials as compared to metals. Ceramics Ceramics are inorganic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030245
EISBN: 978-1-62708-349-2
..., resulting in changes in microstructure and properties. Composite conductivity, however, is not as homogeneous as in metals. In carbon-fiber-reinforced composites, the fibers are electrically conductive, but these are surrounded by an electrically insulating polymer matrix. As a result, the electrical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780404
EISBN: 978-1-62708-281-5
... the origin to the point of fracture, which coincidentally occurs at approximately the same strain as yielding in a ductile polymer. Except for a slight decrease in slope immediately before fracture, the deformation may be considered linearly elastic. Hooke’s law for a homogeneous, isotropic material can...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780267
EISBN: 978-1-62708-281-5
... Abstract This article provides details on several of the classifications of polymer wear mechanisms, using wear data and micrographs from published works. The primary goals are to present the mechanisms of polymer wear and to quantify wear in terms of wear rate. The discussion begins...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780028
EISBN: 978-1-62708-281-5
... structure PLASTICS are so prevalent in our lives that it is easy to overlook the vast differences in their properties and how specialized many polymers have become. Consider the differences between aramid bulletproof vests and the polyurethane foam used in pillows. Why can plates made of crystallized...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030001
EISBN: 978-1-62708-349-2
... Abstract This chapter provides a general description of materials and methods for manufacturing high-performance composites. The materials covered are polymer matrices and prepreg materials and the methods include infusion processes, composite-toughening methods, matrix-toughening methods...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290035
EISBN: 978-1-62708-319-5
... jetting. The chapter provides a detailed description of these constituents. The requirements of a binder as well as the factors determining the physical and thermal properties of polymers are discussed. Then, two factors associated with solvation of polymers, namely solubility parameter and wetting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.9781627083492
EISBN: 978-1-62708-349-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200327
EISBN: 978-1-62708-354-6
... austenite. At a sufficiently high temperature, the ferrite and any carbides present are completely decomposed to produce a homogeneous austenitic microstructure. The process of heating for the purpose of forming a homogeneous austenite microstructure is referred to as austenitizing or solution treating...