Published: 01 December 2006
Fig. 7.127 Left, chemical vapor deposition (CVD)-coated aluminum extrusion dies. Right, demanding heat exchanger sections in AlMgSi0.5 produced with CVD–coated dies. Source: WEFA Singen Gmbh More
Image
Published: 01 August 2012
Fig. 16.15 Applications of physical vapor deposition (PVD) coatings. (a) PVD TiN used for soda can tab punch. (b) PVD TiCN used for AA battery casing extrusion punch. Source: Ref 16.55 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260187
EISBN: 978-1-62708-336-2
... Abstract This chapter discusses the extrusion characteristics of hard aluminum alloys, particularly those in the 5000 and 7000 series. It begins with a review of two studies, one showing how the extrudability of 7 xxx alloys varies with the presence and amount of different alloying elements...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260087
EISBN: 978-1-62708-336-2
... life, and improve productivity in aluminum extrusion. Pye ( Ref 21 ) has reviewed surface modification techniques for preheated H13 extrusion dies and emerging technologies. He has compared deposition materials and different methods that offer good potential for wear resistance. Sundqvist et al. ( Ref...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290251
EISBN: 978-1-62708-319-5
... combinations, and processing ideas, such as binder jetting and extrusion-based additive manufacturing, including bound-metal deposition and fused-filament fabrication. 11.1 Introduction Science fiction is a great resource for looking forward to where technology advances may take us. The ideas of flying...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... and slurry casting, liquid metal infiltration, spray deposition, powder metallurgy, extrusion, hot rolling, and forging. The chapter also provides information on continuous-fiber aluminum and titanium composites as well as particle-reinforced titanium and fiber metal (glass aluminum) laminates...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
..., die compaction, extrusion, injection molding, slip casting, slurry processes, and tape casting. Information on equipment setup, requirements, and the various factors influencing these processes are described. In addition, the chapter provides information on novel approaches and processing costs...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900153
EISBN: 978-1-62708-350-8
... Fig. 1 Core support of the nitrided case on a forging die. Source: Ref 1 Fig. 2 Schematic cross section of an aluminum extrusion die made from H13 steel showing the bearing (wear) surface and a core with hardness of 38 to 44 HRC. Source: Ref 1 Fig. 3 Extrusion presses...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390325
EISBN: 978-1-62708-459-8
... of metals in open-die, closed-die, and impression-die forging and in back extrusion and piercing operations. It presents various ways to achieve fluid-film lubrication in upset forging processes and examines the cause of barreling, defect formation, and folding in the upsetting of cylinders, rings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260055
EISBN: 978-1-62708-336-2
... unloading, and return conveying of the spacers downstream of the aging furnace. Fig. 32 Automatic section stacker. (1) Section stacker depositing in section basket. Source: SMS Engineering Inc. Integrated System The performance of an aluminum extrusion plant depends largely on its auxiliary...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900163
EISBN: 978-1-62708-350-8
... Fig. 1 Extrusion dies lifted from the furnace hearth to allow the plasma glow seam to cover the die completely. Note the die supports (steel tubes) used to maintain cathode potentials. Fig. 2 Masking of blind tapped holes on a component for plasma nitriding. Abstract Stop...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390284
EISBN: 978-1-62708-459-8
... Abstract This chapter deals with the mechanics and tribology associated with the extrusion of bars, sections, and tubes. It covers direct and indirect extrusion processes in detail and demonstrates the use of important equations, relationships, and measurements for determining pressure, force...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980417
EISBN: 978-1-62708-342-3
... Abstract This chapter begins with a description of the requirements of tooling and tooling material for hot extrusion. It covers the processes of designing tool and die sets for direct and indirect extrusion. Next, the chapter provides information on extrusion tooling and die sets for direct...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900071
EISBN: 978-1-62708-350-8
... into the steel surface. Nitride networking also is shown. Fig. 6 Chipping at the pressure point of a gear tooth. Courtesy of Pye Metallurgical Consulting, Inc. Fig. 7 Extrusion die with surface exfoliation. Courtesy of Pye Metallurgical Consulting, Inc. Fig. 8 Cross section through...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980323
EISBN: 978-1-62708-342-3
... Abstract The machinery and equipment required for rod and tube extrusion is determined by the specific extrusion process. This chapter provides a detailed description of the design requirements and principles of machinery and equipment for direct and indirect hot extrusion. It then covers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
... Abstract Compared with other deformation processes used to produce semifinished products, the hot-working extrusion process has the advantage of applying pure compressive forces in all three force directions, enhancing workability. The available variations in the extrusion process enable a wide...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340453
EISBN: 978-1-62708-427-7
... 50% for the last 20 years, but it fell slightly to 45% in 2021 ( Ref 20.6 ). This loss of more than 50 billion cans per year to the recycling stream has an annual financial impact on the order of $800 million. In 2022, only 10 out of 50 states imposed a $0.05–0.10 per container deposit , not just...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.9781627083423
EISBN: 978-1-62708-342-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230295
EISBN: 978-1-62708-298-3
... Abstract The vast majority of beryllium products are manufactured from blocks, forms, or billets of compacted powder that are machined or worked into shape. This chapter describes the metalworking processes used, including rolling, forming, forging, extrusion, drawing, and spinning. It covers...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390001
EISBN: 978-1-62708-459-8
... remained dominant in Europe until recent years, and were often aided by the deposition of a thin copper or copper-tin coat on the steel wire by drawing from baths containing copper sulfate. Like so many innovations, this too was a result of an accident; the coating was observed to develop when hot brass...