Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300227
EISBN: 978-1-62708-323-2
... steel bar in a lathe, and puts an aluminum rod in the tool post, and rubs the rod on the steel, the steel will be mechanically coated with a layer of aluminum. Adhesive transfer is operative; aluminum alloys similarly can gall. The galling resistance may be different for the different alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300163
EISBN: 978-1-62708-323-2
... utility in tribosystems operating in freshwater or saltwater. Aluminum bronzes are thought to be galling resistant. Compatibility testing may be necessary to identify suitable counterfaces for unlubricated sliding of copper alloys. High copper alloys can be very difficult to machine (including...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350043
EISBN: 978-1-62708-315-7
... measurements G 133 Test Method for Linearly Reciprocating Ball-on-Flat Sliding Wear Ball: wear scar diameter, flat: profile G 137 Test Method for Ranking Resistance of Plastic Materials to Sliding Wear Using a Block-on-Ring Configuration Mass loss Surface damage, galling G 98 Test Method...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300421
EISBN: 978-1-62708-323-2
... is an issue, aluminum bronzes such as ASTM International B148 alloy C95300 (86 Cu, 1 Fe, 10 Al) have shown galling resistance against hard steels and other materials. Occasionally, it may be necessary to rub metal surfaces together without a lubricant. High-lead bronzes such as ASTM International B584...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500317
EISBN: 978-1-62708-317-1
... galling wear physical vapor deposition plating sheet metal forming thermal diffusion coating tool wear wear resistance A STAMPING TOOL must be replaced or repaired periodically, when it fails to produce parts within the specified tolerance and/or required surface quality. This is mainly caused...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900201
EISBN: 978-1-62708-350-8
..., and tensile strength. In addition, the process will further improve wear resistance, galling resistance, and corrosion resistance. Another advantage of both ferritic nitrocarburizing and nitriding is that they are low-temperature processes. This means that distortion will be kept to an absolute minimum...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300199
EISBN: 978-1-62708-323-2
... on them, and forging dies have hot steel rubbing on them. The H steels do not get very hard at 43 to 53 HRC. So, to prevent galling and adhesive wear, ejector pins and cores are often nitrided. Thus, a 53 HRC mold with 60 HRC core pins (nitrided H13) reasonably resists adhesive wear. Forging dies...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300079
EISBN: 978-1-62708-323-2
... droplet Fig. 4.5 Typical effect of solid content on slurry erosion Fig. 4.6 The mechanism of slurry erosion Fig. 4.25 Schematic of galling Fig. 4.26 Schematic of fretting corrosion; fretting wear starts the same but reaction product does not form Fig. 4.27...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500107
EISBN: 978-1-62708-317-1
...—Properties—Application , Int. J. Plast. , Vol 16 , 2000 , p 1391 – 1409 10.1016/S0749-6419(00)00015-2 6.15 Mori K. , Maki S. , and Tanaka Y. , Warm and Hot Stamping of Ultra High Tensile Strength Steel Sheets Using Resistance Heating , CIRP Ann. , Vol 54 ( No. 1 ), 2005 , p...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300121
EISBN: 978-1-62708-323-2
... wear on the shaft when rotating with no lubricant Fig. 5.23 Schematic of the use of the ASTM G98 galling test to determine threshold galling stress. Force is sequentially increased until galling occurs Fig. 5.1 Test specimens for ring versus cylinder wear testing Fig. 5.2...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300047
EISBN: 978-1-62708-323-2
... on both plus light oil 0.1 Cd plating on both plus MoS2 0.08 Austenitic stainless steel bolt and nut No lubrication 0.3 Ag plating on both 0.25 Ag plating on both plus light oil 0.1 COF, coefficient of friction Rolling resistance of a golf ball on various rolling surfaces...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120085
EISBN: 978-1-62708-269-3
... of scuffing can be reduced by nitrogen implantation on titanium components. Titanium in hydraulic systems is often used because of the corrosion-resistant nature of the metal and its alloys, but ion implantation has been used to reduce galling against both steel and other titanium alloy counterface materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... resistance and thus increase the corrosion component of the erosion. For example, nitriding stainless steel plug valves solved a galling problem, but the treated surfaces were corroded by the process fluid; they were not corroded by the process fluid without the nitriding. Modifying a material to improve...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300391
EISBN: 978-1-62708-323-2
... are sometimes added for galling resistance (thread lubricant). Greases are typically made in batch processes in a heated/cooled jacketed reactor vessel. The basis of most greases is a soap. Soaps are reaction products of combining a base with organic material. The classic chemistry experiment on making...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000185
EISBN: 978-1-62708-312-6
... sensor bosses must be weldable, machinable for thread tapping, and resistant to galling after exposure to temperatures as high as 1000 °C (1832 °F). Galling is a major concern in this application, because damages caused to a sensor boss during sensor replacement can lead to replacement of a major portion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740163
EISBN: 978-1-62708-308-9
... with tool steel, aluminum bronze, or other wear-resistant hardfacing alloys. Because of its resistance to galling, it is less desirable for forming carbon and stainless steels than for aluminum and copper alloys. Cast steel is also useful for restrike, flanging, and other types of dies that are less likely...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300363
EISBN: 978-1-62708-323-2
... is to use formed plastics to replace the screws and wire tribosystems. Where stainless steel threaded connections are used, the potential for galling exists. Adhesive wear can be a problem for dentists. The tools that are used to scrape and probe teeth must be corrosion resistant and have reasonable...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610585
EISBN: 978-1-62708-303-4
... and case depth to the minimum acceptable design level or by copper plating the outer diameter of the gear blank prior to hobbing. Nitrided cases are very brittle. Consequently, cracking may occur in service prior to realizing any improved wear and galling resistance. This can be avoided by a proper...