1-20 of 468 Search Results for

high-temperature coatings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080003
EISBN: 978-1-62708-304-1
... diffusion coating, chromized coating, has also reportedly been used in boilers. Both of these diffusion coatings are very thin. Coatings have been highly successful in providing protection against oxidation and hot corrosion for the high-temperature components, such as airfoils, in gas turbines...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030025
EISBN: 978-1-62708-282-2
... , 1981 • Holmes D.R. and Rahmel A. , Ed., Materials and Coatings to Resist High-Temperature Corrosion , Applied Science , 1978 • Hot Corrosion Problems Associated With Gas Turbines , STP 421, American Society for Testing and Materials , 1967 • Khanna A.S...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230485
EISBN: 978-1-62708-298-3
... . The High Temperature Oxidation of Beryllium, Part IV: In Water Vapor and in Moist Oxygen , J. Nucl. Mater. , Vol 3 , p 190 – 200 10.1016/0022-3115(61)90006-X Beaver W.W. , and Stonehouse A.J. , 1963 . “ Beryllium: Surface Treatment and Coatings ,” Report NP-14783, Brush Beryllium Co...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610415
EISBN: 978-1-62708-303-4
... for coated alloy divided by time in air for uncoated alloy. Source: Ref 11 A frequent problem encountered in alloy design is that it may be desirable to use a new alloy in a high-temperature structure and the alloy is so new that there is not sufficient data to substantiate its long-term...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500317
EISBN: 978-1-62708-317-1
... 2200–3200 Source: Ref 16.7 , 16.55 Due to the high temperature of the process, softening and distortion are the problems to be addressed in stamping dies. Additional heat treating may be required after coating. Due to distortion, tight tolerances may not be achievable with CVD coatings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460253
EISBN: 978-1-62708-285-3
.... Coatings with greater degrees of particle deformation are typically associated with minimal porosity, high amounts of bonded area, and relatively high values of cohesive strength ( Ref 10.9 ). Fig. 10.4 Particle velocity ( V p ) for d 50 = 42 μm powder versus gas temperature ( T g ) at various...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... temperature at the time of application and the type of powder being applied. Alternatively, some coating systems are characterized by the application method used. For example, for coil-coated metal sheet (commonly steel or galvanized steel), very specialized high-speed roller application equipment is used...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
.... This is a high-temperature process; thus, it is not applicable to rollers made from thin-walled tubes, but some PVD coatings were almost as good, as were some thermal spray coatings. Figure 12.6 shows sand abrasion results (performed in the style of ASTM International G174 with silica-coated film) on some...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280001
EISBN: 978-1-62708-267-9
... Abstract This chapter provides a brief introduction to superalloys and their high-temperature capabilities. It explains how and why they were developed and highlights some of their unique properties, behaviors, and characteristics. It discusses their basic metallurgy, how they are processed...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... be tolerated in subsequent operations. (c) Phosphoric acid cleaner-coaters are often sprayed on parts to clean the surface and leave a thin phosphate coating. (d) Phosphoric acid for cleaning and iron phosphating. Proprietary products for high- and low-temperature application are available. (e...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080249
EISBN: 978-1-62708-304-1
..., Battelle Columbus Laboratories , Columbus, OH , 1972 3. Stringer J. , High Temperature Corrosion in Energy Systems , Rothman M.F. , Ed., The Metallurgical Society of AIME , 1985 , p 3 10.1080/02619180.1985.11753292 4. Stringer J. , Coatings in the Electricity Supply...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080235
EISBN: 978-1-62708-304-1
.... , and Pasin M. , High-Temperature Erosion Resistance of Coatings for Gas Turbine , Trans. ASME , Vol 114 , 1992 , p 242 10.1115/1.2906579 26. Wright I.G. , Nagarajan V. , Merz W.E. , and Stringer J. , The Kinetics of High-Temperature Erosion-Corrosion of Oxidation...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080259
EISBN: 978-1-62708-304-1
... Abstract This chapter discusses material-related problems associated with coal-fired burners. It explains how high temperatures affect heat-absorbing surfaces in furnace combustion areas and in the convection pass of superheaters and reheaters. It describes how low-NOx combustion technology...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080335
EISBN: 978-1-62708-304-1
... Perspective of Fireside Corrosion Problems in Refuse-Fired Boilers , Paper No. 200, Corrosion/93 , NACE , 1993 2. Sorell G. , The Role of Chlorine in High Temperature Corrosion in Waste-To-Energy Plants , Mater. High Temp. , Vol 14 ( No. 2/3 ), 1997 , p 137 10.1080/09603409.1997.11689546...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... energies, the bombarding species will be incorporated into the film unless the substrate temperature is high. In reactive ion plating, the plasma provides ions of reactive species, such as nitrogen, oxygen, or carbon, that are accelerated to the surface to form the desired compounds (nitrides, oxides...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080321
EISBN: 978-1-62708-304-1
.... Parker J.C. , Rosborough D.F. , and Virr M.J. , High Temperature Corrosion Trials at Marchwood Power Station—10,000 Hour Corrosion Probe Trials , J. Inst. Fuel , Feb 1972 , p 95 5. McDowell D.W. , Raudebaugh R.J. , and Somers W.E. , High-Temperature Corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080423
EISBN: 978-1-62708-304-1
.... , Proc. Conf. Performance of High Temperature Materials in Fluidized Bed Combustion Systems and Process Industries , Ganesan P. and Bradley R.A. , Ed., ASM International , 1987 , p 161 13. Morrall F.R. , Wire Wire Prod. , Vol 23 , 1948 , p 484 , 571 14. Kelman...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080005
EISBN: 978-1-62708-304-1
... steels carbon steel chromium-molybdenum steel oxidation oxidation resistance superalloys References 1. Lai G.Y. , unpublished data, 2004 2. Birks N. and Meier G.H. , Introduction to High Temperature Oxidation of Metals , Edward Arnold Ltd...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080067
EISBN: 978-1-62708-304-1
... Abstract Oxidation usually dominates high-temperature corrosion reactions, but under certain conditions, some alloys may be affected by nitridation as well. This chapter explains why nitridation occurs and how it attacks various metals, in some cases, penetrating deeper than oxidation...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080201
EISBN: 978-1-62708-304-1
... Abstract Sulfur is one of the most common corrosive contaminants in high-temperature industrial environments and its presence can cause a number of problems, including sulfidation. This chapter describes the sulfidation behavior of a wide range of alloys as observed in three types of industrial...