Image
Published: 01 November 2011
Fig. 6.22 Schematic showing key components used in parallel gap explosion welding process. Source: Ref 6.11 More
Image
Published: 01 August 1999
Fig. 11.14 Weld interface of an explosive weld of 0.15% C steel plate and commercially pure aluminum plate. (a) 1% nital. 10× (b) and (c) 1% nital. 100×. More
Image
Published: 01 August 1999
Fig. 11.10 Steel to steel (0.15% C) explosive weld, made under conditions that produce a planar weld. (a) Weld interface. 1% nital. 100×. (b) Weld interface. 1% nital. 1000×. (c) Weld interface: heated at 925 °C for 30 min and cooled at 500 °C/h after welding. 1% nital. 1000×. (d) Weld More
Image
Published: 01 August 1999
Fig. 11.11 (Part 1) Steel to steel (0.1 5 % C) explosive weld, made under conditions that produce an undulating weld interface. (a) and (b) Weld interface: sectioned parallel to direction of propagation of jet. (a) 1% nital. 100×. (b) 1% nital. 1000×. (c) and (d) Weld interface More
Image
Published: 01 August 1999
Fig. 11.12 Effects of heat treatment after explosive welding steel to steel (0.15% C). Same weld as illustrated in Fig. 11.11 except for post-welding heat treatment. (a) and (b) Heated at 650 °C for 30 min. (a) 1% nital. 100×. (b) 1% nital. 1000×. (c) and (d) Heated at 925 °C for 30 More
Image
Published: 01 August 1999
Fig. 11.13 Steel to steel (0.15% C) explosive weld made under conditions of considerable overpressure. (a) 1% nital. 100×. (b) 1% nital. 500×. More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290137
EISBN: 978-1-62708-306-5
... such as diffusion welding, forge welding, roll welding, coextrusion welding, cold welding, friction welding, friction stir welding, explosion welding, and ultrasonic welding. coextrusion welding cold welding diffusion welding explosion welding forge welding friction welding roll welding ultrasonic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560309
EISBN: 978-1-62708-291-4
... processes, including electroslag, TIG, gas, electron-beam, and arc welding as well as vacuum diffusion, forge, friction, electrical-resistance, and explosive welding. It also discusses the effect of welding temperature, pressure, and composition on the transformations that occur in and around the weld...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820169
EISBN: 978-1-62708-339-3
... (diffusion welding, explosion welding, friction welding, or ultrasonic welding), brazing, or soldering where alloying between the metals is normally insignificant. This chapter describes the factors influencing joint integrity and discusses the corrosion behavior of dissimilar metal weldments. brazing...
Image
Published: 01 March 2002
Fig. 6.22 Welded cylinder of HA-25 in position for explosive forming. (Dimensions in inches) More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270059
EISBN: 978-1-62708-301-0
...., manufacturing caprolactam was completely destroyed and reduced to ashes, and the surrounding community was demolished with many fatalities, following a powerful explosion of warlike dimensions inside the plant ( Ref 1 ). The details of this disaster have been described in Chapter 2, “Common Causes of Failures...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280091
EISBN: 978-1-62708-267-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500227
EISBN: 978-1-62708-317-1
... 7.9–269 10 2 Explosive forming 9–228 30–748 10 2 –10 4 Magnetic forming 27–228 89–748 10 3 –10 4 Electrohydraulic forming 27–228 89–748 10 3 –10 4 Source: Ref 11.3 Due to the high strain rates, in high-velocity forming of several materials, including aluminum alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930353
EISBN: 978-1-62708-359-1
... bonding, friction welding, brazing, and explosion bonding ( Ref 1 ). Electron beam welding is used in critical applications. Tantalum usually is welded by GTAW. Unalloyed tantalum can be welded with inert gas shielding on both sides of the weld using the same techniques that are used to weld titanium...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.t51180001
EISBN: 978-1-62708-256-3
... of a component, assembly, or structure can be multilevel. In other words, a failure should not be viewed as a single event. The actual physical failure—a fracture, an explosion, damage by heat or corrosion—is the most obvious. However, other levels of failures generally exist that allow the physical event...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700177
EISBN: 978-1-62708-279-2
... , such as friction welding, diffusion welding, ultrasonic welding, roll welding, forge welding, and explosion welding In fusion welding, joining is accomplished by melting the location of the two parts to be joined, in some cases adding filler metal to the joint. Because melting of the base metals occurs...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
... processes. The selection of the appropriate solid-state welding process would depend on joint (part) geometry. A transition joint between a plate and a pipe is best produced using a friction welding process, whereas a joint between two large plate surfaces is best produced using explosive bonding. Because...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270005
EISBN: 978-1-62708-301-0
... Welds Improper fusion Cracks in heat affected zone Wrong filler material Machined parts Poor surface finish Grinding burns Heat treatment Quench cracks Overheating Undertempering Surface treatment Improper cleaning Improper plating Improper post...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230001
EISBN: 978-1-62708-351-5
... of the joint to a temperature below the melting point of the components. Pressure welding (especially in the form of explosive welding) and friction welding are often much faster processes than soldering or brazing (<1 s), while diffusion bonding is much slower (>10 min). The joints have no fillets...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
...Abstract Abstract This chapter describes the processes involved in the fabrication of wrought and cast metal products. It discusses deformation processes including bending and forming, material removal processes such as milling, cutting, and grinding, and joining methods including welding...