Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040010
EISBN: 978-1-62708-428-4
... Abstract This article provides a brief description of commercially important thermal spray processes and gives examples of applications and application requirements. The processes covered are flame, wire arc, plasma, high-velocity oxyfuel processes, detonation gun, and cold spray methods...
Image
Published: 01 March 2001
Fig. 2 Relative costs (based on pounds of alloy deposited) for various weld overlay and thermal spray processes. SAW, submerged arc welding; FCAW, flux-cored arc welding; GMAW, gas metal arc welding; SMAW, shielded metal arc welding; OAW, oxyacetylene gas welding; FLSP, flame spraying; PSP More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... characteristics of flame, arc wire, high-velocity oxyfuel, detonation gun, air plasma, and vacuum plasma thermal spray processes Table 19 Compares the abrasive wear resistance of tungsten carbide coatings applied by detonation gun, plasma, and high-velocity oxyfuel thermal spray processes Table 22...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240395
EISBN: 978-1-62708-251-8
... by the presence of hard chromium carbide particles. Some alloy compositions have tungsten carbide additions to further improve wear resistance. Hardfacing materials are applied by either welding or thermal spraying. Weld overlay is a form of hardfacing that is applied by oxyacetylene or an arc welding process...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
..., or diffusion. anodizing. Forming a conversion coating on a metal surface by anodic ox- idation; most frequently applied to aluminum. arc spraying (ASP). A thermal spraying process using an arc between two consumable electrodes of surfacing materials as a heat source and a compressed gas to atomize and propel...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780153
EISBN: 978-1-62708-281-5
... outdoor aging factors, such as the presence of moisture. Weatherometers Weatherometers include open-flame carbon arc and twin enclosed carbon arc types. Sunshine Open-Flame Carbon Arc The sunshine open-flame carbon arc weatherometer is a lamp that operates in free-flowing air. It can be used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.9781627084284
EISBN: 978-1-62708-428-4
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
...) Attribute Hand wiping Immersion Emulsion Batch spray Continuous conveyor Ultrasonic Handling 2 7 7 5 9 7 Cleanness 4 3 5 7 7 10 Process control 3 6 6 8 9 9 Capital cost 7 8 7 5 4 1 Operating cost 5 8 8 7 6 6 Source: Ref 1 Substrate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... on ceramic and cermet (ceramic-metal) coatings applied by vapor deposition processes or thermal spraying can be found later in this chapter. Glass Linings Glass, particularly low-expansion borosilicate glass (e.g., Pyrex), finds numerous application as a material of construction in the chemical, food...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040001
EISBN: 978-1-62708-428-4
.... This fundamental understanding is critical for spray parameter optimization of process and material. For example, metal oxide ceramics with high melting points and low thermal conductivity typically require high enthalpy and particle temperatures with slow flame velocities for optimum performance and application...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... a coating (fusion) and those that do not melt the substrate (thermal spray). Thermal spray coatings are normally applied to steels, and the ones that are applied by the more energetic processes such as high-velocity oxyfuel (HVOF) or plasma arc spraying (PAS) are finished to usually less than 0.25 mm...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200369
EISBN: 978-1-62708-354-6
... are submerged arc, gas metal arc, gas tungsten arc, plasma arc, plasma powder spray, thermal spray, oxy-fuel metallizing, electron beam, resistance brazing, induction brazing, and laser welding. When using an arc welding process or any process which results in a homogeneous structure, a multipass weld procedure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... and the effect of temperature, pressure, and other process variables on the microstructures and properties developed. beryllium chemical vapor deposition electroplating ion plating microstructure physical vapor deposition plasma arc spraying sputtering thermal evaporation THIS CHAPTER deals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
... discontinuous silicon carbide/aluminum MMCs ( Ref 11 ). Aluminum flame- and arc-sprayed coatings exhibit excellent corrosion resistance for a minimum of 33 months. Zinc arc-sprayed coatings are less corrosion resistant than aluminum thermal-sprayed coatings. Zinc coatings protect the silicon carbide/aluminum...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060429
EISBN: 978-1-62708-261-7
... by a flame. fracture mechanics (LEFM). (2) A quantita- flame hardening. A process for hardening the tive analysis for evaluating structural behav- surfaces of hardenable ferrous alloys in which ior in terms of applied stress, crack length, an intense flame is used to heat the surface and specimen or machine...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040030
EISBN: 978-1-62708-428-4
... Abstract This article presents best practices for the metallographic preparation of specimens produced via thermal spray coating methods. It outlines typical metallographic preparation process flow, highlighting important considerations for obtaining a clear and representative specimen suitable...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.9781627082617
EISBN: 978-1-62708-261-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480161
EISBN: 978-1-62708-318-8
... Abstract Casting is the most economical processing route for producing titanium parts, and unlike most metals, the properties of cast titanium are on par with those of wrought. This chapter covers titanium melting and casting practices -- including vacuum arc remelting, consumable electrode arc...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480265
EISBN: 978-1-62708-318-8
.... It describes several welding processes, including arc welding, resistance welding, and friction stir welding, and addresses related issues such as welding defects, quality control, and stress relieving. The chapter also covers mechanical fastening techniques along with adhesive bonding and brazing...