1-20 of 335 Search Results for

failure mode analysis

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410253
EISBN: 978-1-62708-280-8
... validation, product launch, and continuous improvement. This is followed by sections covering product-process flow diagrams and also the process elements considered for process failure mode and effects analysis. Some of the aspects covered by the engineering specifications to meet the product performance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110461
EISBN: 978-1-62708-247-1
... procedures based on focused ion beam milling used for TEM sample preparation. It describes the principles behind commonly used imaging modes in semiconductor failure analysis and how these operation modes can be utilized to selectively maximize signal from specific beam-specimen interactions to generate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.t51180151
EISBN: 978-1-62708-256-3
... with the investigation and analysis of metallurgical failures that occur in service. It describes the steps of an orderly failure analysis from collecting and examining samples to performing mechanical and nondestructive tests, preparing and examining fractographs and micrographs, determining failure mode, writing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110587
EISBN: 978-1-62708-247-1
..., namely, common mode choke coil and surface mount powder choke coil. capacitors failure analysis failure modes inductors General construction of Tantalum, Aluminum electrolytic, Multi-layer Ceramics, Film, and Super capacitors and Common Mode Choke and Surface Mount inductors are explained...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270031
EISBN: 978-1-62708-301-0
.... The chapter also covers quantitative fractography, fracture surface topography analysis, and the use of oxide dating as well as fault tree and failure modes and effects analysis (FMEA) and computational techniques. fault tree analysis fracture surface topography analysis oxide dating quantitative...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780093
EISBN: 978-1-62708-268-6
...Abstract Abstract After the fault-tree, a failure-cause identification method has identified potential failure causes and the failure analysis team has prepared a failure mode assessment and assignment (FMA&A). The team knows specifically what to search for when examining components...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780171
EISBN: 978-1-62708-268-6
...Abstract Abstract After the failure analysis team hypothesizes failure causes, prepares a failure mode assessment and assignment, and evaluates all potential failure causes, it may find in some cases that several causes are still suspect but cannot be confirmed. In this situation, an experiment...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270130
EISBN: 978-1-62708-301-0
... aircraft. The bolts were removed and analyzed to determine the mode and cause of failure. Based on the results of macroscopy, scanning electron fractography, metallographic examination, and chemical analysis, the failures were caused by stress corrosion cracking, and in one case, overtightening...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780404
EISBN: 978-1-62708-281-5
... introduces the subject of fractography and how it is used in failure analysis. The discussion covers the structure of and fracture and crack-propagation behavior of polymeric materials, the distinction between the ductile and brittle fracture modes on the basis of macroscopic appearance, and the examination...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630257
EISBN: 978-1-62708-270-9
...Abstract Abstract Fracture mechanics is a well-developed quantitative approach to the study of failures. This chapter discusses fracture toughness and fracture mechanics, linear-elastic fracture mechanics, and modes of loading. The discussion also covers plane strain and stress and crack growth...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410009
EISBN: 978-1-62708-280-8
... a design or the process can fail, impairing the product quality or consistency, and what preventive measures or controls need to be implemented to prevent these potential failures. The designer prepares a design failure mode analysis (DFMEA) and the casting engineer prepares a process failure mode analysis...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110513
EISBN: 978-1-62708-247-1
...://www.sciencedirect.com/science/article/pii/S002627140600196X 10.1016/j.microrel.2006.07.048 [7] Tharian , Joy , “ Degradation- and Failure Mode Analysis of III-V Nitride LEDs ”, Master Thesis, May 2007 , Vorarlberg University of Applied Sciences, Bregenz, Austria [8] Tarr , Martin...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110524
EISBN: 978-1-62708-247-1
... , ( 2002 ). 10.1063/1.1448166 19. Suning Xie , Herrick Robert W. , Chamberlin Danielle , Rosner S.J. , McHugo Scott , Girolami Grant , Mayone Myrna , Kim Seongsin , and Widjaja Wilson , “ Failure Mode Analysis of Oxide VCSELs in High Humidity and High...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130001
EISBN: 978-1-62708-284-6
... for, leading to an unprofitable and technically useless product. Failure modes analysis is a procedure in which each potential failure mode is analyzed to determine its effects and the criticality of these effects on the system and to rank each potential failure according to its severity. The criticality...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780417
EISBN: 978-1-62708-281-5
... tested under interlaminar mode I tension loading. Visually, these surfaces exhibit milky white, dull fracture surfaces. Again, failure of the laminate generally occurs in the plane of the reinforcement, and SEM analysis reveals distinctive fractographic features. On these fracture surfaces...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780067
EISBN: 978-1-62708-268-6
... or even thousands of potential causes to assess. The failure analysis team now needs a tool to help manage the evaluation of each hypothesized failure cause. Failure mode assessment and assignment (FMA&A) is a tool designed to help organize the evaluation of hypothesized failure modes. The FMA...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110506
EISBN: 978-1-62708-247-1
... failure mode recognition software for defect classification [3] , data analysis tools based upon statistical methods, and powerful interactive data mining features. (See Figure 1 ). The wealth of signature information available is at the heart of the FA effort, and is often underutilized...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130111
EISBN: 978-1-62708-284-6
...Abstract Abstract This chapter briefly outlines some of the basic aspects of failure analysis, describing some of the basic steps and major concerns in conducting a failure analysis. A brief review of failure types from fracture, distortion, wear-assisted failure, and environmentally assisted...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780109
EISBN: 978-1-62708-268-6
... to correct the conditions that allowed these nonconformances to occur, but the team cannot jump to the conclusion that just because a component is nonconforming it must have caused the failure. Each nonconformance should be compared to the fault-tree analysis and the failure mode assessment and assignment...