1-13 of 13 Search Results for

gloss

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780177
EISBN: 978-1-62708-281-5
... Abstract This article is a brief account of various factors pertinent to the characterization of materials and analysis of optical components, namely transmission, haze, yellowness, refractive index, surface irregularity, birefringence, internal contamination, surface gloss, and color...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310213
EISBN: 978-1-62708-286-0
... abrasive. Finishes No. 3 and 4 are directional, with grit lines typically 1 cm (0.4 in.) in length. Finish No. 3 has a surface roughness average (R a ) of 0.4 to 0.8 µm (15 to 30 µin.). Specular gloss at 85° is typically 40 to 60 (per ASTM D 523, “Standard Test Method for Specular Gloss”). The standards...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... are minimized or avoided Testing for adhesion, color, gloss, and other parameters that may affect the appearance or protective capability of the coating Coating inspection requires training, expertise, and familiarity with various instruments. Inspector training courses are available, and verification...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
..., or to increase resistance to ultraviolet or weathering conditions. Typical pigments include zinc phosphate, zinc molybdate, zinc phosphorus silicate, zinc chromate, and strontium chromate. Miscellaneous compounds added include dryers, flow-control and gloss-control agents, and suspension agents. Although...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780153
EISBN: 978-1-62708-281-5
... to elevated temperature can result in loss of mechanical properties (embrittlement, loss of impact strength, flexibility, and elongation) and loss of electrical properties. Discoloration, cracking, chalking, loss of gloss, and flaking can occur. Cyclic exposure can result in mechanical fatigue failure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.9781627082501
EISBN: 978-1-62708-250-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780259
EISBN: 978-1-62708-281-5
... the loss of gloss caused by impacting carborundum grit ( Ref 9 ). A flat sample is held at 45° and struck with increasing amounts of No. 80 silicon carbide dropped from a height of 635 mm. The relatively mild airborne abrasive action is similar to that encountered by many items in actual use...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... polyurethane top coats are also available as are low volatile-organic compound (VOC) high-performance primers (e.g., epoxy polyamide). The final coating often is tailored to the application. Examples are high gloss on auto bodies and self-cleaning paint on residential siding. Optimum procedures for both...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260149
EISBN: 978-1-62708-336-2
... are sometimes exaggerated by a thin layer of gloss paint. Etching and anodizing can usually remove pick-up particles but cannot always remove all surface defects produced at the press, depending on how much metal is removed in the etch tank. Parson et al. ( Ref 18 ) described the characteristics...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870449
EISBN: 978-1-62708-314-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064