1-20 of 757 Search Results for

fracture properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 August 1999
Fig. 19 (a) Effects of artificial aging on the mechanical and fracture properties of alloy 2024. (b) Effects of artificial aging on the corrosion and stress-corrosion properties of alloy 2024 in NaCl solution More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410405
EISBN: 978-1-62708-265-5
... in low-carbon steels. It also discusses the effect of tempering temperature on the mechanical behavior and deformation properties of medium-carbon steels. deformation fracture microstructure tempering CHAPTER 16, “Hardness and Hardenability,” and Chapter 17, “Tempering of Steel...
Image
Published: 01 August 2005
Fig. 4.42 Fracture toughness properties of 7075-T6 aluminum sheet and plate. Source: Ref 4.10 , 4.48 More
Image
Published: 01 August 2005
Fig. 4.43 Fracture toughness properties of Ti-6Al-4V and 7075-T76 aluminum sheet and plate. Source: Ref 4.50 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610209
EISBN: 978-1-62708-303-4
... Abstract This chapter provides information and data on the fatigue and fracture properties of steel, aluminum, and titanium alloys. It explains how microstructure, grain size, inclusions, and other factors affect the fracture toughness and fatigue life of these materials and the extent to which...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540423
EISBN: 978-1-62708-309-6
... Abstract This appendix provides tensile property and fracture toughness data for various low-alloy and stainless steels. fracture toughness low-alloy steel stainless steel tensile properties LIMITED MECHANICAL PROPERTIES DATA for selected low-alloy steels and stainless steels...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630257
EISBN: 978-1-62708-270-9
... be prevented by specifying proper design and appropriate material properties, along with careful attention to manufacturing and quality control procedures and with other factors. However, a fracture mechanics approach can often be used to determine the key factors leading to the failure. Fracture mechanics can...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860269
EISBN: 978-1-62708-348-5
..., K. K is a function of crack size, applied stress, and structural geometry and can be computed using stress analysis methods. The resistance to fracture is a material property defined as the fracture toughness, K c ; fracture occurs when K = K c . Thus, for a given structural geometry...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540411
EISBN: 978-1-62708-309-6
... Abstract This appendix provides tensile property data for titanium alloys and castings and plane-strain fracture toughness data for Ti-6Al-4V castings. alpha-beta titanium alloys beta titanium alloys titanium castings plane-strain fracture toughness tensile properties LIMITED...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200083
EISBN: 978-1-62708-354-6
... the constant ε f ′ to other material properties. A convenient approximation is to set ε f ′ equal to true fracture strain in a tensile test. In terms of percent reduction in area, %RA, ε f ′ is on the order of (Eq 6-20) ε f ′ ≈ ln  100...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030177
EISBN: 978-1-62708-349-2
... D.C. , 1976 , p 326 10.1021/ba-1976-0154.ch027 7. Ting R.Y. and Moulton R.J. , Fracture Properties of Elastomer Toughened Epoxies , 12th National SAMPE Technical Conference , 1980 , p 265 8. Klug J.H. and Seferis J.C. , Phase Separation Influence...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030193
EISBN: 978-1-62708-349-2
... of the Toughening Mechanisms in Rubber-Modified Epoxy Polymers, Part II: A Quantitative Description of the Microstructure-Fracture Property Relationships , J. Mater. Sci. , Vol 27 , 1992 , p 2763 – 2769 10.1007/BF00540703 15. Kinloch A.J. et al. , Deformation and Fracture Behavior of a Rubber...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630013
EISBN: 978-1-62708-270-9
... mechanical properties plastic deformation WHILE A DETAILED STUDY of mechanical properties of metals is beyond the scope of this work, there are certain facts that must be understood if the task of failure analysis is to be successfully undertaken. Because both fracture and wear are closely related...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630001
EISBN: 978-1-62708-270-9
... the upper eyelets. Therefore, the metal eyelets tend to wear, or abrade, the fibers of the lace. Since the shoelace presumably has uniform mechanical properties along its length, it will eventually wear—and ultimately tear, or fracture—at the location where conditions are most severe...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860371
EISBN: 978-1-62708-348-5
... increases and ductility decreases with decreasing temperature, fracture resistance must be considered when selecting these alloys for service at temperatures below 77 K. Tensile properties of nitrogen-strengthened Cr–Ni–Mn stainless steels. Table 11.5 Tensile properties of nitrogen-strengthened Cr–Ni...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230209
EISBN: 978-1-62708-298-3
... Abstract This chapter describes the effect of processing variables on the mechanical properties of beryllium, including tensile and yield strength, fracture toughness, creep and fatigue strength, ductile-to-brittle transition, and notch sensitivity. It also discusses the effects of chemical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480113
EISBN: 978-1-62708-318-8
... of properties is available to designers and engineers. However, this chapter emphasizes the more basic properties of terminal alloys: hardness; tensile strength; ductility; creep, stress-rupture, and fatigue strengths; toughness; and fatigue crack growth rate (FCGR). The fracture mechanics approach to lifing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780185
EISBN: 978-1-62708-281-5
... Plane-strain fracture toughness and strain energy release rate of plastic materials D 5083 3268 Tensile properties of reinforced thermosetting plastics using straight-sided specimens D 5279 6721 Measuring the dynamic mechanical properties of plastics in torsion Source: Ref 2 Tensile...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540397
EISBN: 978-1-62708-309-6
... Abstract This appendix provides fracture toughness and tensile property data for aluminum alloys in the 2000, 6000, 7000, and 8000 series as well as B201 and D357 aluminum castings and powder metal alloys. aluminum alloys aluminum castings fracture toughness tensile properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540431
EISBN: 978-1-62708-309-6
...- the appearance of propagating fractures in sitive properties of materials. plain-carbon or low-alloy pipe steels over the crystalline fracture. A pattern of brightly re- temperature range where the fracture mode ecting crystal facets on the fracture surface changes from brittle to ductile. See Chapter 4...