1-20 of 698 Search Results for

fatigue curve

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140253
EISBN: 978-1-62708-335-5
... Abstract This data set contains the results of rotating-beam reversed-bending fatigue tests for a wide range of aluminum casting alloys. These fatigue curves are the results of tests on individual lots of material considered representative of the respective alloys and tempers. aluminum...
Image
Published: 01 November 2012
Fig. 14 Schematic showing the fatigue curve with the distribution of lives at three different stress levels. Note that the distribution widens as the stress level decreases. Source: Ref 10 More
Image
Published: 01 July 2009
Fig. 10.15 Fatigue curve for directionally solidified Mar-M 246 More
Image
Published: 01 March 2006
Fig. 11.69 Rotating-beam fatigue curve for aluminum 7075-T6 rod, 1.9 cm (3/4 in.) diam rolled and drawn with various amounts of prestress. Source: Ref 11.76 More
Image
Published: 01 December 1999
Fig. 5.21 Hardness, retained austenite, microcrack density, and bending fatigue curves for carburized and hardened SAE 8620 steel quenched by three methods: direct quench, ASTM 1-3 grain size; single reheat, ASTM 4-5 grain size; double reheat. Source: Ref 43 More
Image
Published: 01 December 2004
Fig. D6.1 213.0-F, permanent mold aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from two lots. Line through data point indicates specimen had nonuniform microstructure. More
Image
Published: 01 December 2004
Fig. D6.2 213.0-F, sand cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.3 224.0-T62, sand cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.4 240.0-F, sand cast aluminum casting rotating-beam fatigue curve. Smooth specimens from three lots More
Image
Published: 01 December 2004
Fig. D6.5 240.0-F, sand cast aluminum casting rotating-beam fatigue curve. Data points for smooth and notched specimens from one lot are compared to curves from previous tests. More
Image
Published: 01 December 2004
Fig. D6.6 242.0-O, sand cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.7 242.0-T571, permanent mold aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.8 242.0-T571, permanent mold aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.9 242.0-T571, sand cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.10 242.0-T571, cast pistons aluminum casting rotating-beam fatigue curve. Smooth specimens are from the wrist pin boss, shaped to Fig. A3.2(a), Appendix 3 . Open circle symbol, cast head down, others cast head up More
Image
Published: 01 December 2004
Fig. D6.11 242.0-T571, cast pistons aluminum casting rotating-beam fatigue curve. Smooth specimens are from the wrist pin boss, shaped to Fig. A3.2(a), Appendix 3 . Solid symbols are vacuum riserless castings (VRC); open symbol is standard. More
Image
Published: 01 December 2004
Fig. D6.12 242.0-T61, permanent mold aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.13 242.0-T75, sand cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.14 242.0-T77, sand cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.15 242.0-T77, sand cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot More