1-20 of 73 Search Results for

general structural alloy 6061

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870063
EISBN: 978-1-62708-299-0
... in 2 xxx alloys is controlled by fabrication practices that can affect the amount, size, and distribution of second-phase intermetallic precipitates. Resistance to IGC corrosion is obtained by use of heat treatments that cause precipitation to be more general throughout the grain structure (e.g., 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870135
EISBN: 978-1-62708-299-0
... and Food Industries , Chemical Publishing Co. , 1964 • Mondolfo L.F. , Aluminum AlloysStructure and Properties , Butterworth & Co. , 1976 (reprinted in 1979 ) 10.1016/B978-0-408-70932-3.50008-5 • Rabald E. , Corrosion Guide , Elsevier Publishing Co. , 1968 10.1016...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
... (9.8 mils/year). Corrosion rates for silicon carbide/aluminum MMCs in seawater are also generally higher than is typical for unreinforced aluminum alloys. This is documented in Ref 11 for discontinuous SiC in 6061 and 5000 series aluminum matrices and in Ref 13 , which reports that silicon...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260149
EISBN: 978-1-62708-336-2
... applications throughout the world. Some 6000-series alloys have a higher level of alloying elements to achieve higher strength for structural and semistructural applications. In general, 6061 (Al-Mg-Si-Cu) and 6082 (Al-Si-Mg-Mn) are the most common alloys offering higher mechanical properties for structural...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460277
EISBN: 978-1-62708-285-3
... and refurbishment of structural engineering components are also discussed. high-pressure cold spray process repair refurbishment aerospace industry oil and gas industry power-generation industry COLD SPRAY COATING TECHNOLOGY, as described in previous chapters, has the capability to provide surface...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460227
EISBN: 978-1-62708-285-3
... and magnesium alloys ( Ref 9.4 – 9.6 ). Several examples of cold spray repairs are presented in this chapter, some of which are also described in the “Aerospace Industry” section of Chapter 11, “Cold Spray Applications in Repair and Refurbishment for the Aerospace, Oil and Gas, and Power-Generation Industries...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870085
EISBN: 978-1-62708-299-0
... of 800× showed the structure to be essentially the same on each specimen and to contain a fairly dense distribution of a very fine precipitate of magnesium silicide (Mg 2 Si) throughout the material. This constituent would be visible only if aluminum alloy 6061 had been heated to temperatures above about...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870161
EISBN: 978-1-62708-299-0
..., as demonstrated by the corrosion of the HAZ of an as-welded structure of alloy 7005 shown in Fig. 2 . In general, the welding procedure that puts the least amount of heat into the metal has the least influence on microstructure and the least chance of reducing the corrosion behavior of aluminum weldments...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870025
EISBN: 978-1-62708-299-0
...Abstract Abstract Aluminum generally has excellent resistance to corrosion and gives years of maintenance-free service in natural atmospheres, fresh waters, seawater, many soils and chemicals, and most foods. This chapter explains why aluminum and aluminum alloys are naturally resistant...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
... reinforced with 10 vol% of alumina particles; 6061/SiC/47f is the alloy 6061 reinforced with 47 vol% of continuous SiC fibers; and A356/C/05c is the casting alloy A356 reinforced with 5 vol% of chopped graphite fibers. 33.1.1 Discontinuously Reinforced Aluminum Composites 33.1.2 Processing DRA...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820143
EISBN: 978-1-62708-339-3
... are not recommended. Source: Aluminum Company of America Relative rating of selected aluminum filler alloys used to fillet weld or butt weld two component base alloys, where one of the base alloys is 6061 or 6070 Table 3(d) Relative rating of selected aluminum filler alloys used to fillet weld or butt weld...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550457
EISBN: 978-1-62708-307-2
...% of silicon carbide whiskers; 7075/Al 2 O 3 /10p is the AA-registered alloy 7075 reinforced with 10 vol% of alumina particles; 6061/SiC/47f is the AA-registered alloy 6061 reinforced with 47 vol% of continuous SiC fibers; and A356/C/05c is an AA-registered casting alloy with 5 vol% of chopped graphite fibers...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
... machine products, automotive parts, cylinders and pistons, fasteners, machine parts, ordnance, recreation equipment, screws and rivets 2219 Structural uses at high temperature (to 315 °C, or 600 °F). High-strength weldments 3003 Most popular general-purpose alloy. Stronger than 1100 with same good...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
... and nameplates 6061 Good formability, weldability, corrosion resistance, and strength in the T-tempers. Good general-purpose alloy used for a broad range of structural applications and welded assemblies including truck components, railroad cars, pipelines, marine applications, furniture, agricultural...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... effect. Alloy 7072, Al-lZn, has a more anodic potential than pure aluminum and is used as the cladding for Alclad 3003, 5052, 6061, and 7075, as well as others. The most widely used alclad products are sheet and plate, although wire, tube, and other forms are also produced. The most generally...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350043
EISBN: 978-1-62708-315-7
... (a) Friction coefficient Source Fixed specimen Moving specimen Static Kinetic Ag Ag IS 0.50 … 1 Au IS 0.53 … 1 Cu IS 0.48 … 1 Fe IS 0.49 … 1 Al Al IS 0.57 … 1 Ti IS 0.54 … 1 Al, alloy 6061-T6 Al, alloy 6061-T6 FOF 0.42 0.34 2 Cu FOF 0.28 0.23...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... alloy 2124 reinforced with 25 volume percent of silicon carbide whiskers; 7075/Al 2 O 3 /10p is the alloy 7075 reinforced with 10 volume percent of alumina particles; 6061/SiC/47f is the alloy 6061 reinforced with 47 volume percent of continuous SiC fibers; and A356/C/05c is the casting alloy A356...
Series: ASM Technical Books
Publisher: ASM International
Published: 15 June 2021
DOI: 10.31399/asm.tb.mpktmse.t56010001
EISBN: 978-1-62708-384-3
... & Steel Technology , Pittsburg, PA , 2011 6. Abbaschian R. , Reed-Hill R.E. , Physical Metallurgy Principles , 4th ed. , CL Engineering , Stamford, CT , 2008 7. Brooks C.R. , Heat Treatment, Structure, and Properties of Nonferrous Alloys , ASM International...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140069
EISBN: 978-1-62708-335-5
... , 4 , 6 , 8 , 9 Typical physical properties of aluminum permanent mold castings Table 8.2(b) Typical physical properties of aluminum permanent mold castings Metric unit values generally derived from engineering/English unit values Alloy Temper Density Specific gravity Average...
Series: ASM Technical Books
Publisher: ASM International
Published: 15 June 2021
DOI: 10.31399/asm.tb.mpktmse.9781627083843
EISBN: 978-1-62708-384-3