1-20 of 1692 Search Results for

high temperature applications

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080003
EISBN: 978-1-62708-304-1
... to the specific high-temperature corrosive environment in the end application. This can lead to premature failures. For example, because of their good weldability, high nickel filler metals, such as filler metal alloy 82 (ERNiCr-3), are sometimes used for welding the alloys that are to be in service...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.9781627083041
EISBN: 978-1-62708-304-1
Image
Published: 01 August 2018
Fig. 14.25 (a) Optical and (b) TEM. Steel for high-temperature application containing C = 0.1%, Cr = 9%, W = 2%, quenched and tempered. Martensite laths in packets. Dislocations and subgrains inside the laths. Carbides precipitated mostly at the lath interfaces. Courtesy of F. Abe, National More
Image
Published: 01 January 2022
Fig. 12.129 High- and low-temperature resistance applications More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280323
EISBN: 978-1-62708-267-9
... Abstract This chapter discusses the failure of superalloy components in high-temperature applications where they are subject to the effects of microstructural changes, melting, and corrosion. It explains how overheating can deplete alloying elements and alter the composition and distribution...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240563
EISBN: 978-1-62708-251-8
... Abstract Superalloys are nickel, iron-nickel, and cobalt-base alloys designed for high-temperature applications, generally above 540 deg C. This chapter covers the metallurgy, composition, and properties of cast and wrought superalloys. It provides information on melting, heat treating...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240547
EISBN: 978-1-62708-251-8
... Abstract Nickel and nickel alloys have an excellent combination of corrosion, oxidation, and heat resistance, combined with good mechanical properties. Nickel alloys can be divided into alloys that combine corrosion and heat resistance, superalloys for high-temperature applications, and special...