1-20 of 224 Search Results for

hand grinding

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030043
EISBN: 978-1-62708-349-2
... to difficulties and complications in holding or clamping. This will be dictated by automated mount head openings and the clamping apparatus or by the ability to hold and control the sample by hand. Following the rough grinding step, the sample(s) should be ready for rough polishing. Rough polishing further...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030115
EISBN: 978-1-62708-349-2
... either by using automated grinding/polishing equipment or by hand grinding/polishing. The “first surface” that is polished will become the surface bonded to a glass slide. It is essential that there are no artifacts created in the polished first face, or it will affect the optical light path on the final...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400087
EISBN: 978-1-62708-258-7
... the mounted specimen is grinding, to provide a flat surface. The grinding operation could take place in the preparation area or in its own area, because of the grinding debris and dust that is generated. Grinding can be done by a hand grinding device, by rotating wheels, or by an automatic grinding/polishing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
... deformation (a) Total deformed layer (b) Type Grade Abrasive cutoff wheel Alumina A 60 DE wheel Proprietary oil-water emulsion 4 16 700 Hand hacksaw 18 t.p.i., roll-set blade Nil 100 55 750 Surface grinding Alumina 28A 46 KVBE wheel 0.001-in feed, machine surface grinding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400169
EISBN: 978-1-62708-258-7
... Types of Desiccators Desiccants Other Means of Specimen Storage Cleaning the Specimen Polishing Cloths Polishing Discs Polishing Abrasives Manual (Hand) Polishing Automatic Polishing Microprocessor-Controlled Grinding/Polisher Machines Electrolytic Polishing Polishing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230199
EISBN: 978-1-62708-298-3
... the procedure. Grinding on the two finer discs (240 and 400 grit) is accompanied by the application of kerosene. The technique consists of holding an oil can containing kerosene in one hand and the mounted specimen in the other hand. While the grinding is being done, several drops of kerosene are applied every...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120313
EISBN: 978-1-62708-269-3
..., in. Nominal hole diam, in. ⅛ ¼ ½ 1 1½ 2 ⅛ ¼ ½ 1 1½ 2 Grade 1, annealed 110–170 100 0.003 0.006 0.009 0.012 0.015 0.020 M-1 or M-2 Right hand, Helix: 10°, CA: 45 °, Per. relief: 10° 375 0.003 0.006 0.009 0.012 0.015 0.020 C-2 RR: 6°, Helix: 7°, Per. relief: 10°, CA: 45...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030023
EISBN: 978-1-62708-349-2
... for mounting composite materials is provided. The steps recommended to achieve a good mounted specimen without voids or specimen pull-out are also described. The chapter discusses the processes for clamping mounted composite samples in automated polishing heads and mounting composite materials for hand...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770199
EISBN: 978-1-62708-337-9
... material (the grit) is aluminum oxide. During the many years that aluminum oxide grinding wheels have been utilized, their benefits and shortcomings have become fairly well understood. When the grinding technique is good, the product is good. On the other hand, deviations from good practice can lead...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720161
EISBN: 978-1-62708-305-8
... that form between specimen and resin are a major contributor to edge rounding. Second, use of semiautomatic and automatic grinding/polishing equipment increases surface flatness and edge retention opposed to manual (hand) preparation. Third, the use of harder, woven or nonwoven, napless surfaces...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220069
EISBN: 978-1-62708-259-4
... to examine the sample is made, careful washing and drying (sample and hands!) should be performed. This should be a rule even if only a brief look at the sample surface is desired to check for the progress of the grinding and polishing operation. The usual practice is to wash under clean water, gently...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030067
EISBN: 978-1-62708-349-2
... of the artifacts, if so desired ( Fig. 4.5 ). This can be performed with automated polishing equipment or by hand, following the procedures described in Chapter 3, “Rough Grinding and Polishing.” Fig. 4.5 Polished boron fiber composite cross section. Bright-field illumination, 10× objective...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320033
EISBN: 978-1-62708-347-8
... Recarburizing Cold Treatment Selection of Materials for Carburized Gears Carbon Content and Case Property Core Hardness of Gear Teeth Microstructure of Carburized Cases Some Carburizing Problems Heat Treat Distortion of Carburized and Hardened Gears Grinding Stock Allowance on Tooth...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250089
EISBN: 978-1-62708-345-4
... a comparison of steels for gear cutting. The operating principles of computer numerical control and hobbing machines are also covered. This is followed by sections that discuss the processes involved in grinding, honing, and lapping of gears. Finally, the chapter provides information on the superfinishing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480293
EISBN: 978-1-62708-318-8
... ... ... Milling ... X X X ... ... ... X Drilling ... ... ... X ... ... X X Tapping ... X ... X ... ... X X Grinding X X ... ... X X ... X Belt grinding X ... ... ... X ... ... X Cut-off X ... ... ... ... ... ... ... Sawing ... ... ... X...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250163
EISBN: 978-1-62708-345-4
... associated with carburizing are then covered, followed by the processes involved in heat treat distortion and shot peening of carburized and hardened gears. Information on grinding stock allowance on tooth flanks to compensate for distortion is also provided. The chapter further discusses the applications...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320133
EISBN: 978-1-62708-347-8
... material to the other. It is also found that the process used during nitriding has a significant effect on the thickness of this white layer. For example, single-stage gas nitriding may result in a white layer of 0.025 to 0.076 mm (0.001–0.003 in.) on materials normally used for gears. On the other hand...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630169
EISBN: 978-1-62708-270-9
...Abstract Abstract This chapter is a detailed account of the general characteristics and effects of and the methods for preventing or reducing different categories of wear failures, namely abrasive (erosive, grinding, and gouging), adhesive, and fretting wear. abrasive wear adhesive wear...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230065
EISBN: 978-1-62708-298-3
... deposits, and the use of chemical activators and conditioning agents. It also explains that hand sorting is still very common because of processing challenges and inefficiencies. bertrandite beryl beryllium ores crushing flotation phenacite BERYLLIUM-CONTAINING ores are treated...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090349
EISBN: 978-1-62708-266-2