1-20 of 31 Search Results for

flammability

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780159
EISBN: 978-1-62708-281-5
...Abstract Abstract This article describes the basic approaches to improving the fire resistance of a polymeric material, considers the burning process on a microscale and macroscale, and discusses various test methods for determining the flammability characteristics of polymeric materials. Test...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870401
EISBN: 978-1-62708-314-0
... and the potential damage it can cause. It discusses the problems associated with moisture absorption and exposure to solvents, fuels, ultraviolet radiation, lightning strikes, thermal oxidation, and extreme temperatures. It also discusses the factors that influence flammability. References References 1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400087
EISBN: 978-1-62708-258-7
... electrolytic procedures. A hot-air blow dryer is nearby to dry the specimens just after etching and rinsing in alcohol. Acid storage and flammable-material storage cabinets are installed near the hood and sink area. These cabinets should be ventilated to the outside of the laboratory. Premixed etchants can...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780115
EISBN: 978-1-62708-281-5
... temperature at 1.82 MPa (0.264 ksi), °C (°F) 150 (298) 130 (266) 130–135 (266–275) Flammability rating … … 94V-0 Burning rate Self-extinguishing Self-extinguishing Self-extinguishing Specific heat, kJ/kg · K (Btu/lb · °F) (e) … … 1.68 (0.40) Coefficient of thermal expansion, 10–6/K...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780055
EISBN: 978-1-62708-281-5
... of part performance requirements. Some, such as flammability, transparency, ultraviolet stability, electrical, moisture, and chemical compatibility, as well as agency approvals, are specified as absolute values or simplified choices. However, mechanical requirements such as stiffness, strength, impact...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290243
EISBN: 978-1-62708-306-5
...-temperature strength Slower cure than with anaerobics or cyanoacrylates Toxic Flammable Odor Limited open time Dispensing equipment required Cyanoacrylate Rapid room-temperature cure One component High tensile strengths Long pot life Good adhesion to metal Dispenses...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550325
EISBN: 978-1-62708-307-2
..., or nonflammable properties. Although some plastics can be formulated to retard flames, their organic nature makes them inherently flammable. Applications under constant stress for which a close tolerance must be held need to be scrutinized in terms of the effects of creep at the application temperature...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780343
EISBN: 978-1-62708-281-5
.... Chiu J. , Applications of Thermogravimetry to the Study of High Polymers , Appl. Polym. Symp. , ( No. 2 ), 1966 , p 25 ; also, Reprint RL-22, E.I. Du Pont de Nemours & Company, Inc . 31. Price D. , Horrocks A. , and Tunc M. , Textile Flammability , Chem. Brit. , Vol...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720183
EISBN: 978-1-62708-305-8
... and eliminates bath flammability. Water suspendible particle concentrates include the necessary wetting agents, dispersing agents, rust inhibitors, and antifoam agents. All ferromagnetic materials retain a residual magnetic field to some degree after being magnetized. This field is negligible in magnetically...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230441
EISBN: 978-1-62708-298-3
...; performance reliability; biological inertness; flammability; special requirements, such as electrical and thermal needs; and/or cost. In this book, reference to specific adhesives is usually made only with regard to the preparation, evaluation, and/or application of adhesives. Adhesives specific for beryllium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780003
EISBN: 978-1-62708-281-5
... (480 °F). Polyketone resins are useful in a broad spectrum of applications that require their unique combination of properties. For example, low flammability, low smoke generation, chemical resistance, high-temperature resistance, and strength make PAEK materials suitable for aircraft/aerospace...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290139
EISBN: 978-1-62708-319-5
Book Chapter

By Eren Billur
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400181
EISBN: 978-1-62708-316-4
...: higher is better) ∘ … • κ ≈ 2.4 GPa    ≈ 348 ksi κ ≈ 1.0 … 1.6 GPa    ≈ 145 … 232 ksi κ ≈2.5 … 3.5 GPa    ≈ 363 … 508 ksi No flammability • … … No environmental impact • … … Usage in hydraulic applications, % ~0 85 10 Legend: •, best; ∘, in-between; …, N/A or worst. Source...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780146
EISBN: 978-1-62708-281-5
... the solubility parameter requirements. When added to an intractable polymer such as PVC, a plasticizer such as dioctyl phthalate (DOP) increases light stability, flammability, and susceptibility to attack by fungi and corrosives. Thus, in spite of moderately good resistance to attack by an oxidizing acid...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.t51180001
EISBN: 978-1-62708-256-3
... tank caused ignition of the flammable fuel/air mixture in the tank. However, eight years after the crash, independent investigations are still ongoing that dispute this conclusion. Some of these investigators contend that a shoulder-fired missile hit the plane and that the government has turned a blind...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300391
EISBN: 978-1-62708-323-2
... Relating to flammability Pour point Ability to stay liquid when cold Ash Residue left after combusting oil Acid number The acidity of an oil Base number The alkalinity of an oil Gravity A viscosity component related to solvency Color Clear to dark Volatility Ease of evaporation...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310163
EISBN: 978-1-62708-326-3
... quenches is that they are not flammable. A disadvantage of synthetic quenches is that the ingredients that are added to water tend to cling to the work, thus reducing their concentration over time. Therefore, it is mandatory that a synthetic quenching bath be analyzed frequently and replenished as required...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.t51180061
EISBN: 978-1-62708-256-3
..., an aircraft crash, and the associated failure investigation, is of very high importance. The 1996 loss of TWA Flight 800, carrying 230 people from New York to Paris, was concluded to have been caused by a stray wire in the center wing fuel tank that ignited the flammable fuel/air mixture. The official failure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050025
EISBN: 978-1-62708-311-9