1-20 of 585

Search Results for growth curves

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140175
EISBN: 978-1-62708-335-5
... Abstract This data set contains approximately 50 growth curves for a wide range of aluminum casting alloys at various temperatures. Growth curves are used to determine the dimensional changes that must be anticipated during service in applications where close dimensional tolerances are required...
Image
Published: 01 December 2004
Fig. D2.1 Growth curves for aluminum alloy 238.0-F, permanent mold. Test specimen: 1.125 diam × 12 in. rod More
Image
Published: 01 December 2004
Fig. D2.5 Growth curves for aluminum alloy 295.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.6 Growth curves for aluminum alloy B295.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 950 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.9 Growth curves for aluminum alloy 319.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.14 Growth curves for aluminum alloy 336.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 950 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.16 Growth curves for aluminum alloy 355.0-F, permanent mold. Specimen: 1.125 diam × 12 in. rod More
Image
Published: 01 December 2004
Fig. D2.17 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 940 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.18 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.20 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 1000 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.21 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 940 °F, cold water quench More
Image
Published: 01 December 2004
Fig. D2.22 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, cold water quench More
Image
Published: 01 December 2004
Fig. D2.23 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 1000 °F, cold water quench More
Image
Published: 01 December 2004
Fig. D2.24 Growth curves for aluminum alloy 355.0-T51, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 8 h at 440 °F More
Image
Published: 01 December 2004
Fig. D2.25 Growth curves for aluminum alloy 355.0-T7, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 5 h at 700 °F plus 12 h at 850 °F, boiling water quench, 8 h at 440 °F More
Image
Published: 01 December 2004
Fig. D2.30 Growth curves for aluminum alloy 360.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.31 Growth curves for aluminum alloy 380.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.32 Growth curves for aluminum alloy 384.0-F, die cast. Specimen: 5 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.33 Growth curves for aluminum alloy 413.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.35 Growth curves for aluminum alloy 443.0-F, die cast. Specimen: 3 16 in. thick plate More